Spectroscopy of stripe order in La1.8Sr0.2NiO4 using resonant soft x-ray diffraction.

Strong resonant enhancements of the charge-order and spin-order superstructure-diffraction intensities in La1.8Sr0.2NiO4 are observed when x-ray energies in the vicinity of the Ni L2,3 absorption edges are used. The pronounced photon-energy and polarization dependences of these diffraction intensities allow for a critical determination of the local symmetry of the ordered spin and charge carriers. We found that not only the antiferromagnetic order but also the charge-order superstructure resides within the NiO2 layers; the holes are mainly located on in-plane oxygens surrounding a Ni2+ site with the spins coupled antiparallel in close analogy to Zhang-Rice singlets in the cuprates.

Journal Article↗

Finite-size effect on magnetic ordering temperatures in long-period antiferromagnets: holmium thin films.

The thickness dependence of the helical antiferromagnetic ordering temperature T(N) was studied for thin Ho metal films by resonant magnetic soft x-ray and neutron diffraction. In contrast with the Curie temperature of ferromagnets, T(N) was found to decrease with film thickness d according to [T(N)(infinity)-T(N)(d)]/T(N)(d) proportional variant (d-d(0))(-lambda(')), where lambda(') is a phenomenological exponent and d(0) is of the order of the bulk magnetic period L(b). These observations are reproduced by mean-field calculations that suggest a linear relationship between d(0) and L(b) in long-period antiferromagnets.

Journal Article↗

Magnetic splitting of valence states in ferromagnetic and antiferromagnetic lanthanide metals

The magnetic splitting of Delta(2) valence states in the heavy lanthanide metals Gd, Tb, Dy, and Ho was studied in epitaxial films by angle-resolved photoemission, revealing an essentially Stoner-like temperature dependence in all cases. It scales linearly with the 4f spin moment, even in the case of the helical antiferromagnet Ho. Such a behavior can be explained by a substantial localization of the corresponding wave function in the c direction. The helical magnetic structure was confirmed for the thin Ho films by in situ resonant magnetic x-ray diffraction.