PubMed Health⌕ Search

Biomedical subjects

Jan De Munck

Publications and source records attributed to Jan De Munck.

23 records · Page 2Linked to original sources

Buonocore memorial lecture. Adhesion to enamel and dentin: current status and future challenges.

Bonding to tooth tissue can be achieved through an "etch&rinse," "self-etch" or "glass-ionomer" approach. In this paper, the basic bonding mechanism to enamel and dentin of these three approaches is demonstrated by means of ultramorphological and chemical characterization of tooth-biomaterial interfacial interactions. Furthermore, bond-strength testing and measurement of marginal-sealing effectiveness (the two most commonly employed methodologies to determine "bonding effectiveness" in the laboratory) are evaluated upon their value and relevance in predicting clinical performance. A new dynamic methodology to test biomaterial-tooth bonds in a fatigue mode is introduced with a recently developed micro-rotary fatigue-testing device. Eventually, today's adhesives will be critically weighted upon their performance in diverse laboratory studies and clinical trials. Special attention has been given to the benefits/drawbacks of an etch&rinse versus a self-etch approach and the long-term performance of these adhesives. Correlating data gathered in the laboratory with clinical results clearly showed that laboratory research CAN predict clinical effectiveness. Although there is a tendency to simplify bonding procedures, the data presented confirm that conventional three-step etch&rinse adhesives still perform most favorably and are most reliable in the long-term. Nevertheless, a self-etch approach may have the best future perspective. Clinically, when adhesives no longer require an "etch&rinse" step, the application time, and probably more importantly, the technique-sensitivity are substantially reduced. Especially "mild," two-step self-etch adhesives that bond through a combined micromechanical and chemical interaction with tooth tissue closely approach conventional three-step systems in bonding performance.

Acid Etching, Dental↗

Microtensile bond strengths of an etch&rinse and self-etch adhesive to enamel and dentin as a function of surface treatment.

In light of the current trend towards "minimal invasive" dentistry, diverse cavity preparation techniques have been introduced as an alternative or addition to common bur instrumentation. This study investigated whether diamond sonoabrasion (SonicSys Micro, Kavo), air abrasion (Prep Start, Danville) and Er:YAG laser irradiation (Fidelis) produce surfaces at enamel/dentin that are equally receptive to bonding as traditional mid-grit diamond-bur (Komet) and 600-grit SiC-paper prepared surfaces, of which the latter two served as controls. An etch&rinse adhesive (OptiBond FL, Kerr) applied with and without prior acid-etching and a self-etch adhesive (Clearfil SE, Kuraray) were employed to bond the restorative composite (Z100, 3M ESPE) to the diversely prepared enamel and dentin surfaces. The microtensile bond strength (microTBS) was determined after 24 hours of storage in water at 37 degrees C. The results indicated that the manner of preparation of enamel and dentin prior to bonding procedures significantly influenced the bonding effectiveness of both the etch&rinse and the self-etch adhesive. Using an etch&rinse adhesive, separate acid-etching of air-abraded and Er:YAG-irradiated enamel and dentin surfaces remains mandatory. Bonding to diamond-sonoabraded and air-abraded enamel and dentin was, in general, not different from bonding to conventional diamond-bur prepared surfaces, whereas, bonding to Er:YAG-irradiated enamel and dentin surfaces in general resulted in a significantly lower bonding effectiveness compared to bonding to diamond-bur prepared surfaces.

Acid Etching, Dental↗

A randomized, controlled trial evaluating the three-year clinical effectiveness of two etch & rinse adhesives in cervical lesions.

A three-year randomized, controlled prospective study evaluated the clinical performance of two three-step etch & rinse adhesives (OptiBond FL, Kerr: O-FL; PermaQuick, Ultradent: PMQ) in Class V cervical erosion-abrasion lesions. The latter adhesive was also tested with two restorative composites with contrasting stiffness in order to evaluate the effect composite stiffness might have on the clinical longevity of cervical restorations. A total of 150 lesions were randomly restored in pairs of the three adhesive/composite combinations (PMQ combined with Amelogen Hybrid: PMQ/A-Hy, Ultradent; PMQ combined with Amelogen Microfill: PMQ/A-Mi, Ultradent; O-FL combined with Prodigy: O-FLJPro, Kerr) per patient and evaluated at baseline, after six months, one year, two years and three years of clinical service. After three years, the retention rate was 100% for O-FL/Pro and 98% for both PMQ/A-Hy and PMQ/A-Mi, thereby, satisfying the "full acceptance" guidelines specified by the American Dental Association. A pairwise comparison showed no significant difference in adhesive performance between restorations made using the microfilled and hybrid composite for any evaluation criteria (p>0.05).

Chi-Square Distribution↗

Effect of conditioner on bond strength of glass-ionomer adhesive to dentin/enamel with and without smear layer interposition.

The effect of a polyalkenoic acid conditioner pretreatment on the bond strength of a glass-ionomer adhesive to tooth substrates with or without smear layer was evaluated. Smear-layer covered and smear-layer free dentin and enamel surfaces were prepared from 24 extracted human molars. Resin composite was bonded to the surfaces using FujiBond LC with or without a polyalkenoic acid conditioner and subjected to microtensile bond strength (microTBS) testing. Failure modes were determined using scanning electron microscopy. For dentin, smear-layer coverage and conditioner treatment did not reveal significant differences in microTBS, which ranged from 20 to 29 MPa. For enamel, smear-layer coverage did not significantly affect microTBS, whereas, the use of conditioner significantly improved microTBS, reaching the same microTBS-values as when bonded to dentin. Regarding failure mode, most dentin specimens failed mixed adhesive cohesively. For enamel, adhesive failures mostly occurred when no conditioner was used, though mixed failures were predominant when the specimens were conditioned beforehand. Bonding of the glass ionomer adhesive to dentin can be achieved without the separate use of a polyalkenoic acid conditioner, even with the interposition of a smear layer. However, instrumented and non-instrumented enamel requires separate conditioning to provide sufficient micro-mechanical retention.

Acrylic Resins↗

One-day bonding effectiveness of new self-etch adhesives to bur-cut enamel and dentin.

Self-etch adhesives try to solve difficulties commonly associated with the clinical application of etch-and-rinse adhesives. Their application procedure is considered less time-consuming and, more importantly, less technique-sensitive. The main objective of this study was to determine the bonding effectiveness to and the interaction with enamel/dentin of three contemporary one- and two-step self-etch adhesives by microtensile bond strength testing (microTBS), Fe-SEM and TEM when compared to a control two-step self-etch and a three-step etch-and-rinse adhesive. The one-step self-etch adhesive, Adper Prompt (3M ESPE), scored the lowest microTBS of all experimental and control adhesives tested. Conversely, the two-step self-etch adhesives Clearfil SE (Kuraray) and OptiBond Solo Plus Self-Etch (Kerr) approached the values obtained by the three-step etch-and-rinse control (OptiBond FL, Kerr) when bonded to enamel and dentin. Ultramorphological characterization showed that interfacial morphology and the pH of the self-etch primer/adhesive are strongly associated. The interaction with dentin varied from the formation of a submicron, hydroxyapatite-containing hybrid layer for the "mild" self-etch adhesive Clearfil SE to a 3-5 microm thick, hydroxyapatite-depleted hybrid layer for the "strong" self-etch adhesive Adper Prompt. The two-step self-etch adhesives AdheSE and OptiBond Solo Plus Self-Etch presented with a hybrid layer with a hydroxyapatite-depleted top part and a hydroxyapatite-containing base part and were therefore classified into a new group of self-etch adhesives, namely "intermediary strong" self-etch adhesives.

Acid Etching, Dental↗