Biodurability of retrieved silicone gel breast implants.

This study analyzed the shells of single-lumen silicone gel breast implants within the general context of device durability in vivo. The investigation included the major types of gel-filled implants that were manufactured in the United States in a 30-year period. The implants analyzed were Cronin seamed (two explants and one control), Silastic 0 and Silastic I (18 explants and seven controls), and Silastic II (22 explants and 43 controls). The biodurability of the explants was investigated with measurements of the mechanical and chemical properties of the various types of silicone gel control and explanted shells, with implantation times ranging from 3 months to 32 years. The shell properties measured for the controls and explants included the stress-strain relationships, tensile strength, elongation, tear resistance, moduli, cross-link density, and amount of extractable material in the shell. In addition, the mechanical properties of shells that had been extracted with hexane were analyzed for both explants and control implants. The silicone gel explants investigated in this study included some of the oldest explants of the various major types that have been tested to date. For assessment of long-term implantation effects, the data obtained in this study were combined with all known data from other institutions on the various major types of gel implants. The study also addressed the failure mechanisms associated with silicone gel breast implants. The results of the study demonstrated that silicone gel implants have remained intact for 32 years in vivo and that degradation of the shell mechanical and chemical properties is not a primary mechanism for silicone gel breast implant failure.

Biomechanical Phenomena↗

Protocol for retrieval and analysis of breast implants.

The Center for Implant Retrieval and Analysis has been established at Washington University's Division of Plastic and Reconstructive Surgery for the purpose of studying implantable devices retrieved after surgery or autopsy and assessing their condition after implantation. Since the early 1990s, significant experience has been gained in testing and analyzing silicone gel breast implants and, to a lesser extent, saline-filled devices. However, there has been no systematic method reported for collecting and evaluating these implants in a way that would permit different laboratories to compare their data. This article offers the plastic and reconstructive surgery community a standardized protocol for analyzing explanted silicone gel and saline-filled breast implants. The protocol gives surgeons a clearly defined approach for removing, handling, documenting, and shipping explanted breast implants. At the same time, biomaterials researchers can use the protocol to acquire implant data with reliable and reproducible methods. Because the study of saline implants has lagged behind the study of silicone gel implants, the article concludes with a demonstration of how this protocol can be applied to obtain mechanical properties data and use scanning electron microscopy to illuminate failure mechanisms of saline devices, including three explants removed after 20+ years in vivo.

Breast Implants↗

In vivo aging characteristics of silicone gel breast implants compared to lot-matched controls.

A study was conducted to investigate the effect of in vivo aging on the physical, mechanical, and chemical properties of Silastic II gel-filled breast implants. In the study, the properties of 16 Silastic II gel-filled explants (retrieved from eight patients), with in vivo duration times ranging from 4 months to 13 years, were compared with lot-matched control (unimplanted) samples. Tensile and tear strength properties were measured for both explant and control shells by using identical testing protocols. The tensile strength properties of shells, which were extracted with hexane to remove non-cross-linked silicones, were also measured. Swelling measurements were used to determine the average molecular weight between cross-links (or entanglements). In addition, scanning electron microscopy was applied in the comparison of the morphological features of the explants and their lot-matched controls. The results of the study suggest that the silicone polymer used to fabricate the shells does not undergo appreciable degradation for up to 13 years in vivo. The study represents an investigation of the world's largest known inventory of explanted breast implants with lot-matched controls.

Breast Implants↗

The effect of cyclic swelling (octamethylcyclotetrasiloxane) on the physical properties of silicone breast implant shells.

Changes in the physical and mechanical properties of silica filled silicone elastomeric films were studied as a function of repeated sorption extraction cycling. The sorption of octamethylcyclotetrasiloxane (D4) on the properties of three silicone filled elastomeric films was analyzed. Two of the films, SILASTIC I and SILASTIC II, were shells of explanted breast implants and the third, a calendered film, prepared with similar composition to the elastomer used for the breast prosthesis were studied. The as-received (AR) SILASTIC I and II films contained 20 and 26.5 wt% non-cross-linked material that was removed by extraction with hexane. The failure properties of the extracted films are significantly higher than those of the AR films. The amount of swelling, weight gain, volumetric change, and the stress- and strain-to-fail of the films were measured in the as-received condition, and after a series of extractions and swellings. Repeated cycling (up to 5 cycles) of extraction-swelling had essentially no effect on the failure properties of films when all the diluent was removed. The effect of diluent on the failure properties of all three films was quite large. The stress-to fail of the swollen film was reduced a factor of 6 compared to baseline extracted samples while the corresponding strain values were reduced a factor of 5. The energy to fail of the swollen compared to baseline films was reduced almost a factor of 50. However, the overall mechanical properties of the films are restored when the diluent was removed. The mechanical forces involved in the swelling process do not degrade the polymer even when cycled through five swell-extract cycles.

Absorption↗