PubMed Health⌕ Search

SEARCH · PubMed Health

Results for “Elastic Modulus”

Explore indexed PubMed citations for clinical trials, systematic reviews and public health research. Read source abstracts and follow each citation to its original PubMed record.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 883 records · Page 49Linked to original sources

At high heparin concentrations, protamine concentrations which reverse heparin anticoagulant effects are insufficient to reverse heparin anti-platelet effects.

Combined effects of heparin and protamine on plasma clot structure and platelet function were studied. Anticoagulant effects were monitored as changes in aPTT. Clot structure was defined in terms of fibrin fiber mass/length ratio (mu) and clot elastic modulus (EM). Platelet function was studied utilizing platelet aggregation and platelet force development (PFD) measurements. Heparin (1 U/ml) prolonged the aPTT from 30 to > 300 seconds, reduced PFD from 5,100 to 0 dynes, decreased mu (in batroxobin-induced gels) from 1.36 to 1.08 x 10(13) daltons/cm and decreased clot EM from 9,600 to 2000 dynes/cm2. Varying amounts of protamine reversed these effects: 16 micrograms/ml normalized the aPTT, 20 micrograms/ml normalized PFD, 32 micrograms/ml corrected mu, and 20 micrograms/ml returned EM to baseline. At high heparin concentrations (4 U/ml), protamine concentrations which corrected anticoagulant effects were inadequate to reverse antiplatelet effects. A protamine concentration of 40 micrograms/ml normalized the aPTT and mu, but 140 micrograms/ml of protamine was required to reverse heparin suppression of force development and clot elastic modulus. Excess protamine inhibited clotting and platelet function. In plasma containing 1 u heparin/ml, 140 micrograms protamine/ml reduced PFD by 83%, prolonged the aPTT by 63%, and reduced clot EM by 75%. In heparin free plasma, > 75 micrograms protamine/ml prolonged the aPTT. Thus, platelet function and clot structure are sensitive to protamine during heparin neutralization, and anti-platelet effects of heparin may persist when the aPTT is completely corrected. Excess protamine inhibits platelet function and compromises clot structure.

Blood Coagulation↗

Aging, carotid artery distensibility, and the Ser422Gly elastin gene polymorphism in humans.

Elastin is a protein of the extracellular matrix that forms the major component of elastic fibers from the arterial wall thickness and plays an important role in elastic properties of large blood vessels. To study the relationships between the Ser422Gly polymorphism in exon 16 of the gene-encoding elastin and the distensibility of 2 different arteries, the radial artery (a muscular artery) and the common carotid artery (an elastic artery), we studied a cohort of 320 subjects (49+/-12 years of age) without evidence of cardiovascular disease and who had never been treated with cardiovascular drugs. Distensibility and elastic modulus were evaluated for the common carotid and the radial arteries with high-resolution echo-tracking devices (NIUS-02 and Wall Track System). The A-to-G nucleotide change corresponding to the Ser422Gly amino acid change was studied by digestion of polymerase chain reaction products with BstNI. Results indicate that genotype frequencies (AA=10%, AG=51%, GG=39%) were in agreement with the Hardy-Weinberg equilibrium. For the carotid artery, a significant decrease in distensibility was observed in subjects carrying the A allele (with AA+AG genotypes) compared with subjects with the GG genotype (13.8+/-6.4 kPa(-1). 10(-3) versus 15.9+/-6.2 kPa(-1). 10(-3), P<0.01), assuming a dominant effect of the A allele. Moreover, the presence of the A allele was associated with a significant increase in elastic modulus (0.98+/-0.40 kPa. 10(3) in subjects with AA+AG genotypes versus 0.83+/-0.41 kPa. 10(3) in subjects with GG genotypes, P<0.01). Multivariate analysis indicated that these results were observed after adjustment for age, gender, and mean arterial blood pressure (P<0.01). In contrast, no association was found between arterial parameters and genotypes for the radial artery. The 2-way analysis of covariance adjusted for mean arterial blood pressure indicated that the association between the A allele and distensibility of the carotid artery was observed only in subjects >50 years of age, assuming for carotid distensibility a significant age effect (P<0.01), genotype effect (P=0.01), and age-genotype interaction (P=0.04). The present results indicate a relationship between the Ser422Gly polymorphism and the distensibility of elastic arteries but not of muscular arteries and suggest that there is an age-genotype interaction for carotid artery distensibility.

Aging↗

[Study of the visco-elastic response of the aortic wall to angiotensin and noradrenaline in the conscious dog by analysis of the instantaneous pressure-diameter relation in the descending aorta].

The viscoelastic behaviour of the aorta has been studied in 7 adult non-anesthesized mongrel dogs, chronically instrumented with a microtransducer pressure (Konigsberg P7) implanted inside the aortic lumen, and 2 ultrasonic crystals diametrically opposed and fixed in the adventitia of the thoracic aorta. Pressure and diameter were analysed in terms of mean values and of systolic diastolic variations, enabling to calculate the elastic modulus of Peterson. After recovery from surgery, and under autonomic blockade by atropine and propranolol, perfusions of angiotensin and norepinephrine were performed at incremental steps of doses. In individual dogs, instantaneous pressure-diameter relationships were formed by the different pressure diameter hysteris loops obtained at each dose of the same drug; the relationships obtained with the two drugs were curvilinear and were mixed at lower pressure ranges, but at highest levels of pressures it was found, that comparatively to angiotensin curve, that of norepinephrine had shifted toward lower diameter. The percent increase in mean diameter from baseline obtained at each dose of the same drug, was positively correlated to the corresponding per cent increase in mean pressure, with angiotensin (r = 0.83 P less than 0.001), and for norepinephrine (r = 0.82 P less than 0.001), but the slope of the relation was lower with angiotensin (22.3 +/- 3.2) than with norepinephrine (12.8 +/- 1.9) (P less than 0.001); likewise, the elastic modulus, for each dose of a same drug, was positively correlated to the corresponding mean pressure for angiotensin (r = 0.53 P less than 0.01), norepinephrine (r = 0.69 P less than 0.001).(ABSTRACT TRUNCATED AT 250 WORDS)

Angiotensin II↗

Influence of cement on a restored crown of a first premolar using finite element analysis.

PURPOSE: The purpose of this study was to examine the influence of the elastic modulus of cement and luting thickness on the resulting stresses in an axially loaded crown cemented onto a first premolar. A comparison of these stresses was also made with the strength of the constituent materials making up the crown. MATERIALS AND METHODS: Examination of the stresses on a restored crown was conducted using finite element analysis. Eight different axisymmetric models containing combinations of In-Ceram or gold coping, using adhesive resin or zinc phosphate cement as the luting agent, with thicknesses of either 0.05 or 0.1 mm were analyzed. RESULTS: The peak tensile principal stresses in the porcelain remained below its material fracture strength. The same was true for the peak stress in the adhesive resin compared to its fracture and chemical bond strength. This was not the case for zinc phosphate. The influence of the luting agent's elastic modulus on the stresses in the crown was minor, and the influence of luting thickness was even less. CONCLUSION: The role of the luting agent was primarily one that effectively transferred the resulting stresses between the relatively stiff coping and underlying dentin. There was no evidence of the luting agent itself playing a significant role in resisting deflection from the applied force.

Aluminum Oxide↗

Effect of adjuvant induced arthritis on the mechanical properties and thermal behavior of skin and tendon.

In rats with adjuvant induced arthritis, the mechanical properties and thermal behavior of the skin and tendon were studied during the acute and chronic phase of the disease. Among the mechanical properties, the tensile strength and elastic modulus were found to decrease markedly both in the skin and tendon of arthritic rats while the extensibility did not show any significant change during the course of the disease. The thermal behavior, namely, shrinkage temperature, denaturation temperature, isometric tension and the temperature at isometric tension were decreased appreciably both in the skin and tendon of arthritic rats, the decrease being prominent during the chronic phase of arthritis. Both the mechanical properties and thermal behavior were correlated with biochemical parameters such as total collagen content and the ratio of the total activity of 14C-hydroxyproline of soluble collagens to insoluble collagen. The results support the concept of impaired collagen crosslinking in adjuvant induced arthritis. Prednisolone and L-thyroxine were administered to arthritic rats and the changes in the mechanical properties and thermal behavior of the skin and tendon of arthritic rats were studied. Both prednisolone and L-thyroxine increased the decreased values of tensile strength and elastic modulus of the skin and tendon in adjuvant induced arthritis. Similarly the decreased values in the thermal behavior of arthritic rats were found to be increased by treatment with prednisolone and L-thyroxine. Results indicated correlations with the beneficial action of prednisolone and L-thyroxine on the impaired collagen crosslinking in adjuvant induced arthritis.

Animals↗

Analysis of a below-knee patellar tendon-bearing prosthesis: a finite element study.

In this study, a finite element (FE) model of a below-knee prosthesis of patellar tendon-bearing (PTB) design, and several altered variations of the model have been constructed. A load of approximately 1.5 times normal body weight (984 N) was applied at the heel of the model to simulate heelstrike conditions. The "base" model was then analyzed and revised iteratively until a model which provided consistency between soft tissue elastic modulus and socket displacement was developed. The interface normal and shear stresses obtained from the analysis of this revised base model were highest (about 961, and 463 KPa, respectively) at the distal anterior tip of the socket/stump. Proximally, higher normal stresses (72-78 KPa) were found medially and posteriorly. Proximal shear stresses were highest posteriorly (79 KPa), although shear stresses medially (51 KPa), and laterally (43 KPa), were also much higher than anteriorly (10 KPa). FE analyses were performed on the altered models to determine the relative effects on socket/stump interface stresses of altering the FE model of the prosthesis. Results of the analysis indicate that fabricating the prosthesis from a material with an elastic modulus ten times lower than that of the revised base model can produce reductions in the maximum pressure of up to 14 percent. Large decreases in maximum pressures (71 percent) resulted from the use of a suction socket rather than a conventional socket. Small changes in stump length (2 cm) caused relatively large pressure changes (16 to 18 percent).

Amputation, Surgical↗

An impedance matching of femoral-popliteal arterial grafts: a theoretical study.

We have proposed a mathematical method to investigate the matching conditions for an arterial graft in the femoral-popliteal region from a mechanical stand-point. Pulsatory blood flow, arterial wall motions, and conservation law are expressed by linear dynamical equations based on strict mechanical and constitutional considerations. To express the physiological blood flow in an actual arterial system, the tethering effects from the surrounding tissue and wall tensions were incorporated. The physiological parameters of arterial wall and tethering were utilized from reported experimental data. By complex analysis, mathematical expressions for the local impedance and reflection coefficient were obtained. They include not only blood properties such as viscosity and density, but also arterial properties including elastic modulus, radius, Poisson ratio, wall thickness, wall tension, frequency, and tethering effects from surrounding tissue. A matching condition was defined for minimizing the local impedance and reflection coefficient. The biophysical background was to reduce any mechanical mismatches, thus minimizing the disturbance of the flow velocity profile and shear stress distribution within the artery. Impedance matching in turn diminishes the negative factors for graft substitution represented by intimal hyperplasia and thrombosis. The calculated impedance and reflection coefficient inversed parabolically to functions of the resistance of the host artery, and there was one host arterial resistance that minimized the impedance and reflection coefficient. The present analysis revealed that for matching host artery with an elevated resistance, the dynamic elastic modulus of the wall of the graft that minimizes the impedance and reflection coefficient was increased. This indicates that for a host artery with a high resistance, an impedance matched stiff wall graft is preferable. For a large radius and a compliant host artery on the other hand, a large compliant graft should be linked. The present theoretical matching conditions will prevent anastomotic hyperplasia and thrombosis in graft substitution.

Blood Vessel Prosthesis↗

Properties of silorane-based dental resins and composites containing a stress-reducing monomer.

OBJECTIVE: To evaluate properties of silorane-based resins and composites containing a stress reducing monomer. METHODS: Resin mixtures and composites were formulated containing (a) a developmental stress reducing monomer [TOSU; Midwest Research Institute]; (b) Sil-Mix (3M-ESPE); (c) photo cationic initiator system. Standard BISGMA/TEGDMA resin (B/T) and composite (Filtek Z250) were used as controls. Polymerization volume change was measured using a NIST mercury dilatometer and polymerization stress using an Enduratec mechanical testing machine. Three point bend tests determined flexural elastic modulus, work of fracture, and ultimate strength (ADA 27; ISO 4049). Fracture toughness was measured using ASTM E399-90. Four groups of resins and composites were tested: Sil-Mix, methacrylate standard, and Sil-Mix with two addition levels of TOSU. An ANOVA was used and significant differences ranked using Student-Newman-Keuls test (alpha=0.05). RESULTS: Polymerization stress values for resins containing TOSU were significantly less than the other materials. Polymerization shrinkage values for Sil-Mix formulations were significantly less than for B/T, but were not different from each other. TOSU-containing formulations generally had somewhat lower mechanical properties values than Sil-Mix or B/T. Polymerization stress values for Sil-Mix-based composites were significantly less as compared to Z250. The 1wt.% TOSU composite had the lowest stress. No difference between composite groups was noted for fracture toughness or work of fracture. For ultimate strength, the 5wt.% TOSU formulation differed significantly from Z250. All Sil-Mix formulations had elastic modulus values significantly different from Z250. SIGNIFICANCE: The ability of TOSU to reduce polymerization stress without a proportional reduction in mechanical properties provides a basis for improvement of silorane-based composites.

Alkanes↗

Estimation of arterial stiffness, compliance, and distensibility from M-mode ultrasound measurements of the common carotid artery.

BACKGROUND AND PURPOSE: Arterial stiffness may indicate early vascular changes that predispose to the development of major vascular disease. The repeatability of a variety of indices of arterial stiffness calculated from a standard carotid arterial M-mode ultrasound image was investigated. METHODS: Twenty-six asymptomatic normal subjects were imaged and had blood pressure recordings on each of two separate occasions at least 1 day apart. Using a computer-assisted method, the maximum and minimum internal diameter and average wall thickness of the right common carotid artery were measured over several cardiac cycles, and the following indices of arterial stiffness and distensibility (compliance) were derived: the pressure-strain elastic modulus (Ep), Young's modulus (E), cross-sectional compliance (CC), and the distensibility coefficient (DC). RESULTS: The repeatability of these measures, expressed as coefficients of variation, was as follows: Ep, 18%; E, 24%; CC, 14%; and DC, 13%. In another group of 20 subjects, the coefficient of variation for repeat examination by different sonographers was Ep, 19%; E, 20%; CC, 14%; and DC, 17% and for the one sonographer using two ultrasound machines was Ep, 13%; E, 13%; CC, 11%; and DC, 13%. These values indicate a moderate level of repeatability. In a univariate analysis each of these indices was significantly related to increasing age (Ep = 1.0 + 12.9 x AGE, r = .80; E = 314.5 + 13.9 x AGE, r = .48; CC = 22.6-0.26 x AGE, r = -.63; DC = 64.0-0.65 x AGE, r = -.78) but not to wall thickness (all P > .47). Using multiple regression techniques to adjust for age, wall thickness is a significant predictor of distensibility (P = .017), cross-sectional compliance (P < .001), and the pressure-strain elastic modulus (P = .019). Because Young's modulus is calculated from wall thickness, it could not be included in the multivariate analysis. CONCLUSIONS: We conclude that estimates of carotid artery distensibility and cross-sectional compliance derived from M-mode ultrasound recordings are moderately repeatable and may provide useful additional end points for trials of atherosclerotic progression.

Adult↗

Marginal and internal adaptation of stratified compomer-composite Class II restorations.

Different approaches have been proposed to improve the adaptation of Class II restorations, including applying low-elasticity modulus base liners. This in vitro fatigue test (or study) evaluated the influence of the compomer base-lining configuration on restoration adaptation. Direct Class II MOD box-shaped composite restorations with or without base and lining (n=3x8) were placed on intact human third molars with proximal margins 1 mm above or under the CEJ. The compomer (Dyract) was applied as a 1 mm-thick lining or as a base, closing proximo-gingival margins. Marginal adaptation was assessed before and after each phase of mechanical loading (250,000 cycles at 50N, 250,000 cycles at 75N and 500,000 cycles at 100N); internal adaptation was evaluated after test completion. Gold-sputtered resin replicas were observed in the SEM and restoration quality evaluated in percentages of continuity (C) at the margins and within the internal interface after sample section. Mechanical loading did not influence adaptation to enamel, while it adversely affected restoration adaptation to dentin for the full composite and compomer-base restorations (C varied, respectively, from 95.2 to 75.3% and from 98.0 to 10.6%). The internal adaptation quality showed the same general trend, however, with reduced scores of continuity. In this experimental condition, application of a low elasticity modulus layer under the restorative material proved advantageous but the compomer should not contact the gingival margins.

Bisphenol A-Glycidyl Methacrylate↗

Effects of hypophysectomy and recombinant human growth hormone on material and geometric properties and the pre- and post-yield behavior of femurs in young rats.

To study the musculoskeletal effects of hypophysectomy (Hx) and a partial replacement treatment with recombinant human growth hormone (rhGH) in rats, we determined the stiffness (elastic modulus, E) and volumetric BMD (vBMD) of cortical bone; the periosteal and endosteal perimeters, area and bending moment of inertia (xCSMI) of the cross sections, and the structural stiffness and pre- and post-yield strength of the femur diaphyses by pQCT and mechanical tests, and the gastrocnemius weight of rats that were either intact (n = 9) or Hx at 15 days of age (20). The latter were otherwise untreated (Hx controls, 4) or given 0.4 (8) or 2.0 (8) IU kg(-1) day(-1), s.c., of rhGH for 45 days starting 15 days after surgery. Hx delayed musculoskeletal development (gastrocnemius weight, bone geometric properties), thus affecting the diaphyseal stiffness and strength. It also reduced the cortical vBMD through an undefined mechanism, and increased the elastic modulus of cortical bone. The Hx also affected the correlation between bone geometric and material properties (xCSMI vs. E), suggesting an antianabolic interaction with the biomechanical control of bone modeling in response to strains caused by mechanical usage. As a result, Hx reduced the stiffness, post-yield, and ultimate strength of the diaphyses. These effects should reflect changes in bone tissue microstructure, perhaps associated with crack generation and progress, but unrelated to bone mineral mass. They are compatible with the induction of a delay in collagen turnover with associated increases in fibers' diameter and crystals' size that may have resulted from the suppression of some other hormones, such as thyroid, prolactin, or other hormones regulated by ACTH. The above doses of rhGH significantly but incompletely prevented the negative Hx effects on bone and muscle development (bone geometric properties, muscle mass). However, rhGH treatment failed to prevent the demineralizing and stiffening effect of Hx on bone tissue and the unusual effects on the post-yield strength (less clearly related to muscle development than the former). Consequently, rhGH treatment tended to preserve the natural relationship between muscle function and bone geometry but not bone strength. The effects of larger rhGH doses and the interaction of other hormones with the described effects remain to be investigated. Nevertheless, these findings would deserve special attention because they challenge the prevailing view that in endocrine-metabolic bone-weakening diseases the bone matrix always has a normal composition.

Aging↗

Effect of water on the physical properties of resin-modified glass ionomer cements.

OBJECTIVES: Resin-modified glass ionomer cements (GIC) are available for clinical use as restorative materials or as liners and bases. This work was conducted to study the effect of water sorption on the physical properties of several resin-modified GIC, by changing the samples' storage conditions. METHODS: The water sorption, the flexural strength, the flexural elastic modulus, the Vickers hardness and the dimensional changes of five resin-modified GICs were measured using specimens aged for 24 h to 3 mon. The specimens were stored at 37 degrees C, either in a dry environment (A), immersed in water (B), stored in a humid environment (C), stored in a humid environment for 1 h and then immersed in water (D), or immersed in water and subsequently dried (B + A). An analysis of variance was used to compare the results. RESULTS: The resin-modified GIC absorb during the first 24 h large amounts of water (114-172 mg/cm3) compared to the conventional GIC (30-63 mg/cm3). Water alters the physical properties of resin-modified GICs: With regard to dry specimens, a decrease in the flexural strength of 20 to 80% was observed for samples immersed in water. Decreases in their flexural elastic modulus (50 to 80%) and in their hardness (approximately 50%) were also observed. Water sorption also provoked an expansion in volume of the immersed specimens, ranging from 3.4 to 11.3% after 24 h. SIGNIFICANCE: The flexural strength and Vickers hardness of the resin-modified GICs are sensitive to the water contained in the tested specimens. A correlation was established between the decrease in their physical properties and the water uptake. However, it should not be concluded that these materials are not adequate for use in applications in direct contact with oral fluids. Probably, resin-modified GIC placed in oral cavities would not be affected to the same extent as in in vitro tests. In an oral environment, the constituents of saliva will certainly decrease the rate of water sorption and will hence delay its effects.

Absorption↗

Quantitative histologic evaluation of LTI carbon, carbon-coated aluminum oxide and uncoated aluminum oxide dental implants.

The response of mandibular bone to identical geometry LTI carbon, carbon-coated aluminum oxide, and uncoated aluminum oxide blade-type dental implants in baboons for 2 years was evaluated using histologic, microradiographic, and scanning electron microscopic methods. In addition, a quantitative histologic analysis was performed identifying the type, amount, and distribution of tissue surrounding the dental implant systems. This is the final phase of a study investigating the effect of implant elastic modulus and implant surface chemical composition on the performance of dental implants. Previous studies have utilized clinical and radiographic evaluations, postretrieval mechanical testing, and finite element stress analysis to evaluate the dental implant performance. The results of the histologic study revealed a direct implant-bone interface with no intervening soft tissue in 16 of the 21 implants (76%). A fibrous tissue interface was observed in 5 of 21 implants (24%). Quantitative histologic results for the implants with a direct implant-bone interface showed statistically larger crestal cortical plates (p less than 0.05) and greater area fraction crestal cancellous bone (p less than 0.05) in the LTI carbon implant compared to the carbon-coated and uncoated aluminum oxide implants. The carbon-coated and uncoated aluminum oxide implants demonstrated statistically greater area fraction cancellous bone at the inferior region of the implant (p less than 0.05) and thinned and reduced crestal cortical plates when compared to the LTI carbon implants. The results indicate that significant stress shielding of the crestal bone had occurred with the rigid carbon-coated and uncoated aluminum oxide implants when compared to the LTI carbon implants which had a material elastic modulus similar to cortical bone. Based upon the histologic results, it appears that the LTI carbon implants with the direct implant-bone interface exhibited a greater potential for long-term successful performance compared to the aluminum oxide substrate implants.

Aluminum↗

A clinical comparison of LTI carbon, alumina, and carbon-coated alumina blade-type implants in baboons.

The clinical performance of LTI carbon, carbon-coated aluminum oxide, and uncoated aluminum oxide blade-type dental implants was studied in baboons. The objective of the study was to determine the effect that implant material elastic modulus and surface composition have on implant performance. Clinical parameters of mobility, sulcus depth, soft tissue characteristics, and radiographic appearance were used in the evaluation. The implants were placed in healed extraction sites in adult female baboons and were used as a distal abutment for a three-unit fixed gold prosthesis. The restorations were allowed to assume normal occlusal function and were left in situ for a period of two years. The radiographic and sulcus depth measurements appeared inferior for the LTI carbon implants and best for the carbon-coated aluminum oxide implants. No differences in mobility or soft tissue characteristics were noted for the three implant systems. Two implants both in the same animal--one LTI carbon and one uncoated aluminum oxide--were definite clinical failures. The results of the study indicate that an elastic modulus mismatch between implant and bone is not an a priori cause of implant failure and that the implant surface composition had little apparent effect on the clinical and radiographic performance of these implant materials.

Aluminum↗

Study of water sorption, solubility and modulus of elasticity of light-cured dimethacrylate-based dental resins.

Polydimethacrylate resins were prepared by photopolymerization of Bis-GMA, TEGDMA, UDMA or Bis-EMA (4) monomer, initiated by camphoroquinone/N,N-dimethylaminoethyl methacrylate system. The study of physical properties of these resins showed that TEGDMA seems to create the most dense polymer network, which however is the most flexible (0.74GPa), absorbs the highest amount of water (6.33 wt%) and releases the lowest amount of unreacted monomer (2.41 microg/mm(3)). UDMA and Bis-EMA (4) create more rigid networks, which absorb lower water and release higher unreacted monomer than TEGDMA. Bis-EMA (4) absorbs the lowest water amount (1.79 wt%) and releases the highest amount of unreacted monomer (14.21 microg/mm(3)). Bis-GMA leads to the formation of the most rigid network (1.43 GPa), which absorbs lower water than the resin made by TEGDMA but higher than the resin made by UDMA and Bis-EMA (4). Copolymers of Bis-GMA with the other monomers were also prepared, using various monomer combinations and molar ratios. Copolymers Bis-GMA/TEGDMA (50/50 and 70/30 wt%) showed significantly higher values for Young's modulus (1.83 and 1.78 GPa) than those predicted by the linear dependence of the values on the copolymer composition. Gradual replacement of TEGDMA with UDMA or/and Bis-EMA (4) in copolymerization with Bis-GMA resulted in more flexible resins with lower water sorption and higher solubility values, depending on the TEGDMA content.

Composite Resins↗

A mechanism for the decrease in stiffness of bioprosthetic heart valve tissues after cross-linking.

It has been reported that the elastic modulus of glutaraldehyde treated bioprosthetic valve materials is lower than that of fresh tissues. This finding appears paradoxic, because cross-linked tissues are usually stiffer than fresh ones. To investigate this phenomenon, the stiffness of 12 each of fresh and glutaraldehyde treated strips of porcine aortic valve cusps was measured at different levels of applied preload. To eliminate shrinkage effects, tissues were fixed while constrained at the gauge length. From paired comparisons of fresh versus fixed, it was found that glutaraldehyde fixed materials had a consistently lower stiffness than fresh tissue at low loads (0.39 N/m for treated vs 0.54 N/m for fresh at a 150 N/m preload), but no difference was found at high loads (1.09 N/m for treated vs 1.07 N/m for fresh at 600 N/ m preload). It is concluded that the observed drop in elastic modulus at low loads is a phenomenon associated with cross-linking of the collagen fiber matrix. Because a cross-linked matrix offers greater resistance to stretch, fixed tissue generates higher tensions at lower strains, at a point on the loading curve where the collagen fibers are more crimped and the slope of the curve is lower. At high loads, however, the stiffness of fixed tissues is equivalent to that of fresh. Measuring stiffness at a given stress or tension, rather than at a particular state of collagen fiber crimp, leads to the apparent lower stiffness of fixed tissues.

Animals↗

Osteon pullout in the equine third metacarpal bone: effects of ex vivo fatigue.

An important concept in bone mechanics is that osteons influence mechanical properties in several ways, including contributing to toughness and fatigue strength by debonding from the interstitial matrix so as to "bridge" developing cracks. Observations of "pulled out" osteons on fracture surfaces are thought to be indicative of such behavior. We tested the hypothesis that osteon pullout varies with mode of loading (fatigue vs. monotonic), cortical region, elastic modulus, and fatigue life. Mid-diaphseal beams from the dorsal, medial, and lateral regions of the equine third metacarpal bone were fractured in four point bending by monotonic loading to failure under deflection control, with or without 10(5) cycles of previous fatigue loading producing 5000 microstrain (15-20% of the expected failure strain) on the first cycle; or sinusoidal fatigue loading to failure, under load or deflection control, with the initial cycle producing 10,000 microstrain (30-40% of the expected failure strain). Using scanning electron microscopy, percent fracture surface area exhibiting osteon pullout (%OP.Ar) was measured. Monotonically loaded specimens and the compression side of fatigue fracture surfaces exhibited no osteon pullout. In load-controlled fatigue, pullout was present on the tension side of fracture surfaces, was regionally dependent (occurring to a greater amount dorsally), and was correlated negatively with elastic modulus and positively with fatigue life. Regional variation in %OP.Ar was also significant for the pooled (load and deflection controlled) fatigue specimens. %OP.Ar was nearly significantly greater in deflection controlled fatigue specimens than in load-controlled specimens (p=0.059). The data suggest that tensile fatigue loading of cortical bone eventually introduces damage that results in osteonal debonding and pullout, which is also associated with increased fatigue life via mechanisms that are not yet clear.

Animals↗

Fast-setting calcium phosphate scaffolds with tailored macropore formation rates for bone regeneration.

Calcium phosphate cement (CPC) is highly promising for craniofacial and orthopedic repair because of its ability to self-harden in situ to form hydroxyapatite with excellent osteoconductivity. However, its low strength, long hardening time, and lack of macroporosity limit its use. This study aimed to develop fast-setting and antiwashout CPC scaffolds with high strength and tailored macropore formation rates. Chitosan, sodium phosphate, and hydroxypropyl methylcellulose (HPMC) were used to render CPC fast-setting and resistant to washout. Absorbable fibers and mannitol porogen were incorporated into CPC for strength and macropores for bone ingrowth. Flexural strength, work-of-fracture, and elastic modulus were measured vs. immersion time in a physiological solution. Hardening time (mean +/- SD; n = 6) was 69.5 +/- 2.1 min for CPC-control, 9.3 +/- 2.8 min for CPC-HPMC-mannitol, 8.2 +/- 1.5 min for CPC-chitosan-mannitol, and 6.7 +/- 1.6 min for CPC-chitosan-mannitol-fiber. The latter three compositions were resistant to washout, whereas the CPC-control paste showed washout in a physiological solution. Immersion for 1 day dissolved mannitol and created macropores in CPC. CPC-chitosan-mannitol-fiber scaffold had a strength of 4.6 +/- 1.4 MPa, significantly higher than 1.2 +/- 0.1 MPa of CPC-chitosan-mannitol scaffold and 0.3 +/- 0.2 MPa of CPC-HPMC-mannitol scaffold (Tukey's). The strength of CPC-chitosan-mannitol-fiber scaffold was maintained up to 42 days and then decreased because of fiber degradation. Work-of-fracture and elastic modulus showed similar trends. Long cylindrical macropore channels were formed in CPC after fiber dissolution. The resorbable, fast-setting, anti-washout and strong CPC scaffold should be useful in craniofacial and orthopedic repairs. The novel method of combining fast- and slow-dissolution porogens/fibers to produce scaffolds with high strength and tailored macropore formation rates to match bone healing rates may have wide applicability to other biomaterials.

Bone Regeneration↗