Titanium for removable dentures. I. Laboratory procedures.

Abstract

To test the hypothesis that titanium (Ti) removable partial dentures (RPDs) would function for a period of at least 2 years without failure, 10 patients were selected to receive dentures made from Ti and Co-Cr. The Ti RPDs were constructed identically to conventional cobalt-chromium (Co-Cr) dentures. Five complete Ti dentures were also included and the laboratory procedures involved for making both complete and partial dentures were evaluated. The detection of internal defects by radiography made the screening of Ti castings possible and led to a rejection of specimens showing porosities of more than 0.5 mm in flexible members. Co-Cr frames on the other hand cannot be screened in this way. The success rate in the casting of Ti was 60% for both partial and complete dentures, but as casting technology has since improved, the rate is expected to be higher, particularly where complete denture palates have optimum thickness. The success rate in the casting of Co-Cr RPDs was 100% without radiographic screening. The weight difference between Ti and Co-Cr RPDs was in the range of 1.3 to 3.9 g at issue and is generally higher as the volume of denture frames increases. A large difference would be of clinical significance in maxillary complete dentures. The low density of Ti allows for the adoption of a useful pre-clinical quality-control process using commonly available dental X-ray units.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

T Mori, T Togaya, M Jean-Louis, M Yabugami. 1997. Titanium for removable dentures. I. Laboratory procedures.. https://doi.org/10.1046/j.1365-2842.1997.d01-301.x

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related citations

Effects of airborne-particle abrasion, sodium hydroxide anodization, and electrical discharge machining on porcelain adherence to cast commercially pure titanium.

The aim of this study was to determine the effect of airborne-particle abrasion (APA), sodium hydroxide anodization (SHA), and electrical discharge machining (EDM) on cast titanium surfaces and titanium-porcelain adhesion. Ninety titanium specimens were cast with pure titanium and the alpha-case layer was removed. Specimens were randomly divided into three groups. Ten specimens from each group were subjected to APA. SHA was applied to the second subgroups, and the remaining specimens were subjected to the EDM. For the control group, 10 specimens were cast using NiCr alloy and subjected to only APA. Surfaces were examined by using scanning electron microscope and a surface profilometer. Three titanium porcelains were fused on the titanium surfaces, whereas NiCr specimens were covered with conventional porcelain. Titanium-porcelain adhesion was characterized by a 3-point bending test. Statistical analysis showed that the porcelain-metal bond strength of the control group was higher than that of the titanium-porcelain system (p < 0.05). There were no significant differences between the bond strengths of titanium groups (p 0.05), except the bond strengths of Noritake Super Porcelain TI-22 groups on which APA and SHA were applied (p < 0.05). SHA and EDM as surface treatment did not improve titanium-porcelain adhesion when compared to APA.

Chromium Alloys↗

Microhardness of Ni-Cr alloys under different casting conditions.

This study evaluated the microhardness of Ni-Cr alloys used in fixed prosthodontics after casting under different conditions. The casting conditions were: (1-flame/air torch) flame made of a gas/oxygen mixture and centrifugal casting machine in a non-controlled casting environment; (2-induction/argon) electromagnetic induction in an environment controlled with argon; (3-induction/vacuum) electromagnetic induction in a vacuum environment; (4-induction/air) electromagnetic induction in a non-controlled casting environment. The 3 alloys used were Ni-Cr-Mo-Ti, Ni-Cr-Mo-Be, and Ni-Cr-Mo-Nb. Four castings with 5 cylindrical, 15 mm-long specimens (diameter: 1.6 mm) in each casting ring were prepared. After casting, the specimens were embedded in resin and polished for Vickers microhardness (VH) measurements in a Shimadzu HMV-2 (1,000 g for 10 s). A total of 5 indentations were done for each ring, one in each specimen. The data was subjected to two-way ANOVA and Tukey's multiple comparison tests (alpha = 0.05). The VH values of Ni-Cr-Mo-Ti (422 +/- 7.8) were statistically higher (p < 0.05) than those of Ni-Cr-Mo-Nb (415 +/- 7.6). The lowest VH values were found for Ni-Cr-Mo-Be (359 +/- 10.7). The VH values obtained in the conditions induction/argon and induction/vacuum were similar (p > 0.05) and lower than the values obtained in the conditions induction/air and flame/air torch (p < 0.05). The VH values in the conditions induction/air and flame/air were similar (p > 0.05). The microhardness of the alloys is influenced by their composition and casting method. The hardness of the Ni-Cr alloys was higher when they were cast with the induction/air and flame/air torch methods.

Chromium Alloys↗

Bond strength of three dental porcelains to Ni-Cr and Co-Cr-Ti alloys.

Ceramometal bond strength has played an important role for the replacement of gold alloys by nickel-chromium alloys in dentistry. This study evaluated the metal/porcelain bond strength of three ceramic systems (Vita VMK 88, Williams and Duceram) associated with three nickel-chromium alloys (Durabond, Lite Cast B and Resistal P) and one experimental cobalt-chromium-titanium alloy. Thirty cast cylinder specimens (15 mm in height; 6 mm in diameter) were obtained for each alloy, in away that 10 specimens of each alloy were tested with each porcelain. Bond strength was measured with an Emic screw-driven mechanical testing machine by applying parallel shear forces to the specimens until fracture. Kruskal-Wallis and Mann-Whitney U tests were used for statistical analysis of the alloy/ceramic combinations (p<0.05). Resistal P/Duceram had significantly higher bond strength (44.38+/-9.12 MPa) (p<0.05) than the other combinations, except for Co-Cr-Ti alloy/Vita VMK 88 (38.41+/-12.64 MPa). The association of the experimental Co-Cr-Ti alloy with Williams porcelain had significantly higher bond strength (28.20+/-3.86 MPa) than the combination of other alloys with the same porcelain (p<0.05). Based of these results and within the limitations of an in vitro study, it may be concluded that the bond strength of the three ceramic systems to the Ni-Cr and Co-Cr-Ti alloys varied significantly, indicating that metal/ceramic compatibility was very important to the bond strength.