Cellular proliferation and macrophage populations associated with implanted expanded polytetrafluoroethylene and polyethyleneterephthalate.

The chronic inflammatory response associated with the abluminal surface of polymeric vascular grafts has been suggested to affect adversely graft neovascularization, the cellular response at the luminal surface of vascular grafts, and overall graft patency. To better understand the source for this chronic inflammation, this study examined two types of macrophages and the amount of cellular proliferation around two widely used graft materials, expanded polytetrafluoroethylene (ePTFE) and polyethyleneterephthalate (PET or Dacron) implanted in the rat for 3 and 5 weeks. Serial sections of explants were analyzed for recruited macrophages (ED1), resident macrophages (ED2), and proliferating cells (PCNA). Results show that Dacron is more inflammatory than ePTFE and that there is a segregated macrophage response; the first 54 micrometer of perigraft tissue were composed predominantly of recruited macrophages (ED1+) while the more distal tissue consisted of resident macrophages (ED2+). Proliferating cells were located predominantly in this same 54 micrometer perigraft region. In subcutaneous tissue they accounted for 23% of all cells present around Dacron after 3 weeks of implantation and 8% after 5 weeks. Conversely, cellular proliferation around ePTFE increased from 4% at 3 weeks to 21% at 5 weeks. In adipose tissue, proliferation levels around the implanted polymers were lower and more similar after 3 and 5 weeks. Serial sections revealed the coordinate expression of PCNA and ED1 antigens by the same individual cells, suggesting that proliferation is a mechanism used to perpetuate the chronic inflammatory response. These results suggest a new target for designing treatments to alter inflammation and improve the healing associated with these biomaterials.

Adipose Tissue↗

Healing response associated with balloon-dilated ePTFE.

Deployment of endovascular grafts composed of a metallic stent surrounded by expanded polytetrafluoroethylene (ePTFE) stretches the polymer beyond its original dimensions, altering the structural characteristics of the ePTFE. We hypothesized this structural modification would alter the healing response associated with the implant. In this study, 4 mm i.d. of ePTFE (30 microns internodal distance) vascular grafts were balloon dilated using angioplasty balloons having final diameters of 6 (1.5X), 8 (2X), 10 (2.5X), 12 (3X), and 18 (4.5X) mm. Following balloon dilatation of the ePTFE, a circular punch (6 mm in diameter) was used to prepare polymer samples for implantation. The ePTFE circular patches were implanted within subcutaneous tissue and epididymal fat pads of male Sprague-Dawley rats. After 5 weeks, the implants were removed and analyzed for fibrous capsule formation, inflammation, and neovascularization associated with the material. Histological analysis revealed the formation of fibrous capsules only with control subcutaneous implants. The inflammatory response associated with subcutaneously implanted ePTFE was decreased significantly following balloon dilatation to at least 2.5 times the original diameter of the graft. In contrast, ePTFE implanted within adipose tissue demonstrated a significantly greater inflammatory response following balloon dilatation when compared to control implants. Only ePTFE balloons dilated to 6 mm and implanted within adipose tissue demonstrated neovascularization to any extent. These data suggest the structural modifications incurred by ePTFE following balloon dilatation dramatically affect the inflammatory response associated with an implant. Therefore, polymeric materials used for endovascular graft technology require designs that consider changes in polymer healing inherent to device design.

Adipose Tissue↗

Effects of balloon dilatation on ePTFE structural characteristics.

The search for less invasive treatments for cardiovascular disease has lead to the development of endovascular stent grafts, metallic and alloy stents surrounded by prosthetic vascular graft material. Introduced intravascularly, the deployment of stent grafts requires balloon dilatation of the device which results in expansion of the stent along with the vascular graft material. We hypothesized that balloon dilatation of stent grafts would alter the physical structure of the prosthetic graft material. In this study, noncompliant angioplasty balloons were used to dilate expanded polytetrafluoroethylene (ePTFE), a material commonly used for endovascular stent-graft technology. The maximal outer diameter (inflated balloon within the lumen) and the recoiled outer diameter (balloon removed) of two types of ePTFE, 3-mm inside diameter (i.d.) thin wall (30-micron internodal distance) and 4-mm i.d. standard wall (30-micron internodal distance), were measured to compare material recoil. Following balloon dilatation, ePTFE samples were prepared for scanning electron microscopic examination and the following parameters were measured: wall thickness, internodal distance, nodal width, interfiber distance, and fiber width. Following primary dilatation, both types of ePTFE recoiled approximately 20% regardless of inflated balloon diameter. However, following eight repetitive balloon dilatations, recoil decreased to approximately 10%. Scanning electron microscopic analysis revealed variations in internodal distance and significant decreases in wall thickness, nodal thickness, and interfiber distance. Fiber width was significantly decreased following dilatation of 3 mm, but not 4 mm ePTFE. Our data support our initial hypothesis that balloon dilatation alters the structure of ePTFE.

Blood Vessel Prosthesis↗

The effects of porosity on endothelialization of ePTFE implanted in subcutaneous and adipose tissue.

Healing of biomaterial implants varies depending on the type and structure of material and the tissue surrounding the implant. In this study we examined structural differences of 30 microm, 60 microm, and 100 microm expanded polytetrafluoroethylene (ePTFE) using scanning electron microscopy, and we also investigated differences in healing for these three different porosity ePTFE grafts implanted within subcutaneous tissue and adipose tissue. Scanning electron microscopic examination of 30 microm, 60 microm, and 100 microm ePTFE revealed structural differences and differences in fiber density within the internodal space. Circular patches (6 mm in diameter) of 30 microm ePTFE were implanted within subcutaneous tissue and epididymal fat pads of male Sprague-Dawley rats. After 5 weeks, the implants were removed and analyzed for fibrous capsule formation, endothelialization, and for activated monocytes and macrophages in association with the material. Histological evaluation revealed dense fibrous capsule formation surrounding only the 30 microm ePTFE subcutaneous implants. From immunohistochemistry data obtained, we generated an Endothelialization Index (measure of neovascularization) and a Monocyte/Macrophage Index (measure of inflammatory response) for each sample. Consistently, 60 microm ePTFE had the greatest Endothelialization Index at both implant sites while 100 microm ePTFE generally had the largest values for the Monocyte/Macrophage Index. These data indicate that both the structure of the material and the site of implant influence the healing characteristics of ePTFE and suggest that activated monocytes and/or macrophages associated with the implant may inhibit endothelialization of ePTFE.

Adipose Tissue↗

Stent versus endovascular graft healing characteristics in the porcine iliac artery.

PURPOSE: To evaluate the healing characteristics of stents versus endovascular grafts in the porcine iliac artery. MATERIALS AND METHODS: A total of 20 iliac arteries in 10 domestic swine were used to evaluate the healing characteristics of stents versus endovascular grafts. Each animal received one stent and one endovascular graft in opposite iliac arteries. The endovascular grafts were constructed with use of 6 cm of expanded polytetrafluoroethylene (ePTFE) (3 mm inner diameter, 30 microm internodal distance) and Palmaz stents (P204 or P188) secured at each end of the graft. A solitary Palmaz stent (P308 or P294) was used on the opposite side. The devices were explanted at 1, 5, and 12 weeks. RESULTS: One of three endovascular grafts and two of three stents were patent at 1 week. Two of three endovascular grafts and all three stents were patent at 5 weeks. All three endovascular grafts and stents were patent at 12 weeks. Gross examination, histologic, and scanning electron microscopy demonstrated differences in the healing response of the two devices. A marked abluminal inflammatory response to the graft material was observed. This resulted in neovascularization of the tissue along the abluminal surface of the graft. In addition, marked neointimal thickening at the unsupported section of the endovascular graft resulted in significant luminal narrowing. CONCLUSION: The porcine model may be used for evaluating the healing characteristics of endovascular grafts. Intravascular placement of ePTFE prosthetic graft material dramatically alters the healing of this type of graft material. The graft material did not prevent the formation of a progressively thickening neointima.

Animals↗

Inflammation and neovascularization associated with clinically used vascular prosthetic materials.

This study was designed to evaluate and compare healing characteristics, specifically neovascularization and inflammation, of polymeric vascular graft materials commonly used in clinical applications. Our hypotheses were (i) polymeric materials used in vascular graft manufacture stimulate chronic inflammation and (ii) inflammation and neovascularization of polymeric materials are related. Impra and Gore-Tex ePTFE, Meadox weavenit and woven Dacron, Hemashield microvel and woven Dacron, and Golaski microknit Dacron were implanted as 6-mm diameter disks within rat subcutaneous and adipose tissue. Following 5 weeks of implantation samples were evaluated by histological and immunocytochemical analysis. Sections were stained using hematoxylin and eosin or reacted with ED1 antibody and GS1 lectin to quantify inflammation and neovascularization. respectively. The extent of inflammation and neovascularization were influenced by both tissue site of implantation and polymer characteristics. For subcutaneous implants, inflammation was graded as follows: Meadox weavenit > Hemashield woven > Meadox woven > Gore-Tex ePTFE > Hemashield microvel > ImpraePTFE > Golaski microknit, while only the Golaski microknit neovascularized. Inflammation was graded as follows for adipose implants: Hemashield woven > Hemashield microvel > Meadox weavenit > Meadox woven > Gore-Tex ePTFE > Golaski microknit > Imnpra ePTFE, while the following order of neovascularization was observed: Impra ePTFE > Gore-Tex ePTFE > Golaski microknit. The degree of inflammation following biomnaterial implantation has a profound effect on implant neovascularization. These data suggest an inverse relationship exists between inflammation and neovascularization.