[A study on the color difference between Au-Pt alloy porcelain and Ni-Cr alloy porcelain].

OBJECTIVE: To investigate the color difference between Au-Pt alloy porcelain and Ni-Cr alloy porcelain. METHODS: 30 metal-ceramic specimens with different dentin porcelain thickness were fabricated with two types of metal-ceramic alloy, each type of alloy had 15 specimens. L*, a*, b* were measured after opaque porcelain was applied, and dentin porcelain was fired 1, 3, 5, 7 times by MINOLTA CR-100. Then delta E was calculated which reflected the color difference between high-gold alloy porcelain and Ni-Cr alloy porcelain. RESULTS: Comparing with Ni-Cr alloy porcelain, the color of Au-Pt alloy porcelain was reddish, yellowish and less bright. The delta E between high-gold alloy porcelain and Ni-Cr alloy porcelain in shade A2 was largest when opaque porcelain was applied. It decreased when dentin porcelain was applied. It became smallest when fired 3 times, and increased along with the increase of fire times. It was larger than 1.5 except firing 3 times. When dentin porcelain was applied, delta E which was larger than 1.5 among different dentin porcelain thickness decreased along with the increase of dentin porcelain thickness. CONCLUSION: The color difference between the two types of metal-ceramic alloy should be carefully taken into account in order to improve the quality of color matching.

Chromium↗

[Three-dimensional finite element stress analysis of different designs of shape in all-ceramic crowns].

OBJECTIVE: The purpose of this study was to examine the effect of different occlusal thickness on the stress distribution of all-ceramic crowns of the mandibular first molar. METHODS: Three-dimensional finite element analysis was made. RESULTS: It was found that under the simulated applied loads, the values of tensile and shear stress varied with the occlusal thickness, and much greater values of such stresses were noticed in the all-ceramic crowns 1.0 mm in occlusal thickness, compared with those in the crowns 1.5 mm and 2.0 mm in occlusal thickness. CONCLUSION: These results could serve as a theoretic foundation for the clinical application of all-ceramic crown, suggesting that the occlusal thickness of the crown should not be lower than 1.5 mm in order that the resistance of the all-ceramic crown against fracture might be strengthened.

Ceramics↗

[Study on color masking ability of restoration material Vita Mark II].

OBJECTIVE: The purpose of this study was to evaluate the color masking ability of Computer Aided Design/Computer Aided Manufacture(CAD/CAM) machining ceramic Vita Mark II, this ability was affected by thickness and shade. METHODS: Each of 5 specimens of 0.5 mm, 1.0 mm and 1.5 mm Vita Mark II A3C/18 and A2C/18 were prepared and the color change was measured after the substrate simulating stained teeth was covered with the specimen. RESULTS: Statistically significant differences (P < 0.01) were recorded in the substrates covered with different thickness and shade of Vita Mark II. The color changes (delta E) were 15.181, 17.691, 19.667 and 15.653, 16.880, 18.002 after the substrates were covered with 0.5 mm, 1.0 mm and 1.5 mm Vita Mark II A3C/18 and A2C/18. CONCLUSION: As a dental material, CAD/CAM Vita Mark II has high quality to mask the underlying color. Being a veneer, the masking ability with A2C/18 is better than that with A3C/18, but being an inlay, the result is reverse.

Color↗

[Expression of IL-6 and it's mRNA transcription in the process of rat periodontium remodeling influenced by various bite forces].

OBJECTIVE: To study the expression of IL-6 in periodontal ligament fibroblasts (PLF) and osteoblasts in order to explain the molecular mechanism of the bite forte on periodontium remodeling. METHODS: A rat model of different bite forces was established to study the expression of IL-6 and IL-6 mRNA in the PLF and osteoblasts with immunohistochemical (IHC) and in situ hybridization (ISH) techniques. RESULTS: In the group of disuse bite force, the expression of IL-6 and IL-6 mRNA in the PLF and osteoblasts enhanced apparently compared with that in the group of normal bite force. The gray level values enhanced respectively from 6.5886 +/- 1.6 to 38.8381 +/- 9.5 and from 11.8337 +/- 2.8 to 57.2623 +/- 13.6. The loosely arrangement of periodontal fibers and the resorption of alveolar bone were observed in histological study. In the group of compensation bite force, the same result was observed with IHC and ISH, the gray level values enhanced respectively from 6.3119 +/- 1.5 to 45.5456 +/- 11.1 and from 11.7714 +/- 2.8 to 81.9391 +/- 19.5, but the increase of periodontal fibers, the resorption and formation of alveolar bone were observed simultaneity in histological study. CONCLUSIONS: With the change of bite force, the expression of IL-6 and IL-6 mRNA in PLF and osteoblasts presents a certain regulation. IL-6 may play important roles in the effect of bite force on periodontium remodeling.

Animals↗

Effect of layering feldspathic porcelain on resulting veneer color with aluminum oxide core.

OBJECTIVE: To evaluate the resulting color of veneers affected by adding a layer of veneering porcelain on Procera aluminium oxide core. METHODS: Fifteen aluminium oxide disks were randomized into three groups. Each of five disks was veneered with porcelain of the Vita shade Al, A2 and B4 respectively. The color of the substrate covered with non-veneered disks and the veneered disks was measured separately and the color differences were calculated. RESULTS: Statistically significant differences (P < 0.01) in color coordinates of dark substrate were recorded between the substrate covered by an aluminium oxide disks and the addition of veneering porcelain to aluminium oxide disks. Mean coordinates color difference (DeltaE, DeltaL *, Deltaa *, Deltab *) after adding the three shades of veneering porcelain showed increase from Al (2.311) to A2 (4.313) to B4 (8.778) in DeltaE, decrease from Al (-1.530) to A2 (-3.369) and B4 (-3.358) in DeltaL *, and increase from Al (-1.440) to A2 (2.198) to B4 (7.955) in Deltab *. The direction of the color modification correlated with values obtained from the liberation. The resulting color was also affected by the color of the underlying structure. CONCLUSION: This study illustrates that color of aluminium oxide shell could be modified with feldspathic veneering porcelain, which may be used by practitioners to alter the esthetic outcome of porcelain veneers.

Aluminum Oxide↗

[The preparation procedure of TiAdapt abutment effect on the implant to abutment joint stability].

OBJECTIVE: This study was designed to determine the difference in the implant to abutment joint stability resulting from the preparation procedure in adjusting the TiAdapt abutment. METHODS: Thirty Branemark implants (10RP, 10NP, 10WP) and 10 TiAdapt RP, TiAdapt NP and TiAdapt WP abutments formed the experimental populations of 3 groups. Samples in each groups were further divided into subgroups A and B. Subgroup A was operated with preparation procedure whereas the other served as control. The torque required and the gap between abutment and implant before and after preparation were measured. RESULTS: There were no significant differences in group RP and group WP; there were significant differences in group NP at the significance level of 0.05. CONCLUSION: These results indicate that the implant to abutment joint stability has been strengthened by the abutment preparation procedure.

Dental Abutments↗

[Comparison of machinability of two types of dental machinable ceramic].

OBJECTIVE: In terms of the problems of now available dental machinable ceramics, a new type of calcium-mica glass-ceramic, PMC-I ceramic, was developed, and its machinability was compared with that of Vita MKII quantitatively. Moreover, the relationship between the strength and the machinability of PMC-I ceramic was studied. METHODS: Samples of PMC-I ceramic were divided into four groups according to their nucleation procedures. 600-seconds drilling tests were conducted with high-speed steel tools (Phi = 2.3 mm) to measure the drilling depths of Vita MKII ceramic and PMC-I ceramic, while constant drilling speed of 600 rpm and constant axial load of 39.2 N were used. And the 3-point bending strength of the four groups of PMC-I ceramic were recorded. RESULTS: Drilling depth of Vita MKII was 0.71 mm, while the depths of the four groups of PMC-I ceramic were 0.88 mm, 1.40 mm, 0.40 mm and 0.90 mm, respectively. Group B of PMC-I ceramic showed the largest depth of 1.40 mm and was statistically different from other groups and Vita MKII. And the strength of the four groups of PMC-I ceramic were 137.7, 210.2, 118.0 and 106.0 MPa, respectively. CONCLUSION: The machinability of the new developed dental machinable ceramic of PMC-I could meet the need of the clinic.

Dental Porcelain↗

Enhanced anti-B-cell tumor effects with anti-CD20 superantibody.

The data presented here describe a novel approach to enhance the use of antibodies in diagnostic and therapeutic applications. Using a peptide copied from a rare self-binding (autophilic) antibody structure, the authors were able to convert by chemical cross-linking an anti-CD20 antibody to a self-binding (autophilic) structure. The autophilic antibody exhibited better binding to target tumor cells than the naked antibody. By the mechanism of hyper-cross-linking a B-cell receptor (CD20) on tumor cells, the rate of apoptosis is significantly increased, leading to strong inhibition of tumor growth in culture. The demonstration of enhanced binding and apoptosis targeting the CD20 B-cell marker serves as an example for developing second-generation therapeutic antibodies against non-Hodgkin lymphoma.

Amino Acid Sequence↗

Enhancing tumor targeting and apoptosis using noncovalent antibody homodimers.

A rare type of antibody that spontaneously binds to each self (homodimerizes) has been described. This self-binding (autophilic) antibody provides stronger protection against bacterial infection than a non self-binding antibody with identical specificity and affinity due to increase of polymeric avidity. A peptide derived from the self-binding domain of the autophilic antibody was crosslinked to the Fc carbohydrate of two monoclonal antibodies specific for the B-cell receptor (BCR) of a murine and a human B-cell tumor. Peptide-crosslinked antibodies bind to themselves on solid phase ELISA as homodimer and establish in solution a monomer-dimer equilibrium. Autophilic antibodies bind to their respective tumor target cells with increased efficiency as determined by FACS analysis. They also induce twice the amount of apoptosis of target tumor cells than the control antibodies. Furthermore, the modified antibodies inhibit tumor growth in culture more efficiently than the control antibodies. Criss-cross protocols in FACS, apoptosis, and growth inhibition indicate the specificity of targeting the BCR with autophilic antitumor antibodies. The chemical approach of increasing the binding of antibodies without creating chemically crosslinked dimers mimics naturally occurring autophilic antibodies and represents a simple and attractive alternative to chemical dimerizing and antibody engineering techniques for improving their antitumor effect. Furthermore, these results provide a guide to incorporate the self-binding peptide into the structure of antibodies using modeling and molecular crafting techniques.

Animals↗