PubMed Health⌕ Search

Biomedical subjects

Zoltan Rethy

Publications and source records attributed to Zoltan Rethy.

2 recordsLinked to original sources

Release dynamic process identification for a cement based material in various leaching conditions. Part II. Modelling the release dynamics for different leaching conditions.

This paper deals with process identification and model development for the case of a porous reference material leaching under certain hydrodynamic conditions. Four different dynamic leaching tests have been applied in order to take into account different types of solid/liquid contact conditions corresponding to various real leaching scenarios: monolithic and granular material with sequential eluate renewal, and granular material and continuously renewed eluate with different hydrodynamic conditions (dispersion, residence time). A coupled chemical-mass transfer model has been developed to describe the leaching behaviour under all experimental conditions. Diffusion has been considered as the mass transport mechanism inside the saturated porous material and dispersive convection as that in the leachate. Two specific phenomena have been identified and considered in the model: (i) the early surface dissolution of the material which results in high Ca concentration and (ii) the late weak dissolution of Na and K giving rise to a long-term residual release. The intrinsic material parameters such as the initial concentrations in the pore water and solid phases were determined by applying equilibrium leaching tests and geochemical modelling. Diffusion coefficients for different elements and the late solubility of alkalines have been found to reach the same values in the four tests. The estimated values of the surface dissolution kinetic constant have shown a dependence on leachate hydrodynamics when the thickness of the degraded layer is nearly the same in the four tests (intrinsic parameter of the material). The competition between the four main dynamic processes, i.e. diffusion, convection, late dissolution, and surface dissolution, has been emphasized and compared in the four leaching tests: the hydrodynamic dispersion and the residence time had no effect on the leaching behaviour of alkalines, which is controlled by diffusion, whereas the behaviour of calcium (a major element of the material) was strongly influenced. This has significant effects on eluate pH values and on the concentration of Pb (the monitored pollutant). The model was then applied to simulate a landfill scenario in the case of a stabilized/solidified incinerator residue containing heavy metals and chloride. A high rain infiltration level and the use of small blocs are favourable conditions for enhanced pollutant release.

Construction Materials↗

Release dynamic process identification for a cement based material in various leaching conditions. Part I. Influence of leaching conditions on the release amount.

In this paper we investigate at laboratory scale the influence of the liquid/solid leaching conditions on the release of different chemical species from a reference porous material obtained by solidification of PbO and CdO with Portland cement. The pH influence on the dissolution of pollutants and the initial pore solution composition (target elements: Na(+), K(+), Ca(2+), Pb(2+), Cd(2+), SO(4)(2-)) were assessed by applying a methodology consisting of two equilibrium leaching tests, the Acid Neutralization Capacity (ANC) and the Pore Water (PW) tests and geochemical modelling. Samples of the same material were submitted in parallel to four different dynamic leaching tests in order to determine the influence of the sample shape (monolithic or granular) and eluate hydrodynamics (instantaneous L/S ratio, eluate renewal) on the leaching of the target elements. The comparison criteria were the eluate saturation state, the cumulative release and the released flux. Generally, the eluates obtained in the tests applied on granular material were more concentrated, even saturated for the eluate pH value with respect to Ca(2+), Pb(2+) and SO(4)(2-). The consequence of the eluate saturation is the slowing down effect on the dynamic release. The highest released flux was observed for the Monolith Leaching Test (MLT) involving the highest instantaneous L/S ratio and the lowest solid/liquid exchange surface and for which no saturation was observed, except Pb(2+) and SO(4)(2-) in some eluates. The maximum cumulative released-mass was obtained for the Column Leaching Test (CLT) applied on granular material having the highest exchange surface, the lowest instantaneous L/S and a continuous input flow of the leachant. The experimental results demonstrate the significance of the liquid/solid contact type which is also a scenario specific parameter.

Calcium↗