Biodegradable polymeric matrices for bioartificial implants.

Abstract

Biomaterials made of polymers, metals or their alloys, ceramics and their composites, are used as implants to restore or to replace the damaged soft and hard tissue/organ functions for an intended time period. Biomaterials made of synthetic materials are very simple materials compared to their natural counterparts, they only replace very simple functions of the damaged tissue during healing. Natural tissues have been used for both soft and hard repair and replacement, but they do have serious limitations such as: shortage of donor tissue, donor site morbidity, unpredictable resorption characteristics, immunogenic response, risk of disease transmission, and ethical limitations. Tissue engineering is a relatively new approach, in which healthy mammalian cells are used with supporting matrices, usually made of either natural or synthetic polymers as composite bioartificial implants. Primary cells, especially embryonic stem cells, cell lines, hybridomas, genetically modified cells are considered as potential sources for this application. Both closed and open matrices are used as support matrices. Nondegradable and biocompatible microcapsules and hollow fibers are utilized in closed systems, especially for immunoprotection of the transplanted cells. Biodegradable polymers, both natural and synthetic are used in the preparation of bioartificial implants carrying only autogenic cells.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

E Pişkin. 2002. Biodegradable polymeric matrices for bioartificial implants.. https://doi.org/10.1177/039139880202500514

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related citations

Synthesis of gold functionalized poly-bisvinylethyleneurea/silica hybrid materials.

Novel gold/poly-(1,3-divinyl-imidazolid-2-one)/silica [poly-bisvinylethyleneurea (poly-BVU)/silica)] hybrid particles have been produced by adsorption and spontaneously occurring in situ reduction of Au(3+) cations on the surface of poly-BVU/silica hybrid particles. The successful functionalization of the poly-BVU/silica particles with gold nanoclusters has been evidenced by UV/vis and XPS spectroscopy as well as scanning electron microscopy. The size of the resulting gold clusters, estimated by means of the Mie-Drude theory on the full peak width at half-maximum of the surface plasmon UV/vis absorbance, correlates with the polymer content of the poly-BVU/silica hybrid particles used for the modification. Therefore, it is possible to control the size of the gold clusters simply by adjusting the monomer/silica ratio in the polymerization process, which corresponds with the polymer content of the hybrids.

Biocompatible Materials↗

Evaluation of thermal- and photo-crosslinked biodegradable poly(propylene fumarate)-based networks.

Biodegradable networks of poly(propylene fumarate) (PPF) and the crosslinking reagent poly(propylene fumarate)-diacrylate (PPF-DA) were prepared with thermal- and photo-initiator systems. Thermal-crosslinking was performed with benzoyl peroxide (BP), which is accelerated by N,N-dimethyl-p-toluidine (DMT) and enables injection and in situ polymerization. Photo-crosslinking was accomplished with bis(2,4,6-trimethylbenzoyl) phenylphosphine oxide (BAPO), which is activated by long-wavelength UV light and facilitates material processing with rapid manufacturing techniques, such as stereolithography. Networks were evaluated to assess the effects of the initiators and the PPF/PPF-DA double bond ratio on the mechanical properties. Regardless of the initiator system, the compressive properties of the PPF/PPF-DA networks increased as the double bond ratio decreased from 2 to 0.5. BAPO/UV-initiated networks were significantly stronger than those formed with BP/DMT. The compressive modulus of the photo- and thermal-crosslinked PPF/PPF-DA networks ranged from 310 +/- 25 to 1270 +/- 286 MPa and 75 +/- 8 to 332 +/- 89 MPa, respectively. The corresponding fracture strengths varied from 58 +/- 7 to 129 +/- 17 MPa and 31 +/- 13 to 105 +/- 12 MPa. The mechanical properties were not affected by the initiator concentration. Characterization of the network structures indicated that BAPO was a more efficient initiator for the crosslinking of PPF/PPF-DA, achieving a higher double bond conversion and crosslinking density than its BP counterpart. Estimated average molecular weights between crosslinks (Mc) confirmed the effects of the initiators and PPF/PPF-DA double bond ratio on the mechanical properties. This work demonstrates the capability to control the properties of PPF/PPF-DA networks as well as their versatility to be used as an injectable material or a prefabricated implant.

Biocompatible Materials↗

A biodegradable electrical bioconductor made of polypyrrole nanoparticle/poly(D,L-lactide) composite: A preliminary in vitro biostability study.

The electrical stability of a novel polypyrrole (PPy)/poly(D,L-lactide) (PDLLA) composite was studied in vitro and compared with that of PPy-coated polyester fabrics. Specimens were incubated in Ringer's solution at 37 degrees C for up to 8 weeks with or without the circulation of DC current under a constant 100 mV voltage. In situ current variation with incubation time was recorded. The AC volume electrical conductivity of the specimens before and after incubation in phosphate-buffered saline was recorded using a frequency analyzer. Water absorption and weight loss were monitored metrologically. Changes in the oxidation state of incubated PPy were analyzed with X-ray photoelectron spectroscopy. The morphological changes were observed with scanning electron microscopy, and the glass transition temperature of the PDLLA was investigated using differential scanning calorimetry. The PPy/PDLLA composite in Ringer's solution sustained a relatively stable conductivity up to 8 weeks after an initial period of "conditioning." The PPy-coated fabrics experienced a rapid loss of conductivity when subjected to electrical circulation and regained part of it when disconnected. The volume conductivity of the nonincubated PPy/PDLLA membrane behaved as a typical conductor in the low-frequency range. The mechanisms involved in the various electrical behaviours of the PPy/PDLLA composite and PPy-coated fabrics are discussed. In conclusion, the PPy/PDLLA composite was able to deliver a biologically significant electrical current in a simulated biological solution for up to 8 weeks and therefore may be considered as a first-generation synthetic biodegradable bioconductor.