Failure of Dacron prostheses caused by structural defect.

Intrinsic prosthetic failure is quite uncommon since the advent of Dacron prostheses. Only 24 cases of arterial prosthetic failure have been described in the literature. Our experience consists of two additional failures of knitted Dacron prostheses. The first patient developed aortojejunal fistula due to a defect of the aortic prosthesis 6 years after resection and replacement of an abdominal aortic aneurysm. The analysis of the graft revealed a defect in the form of a dropped stitch, which caused a weak spot where the prosthesis was able to be torn apart longitudinally. The second patient had femoropopliteal bypass and 6 years later developed degeneration with aneurysmal formation of the entire length of the prosthesis. Optical microscopy of this prosthesis exhibited mostly transverse failures which were coincident with valleys of the corrugated prosthesis. This was indicative of a defect that rendered the corrugation root too weak to withstand normal arterial pressures. This presentation emphasizes the seldom and serious complication of prosthetic failure due to defect of the prosthetic material. Details of scanning electron microscopy of the prosthesis, clinical presentation, angiography, and pathological findings with treatment also are discussed.

Aorta, Abdominal↗

A metallurgical examination of fractured stainless-steel ASIF tibial plates.

Between 1970 and 1973 99 tibial fractures were treated by rigid internal fixation with ASIF plates. The fractures were all regarded as sufficiently stable for exercise without weight bearing, thus needing no additional external support during the healing period. Four of the plates broke late in the healing period, after the onset of weight bearing. These fractures had some degree of delayed union with slight resorption of the bone ends, resulting in cyclical bending of the plate. Examination of 2 of the fractured plates by scanning electron microscopy, electron microprobe analysis and optical metallography revealed that the primary cause of plate fracture was fatigue. There was no evidence that corrosion fatigue or inclusion content were factors leading to plate fracture.

Adult↗