Biocompatible polyurethane-based hydrogel.

Abstract

A polyurethane polymer developed at W. R. Grace has been evaluated for a variety of biomedical applications. The primary property of the polymer exploited for these applications is its ability to prevent protein adsorption when coated on a surface. The prepolymer consists of a trifunctional poly(ethyleneoxide-propylene oxide) triol end capped with isophorone diisocyanate. The prepolymer is reactive with water and can be converted to a hydrogel, a thin coating, or a soluble conjugate with another compound. Each category lends itself to separate biomedical applications which are described in detail. The non-toxic nature of the polymer was demonstrated in a number of systems and suggests its utility in biomedical applications.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

J A Braatz. 1994. Biocompatible polyurethane-based hydrogel.. https://doi.org/10.1177/088532829400900104

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related citations

Three-dimensional porous nano-hydroxyapatite@gelatin composite as efficient adsorbent for uranyl ion removal from low-level radioactive wastewater.

The contamination of water resources by uranyl (UO22+) ions poses significant environmental and health risks, requiring the development of efficient and sustainable remediation strategies. Adsorption-based techniques have emerged as promising approaches in the field of UO22+ removal, but the design of cost-effective, high-capacity, and environmentally friendly adsorbents remains challenging. In this study, a three-dimensional porous nano-hydroxyapatite@gelatin (nHAP@Ge) composite was synthesized through glutaraldehyde cross-linking, combining the structural stability of Ge with the high uranium affinity of nHAP. The optimized nHAP@Ge, with a nHAP:Ge mass ratio of 1:0.5, exhibited exceptional UO22+ removal efficiency (97 %), along with high adsorption capacity (364.03 mg/g). Systematic characterizations using scanning electron microscopy (SEM), thermogravimetric analysis (TGA), Fourier transform infrared (FT-IR) spectroscopy, and X-ray photoelectron spectroscopy (XPS) methods revealed that the porous structure and surface functional groups (-OH, Ca2+, and PO43-) of the material synergistically contributed to binding UO22+ species. Furthermore, the incorporation of nHAP into the Ge framework resulted in enhanced thermal stability while significantly improving the UO22+ adsorption performance. This work presents a scalable, eco-friendly, and recyclable strategy for the effective treatment of uranium-contaminated water, with potential applications in nuclear wastewater treatment and environmental remediation.

Adsorption

Differential mechanisms of retinoid transfer from cellular retinol binding proteins types I and II to phospholipid membranes.

Cellular retinol-binding proteins types I and II (CRBP-I and CRBP-II) are known to differentially facilitate retinoid metabolism by several membrane-associated enzymes. The mechanism of ligand transfer to phospholipid small unilamellar vesicles was compared in order to determine whether differences in ligand trafficking properties could underlie these functional differences. Unidirectional transfer of retinol from the CRBPs to membranes was monitored by following the increase in intrinsic protein fluorescence that occurs upon ligand dissociation. The results showed that ligand transfer of retinol from CRBP-I was >5-fold faster than transfer from CRBP-II. For both proteins, transfer of the other naturally occurring retinoid, retinaldehyde, was 4-5-fold faster than transfer of retinol. Rates of ligand transfer from CRBP-I to small unilamellar vesicles increased with increasing concentration of acceptor membrane and with the incorporation of the anionic lipids cardiolipin or phosphatidylserine into membranes. In contrast, transfer from CRBP-II was unaffected by either membrane concentration or composition. Preincubation of anionic vesicles with CRBP-I was able to prevent cytochrome c, a peripheral membrane protein, from binding, whereas CRBP-II was ineffective. In addition, monolayer exclusion experiments demonstrated differences in the rate and magnitude of the CRBP interactions with phospholipid membranes. These results suggest that the mechanisms of ligand transfer from CRBP-I and CRBP-II to membranes are markedly different as follows: transfer from CRBP-I may involve and require effective collisional interactions with membranes, whereas a diffusional process primarily mediates transfer from CRBP-II. These differences may help account for their distinct functional roles in the modulation of intracellular retinoid metabolism.

Adsorption

An integrated process for the production of toxic catechols from toxic phenols based on a designer biocatalyst.

We describe the biocatalytic production of 3-phenylcatechol from 2-phenylphenol with the whole cell biocatalyst Escherichia coli JM101 (pHBP461). The recombinant produces 2-hydroxybiphenyl 3-monooxygenase, an enzyme from Pseudomonas azelaica HBP1. This enzyme introduces a hydroxyl-group at the C3-position of a variety of 2-substituted phenols, such as 2-phenylphenol. This permits the biocatalytic production of 3-substituted catechols, which are difficult to synthesize chemically. Both 2-phenylphenol and 3-phenylcatechol are highly toxic to E. coli. The toxic effects of 2-phenylphenol were minimized by feeding this substrate to the reactor at a rate slightly below the maximum biooxidation rate. As a result, the substrate concentration in the reactor remained below toxic levels during the bioconversion. The toxic product formed was removed by continuous adsorption on the solid resin Amberlite XAD-4. To this end the reaction mixture, containing the biocatalyst, was pumped continuously through an external loop with a fluidized bed of the resin. This resin efficiently and quantitatively adsorbed both 3-phenylcatechol and the remaining trace amounts of 2-phenylphenol. Consequently, the concentrations of these compounds were kept at subtoxic levels (below 100 mg L-1) and gram amounts of 3-phenylcatechol were produced with space-time yields of up to 0.39 g L-1 h-1. The product was recovered from the resin by acidic methanol elution and purified by recrystallization from n-hexane resulting in overall yields exceeding 59%. The optimized system served as a surprisingly simple and efficient integrated process, that allows the bioconversion of toxic substrates to toxic products with whole cell biocatalysts.

Adsorption