Abstract

4 Plaster substitutes were tested in order to obtain some information about their reaction to stress. 2 materials are made of glass fibre with resin (Scotchcast and Lightcast), one from another artificial product (Baycast) and the fourth consists of a mesh of pure resin (Hexelite). Their resistance to bending forces was correlated to the weight of the samples used. The results indicated that a product containing glass fibre as carrier for the resin is the most robust.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

O Wruhs, J Poigenfürst. 1982. [Material testing of modern plaster substitutes].. https://pubmed.ncbi.nlm.nih.gov/6131578/

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related citations

Gap index: a good predictor of failure of plaster cast in distal third radius fractures.

The aim of this study was to assess the usefulness of the cast index and an indigenously developed gap index as measures of poor moulding of plaster. Twenty cases of re-manipulation of distal third radius fractures in children excluding growth plate injuries were compared with a control of 80 patients. A significant difference (<0.001) was observed in the cast index and the gap index of both the groups. The gap index was more sensitive than the cast index in predicting failure. At a level of cast index of more than 0.8 the relative risk of failure is 6.8 as compared with 35 when the sum of the gap index is more than 0.15. The gap index is a better predictor of failure than the cast index. A quick assessment of these indices is a good practice before accepting any plaster following a manipulation of distal radial fractures.

Casts, Surgical↗