Isolation and characterization of UHMWPE wear particles down to ten nanometers in size from in vitro hip and knee joint simulators.

There is currently considerable interest in the wear debris and osteolytic potential of different types of bearings used in total joint replacements. The biological activity of the wear debris is dependent on the size and volume of the particles produced. Wear volume also plays an important role in the functional biological activity of a joint replacement. In vitro studies have shown that crosslinking of ultra high molecular weight polyethylene (UHMWPE) acetabular cups and tibial trays produces a reduction in wear volume, and crosslinking has now been introduced clinically for both types of prostheses. Previous studies have identified both micron and submicron-sized polyethylene wear particles. The aim of this study was to characterize the wear and wear particles generated from moderately crosslinked GUR 1,020 GVF UHMWPE acetabular cups and tibial trays in hip and knee joint wear simulators down to 10 nanometers in size. The wear rates of the two prosthesis types were very similar at 25.6 +/- 5.3 mm(3) per million cycles for the hip prostheses and 22.75 +/- 5.95 mm(3) per million cycles for the knee prostheses. Nanometer-sized wear particles were isolated and characterized from both hip and knee simulator lubricants for the first time. Significantly higher numbers (p < 0.05) of particles in the nanometer (<0.1 microm) size range were produced by the hip prostheses compared to the knee prostheses. The knee prostheses produced larger particles, with the mode of particle size in the 0.1-1.0 microm size range, compared to <0.1 microm size range for the hip prostheses. In addition, the knee prostheses produced a greater volumetric concentration of wear particles in the 1.0-10 microm size range, and consequently lower specific biological activity and functional biological activity indices. These results indicated that the knee prostheses had a lower osteolytic potential compared to the hip prostheses.

Biocompatible Materials↗

The influence of design, materials and kinematics on the in vitro wear of total knee replacements.

Debris-induced osteolysis due to surface wear of ultra high molecular weight polyethylene (UHMWPE) bearings is a potential long-term failure mechanism of total knee replacements (TKR). This study investigated the effect of prosthesis design, kinematics and bearing material on the wear of UHMWPE bearings using a physiological knee simulator. The use of a curved fixed bearing design with stabilised polyethylene bearings reduced wear in comparison to more flat-on-flat components which were sterilised by gamma irradiation in air. Medium levels of crosslinking further improved the wear resistance of fixed bearing TKR due to resistance to strain softening when subjected to multidirectional motion at the femoral-insert articulating interface. Backside motion was shown to be a contributing factor to the overall rate of UHMWPE wear in fixed bearing components. Wear of fixed bearing prostheses was reduced significantly when anterior-posterior displacement and internal-external rotation kinematics were reduced due to decreased cross shear on the articulating surface and a reduction in AP displacement. Rotating platform mobile bearing prostheses exhibited reduced wear rates in comparison to fixed bearing components in these simulator studies due to redistribution of knee motion to two articulating interfaces with more linear motions at each interface. This was observed in two rotating platform designs with different UHMWPE bearing materials. In knee simulator studies, wear of TKR bearings was dependent on kinematics at the articulating surfaces and the prosthesis design, as well as the type of material.

Biocompatible Materials↗

Blood ordering protocol based on proposed surgical implant in fractured neck of femur patients.

INTRODUCTION: Fractured neck of femur patients frequently require blood transfusion. To improve the efficiency of blood ordering, we present a protocol which orders blood specific for the proposed surgical implant. PATIENTS AND METHODS: A retrospective audit over a 1-year period was performed. Patients were divided into six groups dependent on proposed surgical implant. The mean postoperative drop in haemoglobin concentration, the cross-match to transfusion ratio and transfusion indexes were calculated. RESULTS: Statistically significant differences in blood loss were found dependent on implant used. Using guidelines created by the British Committee for Standards in Haematology on the implementation of a maximum surgical blood ordering schedule, a new protocol for blood ordering based on proposed surgical implant was created. CONCLUSIONS: In fractured neck of femur patients awaiting operation, the type of implant can be used to anticipate blood loss and as a guide to blood ordering.

Analysis of Variance↗

Influences of sterilising techniques on polyethylene wear.

Over the last 10 years there has been increasing concern over wear of polyethylene and osteolytic potential in the knee. During this period there have been considerable developments in both the design, materials and sterilisation techniques used for polyethylene in the knee. This paper reviews wear performance of polyethylene sterilised by different techniques, under a range of kinematics conditions in a single knee joint simulator system. Reducations in polyethylene wear were found with both stabilised polyethylene and cross-linked polyethylene, and with rotating platform mobile bearing designs.

Biomechanical Phenomena↗

Wear of surface engineered metal-on-metal hip prostheses.

The wear of existing metal-on-metal (MOM) hip prostheses (1 mm3/million cycles) is much lower than the more widely used polyethylene-on-metal bearings (30-100 mm3/million cycles). However, there remain some potential concerns about the toxicity of metal wear particles and elevated metal ion levels, both locally and systemically in the human body. The aim of this study was to investigate the wear, wear debris and ion release of fully coated surface engineered MOM bearings for hip prostheses. Using a physiological anatomical hip joint simulator, five different bearing systems involving three thick (8-12 microm) coatings, TiN, CrN and CrCN, and one thin (2 microm) coating diamond like carbon (DLC) were evaluated and compared to a clinically used MOM cobalt chrome alloy bearing couple. The overall wear rates of the surface engineered prostheses were at least 18-fold lower than the traditional MOM prostheses after 2 million cycles and 36-fold lower after 5 million cycles. Consequently, the volume of wear debris and the ion levels in the lubricants were substantially lower. These parameters were also much lower than in half coated (femoral heads only) systems that have been reported previously. The extremely low volume of wear debris and concentration of metal ions released by these surface engineered systems, especially with CrN and CrCN coatings, have considerable potential for the clinical application of this technology.

Biomedical Engineering↗

Total hip arthroplasty using the Wroblewski golf ball cup inserted through the posterior approach. A high rate of dislocation.

The Wroblewski golf ball acetabular cup was introduced by surgeons using the trochanteric osteotomy approach for revision total hip replacement (THR) in order to reduce the rate of dislocation. We have routinely used the Ogee long posterior wall (Ogee LPW) and the Wroblewski angle bore cups in THR. Although the new Wroblewski golf ball cup performed well there was a significant early rate of dislocation of 20%. Our rate of dislocation over a period of ten years using the Ogee LPW and Wroblewski angle bore cups had been 0.52%. We present our findings and an investigation as to why the new cup has such a high rate of dislocation when used with the posterior approach. We show that a relatively small change in the design of the acetabular component resulted in significant adverse clinical results.

Adolescent↗

Comparison of the cytotoxicity of clinically relevant cobalt-chromium and alumina ceramic wear particles in vitro.

Concern over polyethylene wear particle induced aseptic loosening of metal-on-polyethylene hip prostheses has led to renewed interest in alternative materials such as metal-on-metal and alumina ceramic-on-alumina ceramic for total hip replacement. This study compared the effects of clinically relevant cobalt-chromium and alumina ceramic wear particles on the viability of U937 histiocytes and L929 fibroblasts in vitro. Clinically relevant cobalt-chromium wear particles were generated using a flat pin-on-plate tribometer. The mean size of the clinically relevant metal particles was 29.5+/-6.3 nm (range 5-200 nm). Clinically relevant alumina ceramic particles were generated in the Leeds MkII anatomical hip simulator from a Mittelmieier prosthesis using micro-separation motion. This produced particles with a bimodal size distribution. The majority (98%) of the clinically relevant alumina ceramic wear debris was 5-20 nm in size. The cytotoxicity of the clinically relevant wear particles was compared to commercially available cobalt-chromium (9.87 microm+/-5.67) and alumina ceramic (0.503+/-0.19 microm) particles. The effects of the particles on the cells over a 5 day period at different particle volume (microm(3)) to cell number ratios were tested and viability determined using ATP-Lite(TM). Clinically relevant cobalt-chromium particles 50 and 5 microm(3) per cell reduced the viability of U937 cells by 97% and 42% and reduced the viability of L929 cells by 95% and 73%, respectively. At 50 microm(3) per cell, the clinically relevant ceramic particles reduced U937 cell viability by 18%. None of the other concentrations of the clinically relevant particles were toxic. The commercial cobalt-chromium and alumina particles did not affect the viability of either the U937 histiocytes or the L929 fibroblasts.Thus at equivalent particle volumes the clinically relevant cobalt-chromium particles were more toxic then the alumina ceramic particles. This study has emphasised the fact that the nature, size and volume of particles are important in assessing biological effects of wear debris on cells in vitro.

Aluminum↗

In vitro analysis of the wear, wear debris and biological activity of surface-engineered coatings for use in metal-on-metal total hip replacements.

Extremely low wear rates have been reported for metal-on-metal total hip replacements, but concerns remain about the effects of metal ion release, dissolution rates and toxicity. Surface-engineered coatings have the potential to improve wear resistance and reduce the biological activity of the wear debris produced. The aim of this study was to examine the wear and wear debris generation from surface-engineered coatings: titanium nitride (TiN), chromium nitride (CrN) and chromium carbon nitride (CrCN) applied to a cobalt-chrome alloy (CoCr) substrate. The coatings were articulated against themselves in a simple geometry model. The wear particles generated were characterized and the cytotoxic effect on U937 macrophages and L929 fibroblasts assessed. The CrN and CrCN coatings showed a decrease in wear compared to the CoCr bearings and produced small (less than 40 nm in length) wear particles. The wear particles released from the surface engineered bearings also showed a decreased cytotoxic effect on cells compared to the CoCr alloy debris. The reduced wear volumes coupled with the reduced cytotoxicity per unit volume of wear indicate the potential for the clinical application of this technology.

Cell Survival↗

Prediction of violent recidivism.

OBJECTIVE: To describe the changes and improvements in accuracy of the prediction of violent recidivism. METHOD: The evolution of better prediction models is described by reviewing the more significant methods used and referring to the results of their application. RESULTS: Development of instruments such as the Psychopathy Checklist-Revised, the Violence Risk Assessment Guide (VRAG), the HCR-20 and the multiple-item comprehensive questionnaire of Monahan and Steadman has substantially improved accuracy in risk assessment. The presence of full-blown psychopathy has proven itself a better predictor of violence than has a diagnosis of antisocial personality disorder according to the Diagnostic and Statistical Manual (DSW-IV). Shortcomings to the efficacy of the current instruments stem from the difficulty in detecting violence-proneness in persons who eventually assault or murder one or two persons (usually family members), but who have no, or a limited, record of past violence. Persons from affluent backgrounds are more adept at evading arrests or convictions than are the poor. Adolescent sons abused by parents are at risk to commit violent acts later on, but the community has little power to detect or intervene until these acts are committed. CONCLUSION: Prediction of violence has significantly improved over the last 20 years, thanks to the development of objective instruments of risk assessment.

Antisocial Personality Disorder↗

Investigation of wear of knee prostheses in a new displacement/force-controlled simulator.

The performance of two knee simulators designed by ProSim (Manchester, UK) was evaluated by comparison of the wear seen in the press-fit condylar (PFC) Sigma (DePuy) knee prosthesis. Twelve specimens of the same design and manufacturing specification, were subjected to a wear test of 2 x 10(6) cycles duration using bovine serum as a lubricant. The anterior/posterior displacement and internal/external rotation inputs were based on the kinematics of the natural knee. International Standards Organization (ISO) standards were used for the flexion and axial load. The wear rates and wear scar areas were compared across all stations. The mean wear rates found were 17.6+/-5 mm3/10(6) cycles for stations 1 to 6 and 19.6+/-4 mm3/10(6) cycles for stations 7 to 12, resulting in an overall mean wear rate of 18.1+/-3 mm3/10(6) cycles. The differences between the two simulators were not significant. The average wear scar area seen on inserts from stations I to 6 was calculated at 32.4+/-1 per cent of the intended articulating surface. Similarly on stations 7 to 12 the average wear scar area was 30.7+/-3 per cent. The wear scars seen were a good physiological representation of those found from clinical explant data. This study has shown good repeatability from the simulator, both within and between the simulators.

Arthroplasty, Replacement, Knee↗

Comparison of wear, wear debris and functional biological activity of moderately crosslinked and non-crosslinked polyethylenes in hip prostheses.

The wear, wear debris and functional biological activity of non-crosslinked and moderately crosslinked ultrahigh molecular weight polyethylene (UHMWPE) acetabular cups have been com pared when articulating against smooth and intentionally scratched femoral heads. Volumetric wear rates were determined in a hip joint simulator and the debris was isolated from the lubricant and characterized by the percentage number and volumetric concentration as a function of particle size. The volumetric concentration was integrated with the biological activity function determined from in vitro cell culture studies to predict an index of specific biological activity (SBA). The product of specific biological activity and volumetric wear rate was used to determine the index of functional biological activity (FBA). On smooth femoral heads the crosslinked UHMWPE had a 30 per cent lower wear rate, but it had a greater percentage volume of smaller, more biologically active particles, which resulted in a similar index of FBA compared with the non-crosslinked material. On the scratched femoral heads the volumetric wear rate was three times higher for the moderately crosslinked UHMWPE and two times higher for the non-crosslinked UHMWPE compared with the smooth femoral heads. This resulted in a higher wear rate for the moderately crosslinked material on the scratched femoral heads. All the differences in wear rate were statistically significant. There were only small differences in particle volume concentration distributions, and this resulted in similar indices of FBA which were approximately twice the values of those found on the smooth femoral heads. Both materials showed lower wear and FBA than for previously studied aged and oxidized UHMWPE gamma irradiated in air. However, this study did not reveal any advantage in terms of predicted FBA for moderately crosslinked UHMWPE compared with non-crosslinked UHMWPE.

Acetylene↗

An in vitro study of the reduction in wear of metal-on-metal hip prostheses using surface-engineered femoral heads.

Although the wear of existing metal-on-metal (MOM) hip prostheses (1 mm3/10(6) cycles) is much lower than the more widely used polyethylene-on-metal bearings, there are concerns about the toxicity of metal wear particles and elevated metal ion levels, both locally and systemically, in the human body. The aim of this study was to investigate the possibility of reducing the volume of wear, the concentration of metal debris and the level of metal ion release through using surface-engineered femoral heads. Three thick (8-12 microm) coatings (TiN, CrN and CrCN) and one thin (2 microm) coating (diamond-like carbon, DLC), were evaluated on the femoral heads when articulating against high carbon content cobalt-chromium alloy acetabular inserts (HC CoCrMo) and compared with a clinically used MOM cobalt-chromium alloy bearing couple using a physiological anatomical hip joint simulator (Leeds Mark II). This study showed that CrN, CrCN and DLC coatings produced substantially lower wear volumes for both the coated femoral heads and the HC CoCrMo inserts. The TiN coating itself had little wear, but it caused relatively high wear of the HC CoCrMo inserts compared with the other coatings. The majority of the wear debris for all half-coated couples comprised small, 30 nm or less, CoCrMo metal particles. The Co, Cr and Mo ion concentrations released from the bearing couples of CrN-, CrCN- and DLC-coated heads articulating against HC CoCrMo inserts were at least 7 times lower than those released from the clinical MOM prostheses. These surface-engineered femoral heads articulating on HC CoCrMo acetabular inserts produced significantly lower wear volumes and rates, and hence lower volumetric concentrations of wear particles, compared with the clinical MOM prosthesis. The substantially lower ion concentration released by these surface-engineered components provides important evidence to support the clinical application of this technology.

Carbon↗

Quantitative analysis of UHMWPE wear debris isolated from the periprosthetic femoral tissues from a series of Charnley total hip arthroplasties.

Submicrometer and micrometer-sized UHMWPE wear particles have been associated with osteolysis and failure of total hip replacements. A previous study by Tipper et al. examined the wear debris isolated from the acetabular periprosthetic tissues from 18 Charnley total hip replacements, and compared this data to the tribological variables of the prostheses. The present study aimed to isolate the UHMWPE wear debris from the femoral periprosthetic tissues from 10 of the same cohort of patients, and compare it with the debris isolated from the corresponding acetabular tissues. A variety of particle morphologies were observed, discrete submicrometer particles, along with flakes and fibrils. The particle size distributions ranged from 0.1 to >250 microm, however, the largest particles were only found in samples when the femoral head damage was characterised as low (R(pm) < 0.2 microm). The mode of the frequency distribution of particles was in the range of 0.1-0.5 microm for all the femoral tissues. Considerable variations were found in the mass distributions of the wear particles as a function of size for different patients. The net mass of debris isolated from the femoral tissues was significantly lower (p < 0.05, Student's t-test) than from the corresponding acetabular tissues. This along with considerable spatial variation in the net mass of debris isolated from the different regions of the same sample of acetabular tissue, indicates that the transportation of the debris has a marked effect on the net mass of debris accumulated in different tissues.

Acetabulum↗

Quantitative characterization of polyethylene debris isolated from periprosthetic tissue in early failure knee implants and early and late failure Charnley hip implants.

This study isolated and characterized UHMWPE particles from 3 explant groups: early Charnley hip failures (ECE; < 10 years), late Charnley hip failures (LCE; > 10 years) and early knee failures (EKE; < 10 years). Debris isolated from the 3 groups had percentage particle number and percentage volumetric concentration distributions that were not significantly different. The greatest number of particles were found in the 0.1-0.5 microm size range and 19-20.6% of the volumetric concentration was below 1 microm in size in all groups. However, there were significant differences in the total volumetric concentration of debris isolated per g of tissue. LCE had significantly higher volumes of debris than ECE and EKE, there was no significant difference in the volume of debris from the EKE and ECE. The mean aspect ratio and mean irregularity ratio of the LCE group were also significantly higher than the ECE and EKE, suggesting that different wear mechanisms were occurring in the late Charnley group compared to the early Charnley and knee groups. These results also suggest that early knees, with normal surface wear, may have similar wear mechanisms to early Charnley hips and indicate that similar volumes of biologically active micrometer and sub-micrometer UHMWPE particles were produced. This may have important implications in the longer-term outcome of total knee arthroplasties, because it indicates a similar potential for osteolysis induced by wear debris.

Aged↗

A novel low wearing differential hardness, ceramic-on-metal hip joint prosthesis.

Osteolysis and loosening of artificial joints caused by polyethylene wear debris has prompted renewed interest in alternative bearing materials for hip prosthesis designs. Lower wearing metal-on-metal (MOM) and ceramic-on-ceramic prostheses are being used more extensively, and there is considerable interest in further improving on their performance. This study investigated the wear properties and debris morphology of a novel differential hardness ceramic-on-metal (COM) prosthesis, in comparison with MOM articulations in a physiological anatomical hip joint simulator. The COM pairings were found to have wear rates approximately 100-fold lower than the MOM pairings. The MOM pairings showed a higher "bedding in" wear rate (3.09+/-0.46mm(3)/10(6) cycles) in the first million cycles, which then reduced to a steady state wear rate of 1.23+/-0.5mm(3)/10(6) cycles. The wear rate of the COM pairings over the duration of the test was approximately 0.01mm(3)/10(6) cycles with very little wear detected on the surface of the prosthesis components. The wear particles from both articulations were oval to round in shape and in the nanometer size range. After one million cycles the mean maximum diameter of the MOM and COM wear particles were 30+/-2.25 and 17.57+/-1.37nm, respectively. After five million cycles the wear particles were statistically significantly smaller than at one million cycles, 13.9+/-0.72nm for the MOM pairings and 6.11+/-0.40nm for the COM pairings. The wear rates of the MOM prostheses were representative of clinical values. The use of differential hardness COM pairings dramatically reduced the wear rate compared to MOM hip prostheses. The wear particles from the MOM articulation were similar to particles found in retrieved tissues from around MOM prostheses. The extremely low wearing differential hardness COM bearings presented in this study produced far smaller volumetric particle loads compared to MOM prostheses currently used clinically.

Biocompatible Materials↗

Comparison of the response of three human monocytic cell lines to challenge with polyethylene particles of known size and dose.

The response of three human monocytic cell lines (Monomac-1, U937 and THP-1) to challenge with polyethylene particles of known size and dose was evaluated. Particles with a mean size of 0.21, 0.49, 4.3, 7.2, and 88 microm were co-cultured with the cells for 24 hours prior to the assessment of cell viability and production of the pro-inflammatory cytokines, IL-1beta, IL-6 and TNFalpha. Additionally, GM-CSF and prostaglandin E2 were measured in culture supernatants from particle stimulated U937 cells. All particle fractions were evaluated at particle volume (microm3) to cell number ratios of 100 : 1, 10 : 1, 1 : 1 and 0.1 : 1. None of the test fractions had any effect on cell viability. Only the response of the U937 cell line was demonstrated to be comparable to that of primary macrophages as determined in a previous study. Furthermore only particle volume to cell number ratios of 10 : 1 or greater consistently stimulated significantly enhanced levels of cytokine secretion with particles within the phagocytosable size range (0.1 to 10 microm) being the most biologically active. No response was observed when U937 macrophages were stimulated with the largest (88 microm) particles at any of the volume ratios tested in this study. These results suggest that the size and volume of polyethylene particles are critical factors in macrophage activation. In addition, the U937 cell line has been shown to be a suitable model for the in vitro study of macrophage-particle interactions.

Journal Article↗

Comparative study of the activity of total hip arthroplasty patients and normal subjects.

The walking activity of normal subjects and total hip arthroplasty (THA) patients from the Wrightington Hospital for Joint Disease and The General Infirmary at Leeds was assessed by means of electronic pedometers. The principal objectives were to establish the extent to which joint arthroplasty patients recover their activity relative to normal subjects and to establish the number of loading cycles to which prostheses should be subjected in joint simulator studies of implant performance. A further objective was to establish an experimental procedure for the assessment of the role of activity in contributing to the well-known scatter in the measurements of femoral head penetration into acetabular cups in in vivo studies of implant performance. The last-mentioned issue is addressed in another article ([1]). The walking activity of 2 normal subjects of disparate ages was assessed during 1 full year. It was concluded that fair estimates of activity could be achieved by recording pedometer readings during successive 2- to 4-week periods. This approach was adopted in the full assessment of the walking activity of cohorts of normal subjects and THA patients. Linear regression expressions relating the number of steps taken daily and the annual number of loading cycles on each leg to age are presented for normal subjects and THA patients. In all cases, activity declines with age, but it is shown that total joint arthroplasty is not at all restrictive on walking activity-a remarkable testimony to the efficacy of total joint arthroplasty. Attention is drawn, however, to different levels of activity of THA patients recorded in the present United Kingdom study and a similar survey conducted in California.

Activities of Daily Living↗

Comparison of weight changes after total hip or knee arthroplasty.

A prospective study of the effect on weight in 192 patients after total hip arthroplasty (THA) (124 hips) or total knee arthroplasty (TKA) (68 knees) was performed. Patients' weights at 1 year after THA or TKA were compared with their preoperative weights. There was little or no effect on a patient's weight after TKA. Women undergoing THA gained on average 3.1 kg (6.8 lb), whereas men gained on average 2.5 kg (5.5 lb). This information may be of benefit to a surgeon whose patient needs encouragement to lose weight before undergoing a THA.