PubMed Health⌕ Search

PubMed · 16440090

VideoAFM--a new tool for high speed surface analysis.

Abstract

The VideoAFM provides a 1000 fold increase in image rate compared to conventional atomic force microscopes, giving nanometre resolution images of surfaces at a rate of 15 frames s(-1), which is approximately 1 million pixels s(-1). Images of high stiffness surfaces such as calibration grids are provided for the first time, and allow for a more rigorous examination of the meaning of the data obtained with the VideoAFM. Instrumental changes that could provide true topographic images are discussed. The advantages of a high speed scanning technique that is integrated within a conventional AFM are outlined. Particular emphasis is given to the capability to 'tile' images, and hence rapidly map large areas with nanometre resolution. It is found that the inherent increase in stability that comes from a high frame rate leads to the possibility of manually manipulating the sample while maintaining a sharp image, allowing real-time user interaction with the AFM. The possible application of the VideoAFM approach for the very rapid analysis of surface properties and, ultimately, surface chemistry is discussed and some possible routes are given.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Jamie K Hobbs, Cvetelin Vasilev, Andrew D L Humphris. 2005-11-11. VideoAFM--a new tool for high speed surface analysis.. https://doi.org/10.1039/b511330j

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related citations

AFM fishing nanotechnology is the way to reverse the Avogadro number in proteomics.

Future development of proteomics may be hindered by limitations in the concentration sensitivity of widespread technological approaches. The concentration sensitivity limit (CSL) of currently used approaches, like 2-DE/LC separation coupled with MS detection, etc., varies from 10(-9) to 10(-12) M. Therefore, proteomic technologies enable detection of up to 20% of the protein species present in the plasma. New technologies, like atomic force microscopy (AFM molecular detector), enable the counting of single molecules, whereas biospecific fishing can be used to capture these molecules from the biomaterial. At the same time, fishing also has thermodynamic limitations due to the reversibility of the binding. In cases where the fishing becomes irreversible, its combination with an AFM detector enables the registration of single protein molecules, and that opens up a way to lower the CSL down to the reverse Avogadro number.

Microscopy, Atomic Force↗

Single molecule studies of protein folding using atomic force microscopy.

Atomic force microscopy (AFM) offers new insights into the ability of proteins to resist mechanical force. The technique has been opened up by the availability of easy-to-use instruments that are commercially available, so that the technique no longer relies on the need to build instruments in the lab. Indeed it may become common for AFM instruments to sit beside stopped-flow apparatus in protein folding laboratories. In this chapter, we describe the instrument set-up, the preparation of suitable protein substrate, and the collection of data. Data selection and analysis are more complex than for conventional stopped-flow ensemble studies, but offer new insights into the function of proteins in vivo.

Microscopy, Atomic Force↗

Deposition of DNA rafts on cationic SAMs on silicon [100].

We demonstrate a guided self-assembly approach to the fabrication of DNA nanostructures on silicon substrates. DNA oligonucleotides self-assemble into "rafts" 8 x 37 x 2 nm in size. The rafts bind to cationic SAMs on silicon wafers. Electron-beam lithography of a thin poly(methyl methacrylate) (PMMA) resist layer was used to define trenches, and (3-aminopropyl)triethoxysilane (APTES), a cationic SAM precursor, was deposited from aqueous solution onto the exposed silicon dioxide at the trench bottoms. The remaining PMMA can be cleanly stripped off with dichloromethane, leaving APTES layers 0.7-1.2 nm in thickness and 110 nm in width. DNA rafts bind selectively to the resulting APTES stripes. The coverage of DNA rafts on adjacent areas of silicon dioxide is 20 times lower than on the APTES stripes. The topographic features of the rafts, measured by AFM, are identical to those of rafts deposited on wide-area SAMs. Binding to the APTES stripes appears to be very strong as indicated by "jamming" of the rafts at a saturation coverage of 42% and the stability to repeated AFM scanning in air.

Microscopy, Atomic Force↗