An ex vivo study of the effects of retained coronal dentine on the strength of teeth restored with composite core and different post and core systems.

AIM: To investigate the fracture resistance and fracture patterns of teeth restored with composite cores supported by different pre-fabricated post systems and different heights of remaining coronal dentine. METHODOLOGY: Four groups of 30 single rooted teeth were used. Each group was divided into three subgroups of 10 teeth each and restored with carbon fibre, glass fibre, or Radix titanium posts luted with dual cure resin cement. The control group A had no retained coronal dentine. Groups B, C and D had 2, 3 and 4 mm of retained buccal and lingual coronal dentine, respectively. Teeth were tested to failure using an Instron Universal Testing Machine. Subsequently, the fracture mode of specimens was recorded. RESULTS: Teeth with retained dentine were more resistant to fracture (P = 0.001). Tooth fracture resistance was not significantly different between groups B, C and D. Within group A, titanium posts were associated with higher fracture resistance than fibre posts. Within the other groups, tooth fracture resistance was not related to post material. Within groups C and D, fracture resistance of teeth restored with carbon fibre posts was significantly higher than those restored with glass fibre posts. The dominant fracture mode in group A was core and vertical oblique root fracture whilst a combination of core, coronal dentine and root fracture occurred in the other groups. CONCLUSIONS: Fracture resistance of teeth increased with the presence of retained coronal dentine. The use of glass and carbon fibre posts did not improve the fracture resistance or the fracture pattern of teeth when compared with metal titanium posts regardless of the presence of retained coronal dentine. The dominant fracture pattern of teeth was not related to the amount of retained dentine if it was >2 mm high.

Carbon↗

A morphological comparison of radicular dentin following root planing and treatment with citric acid or tetracycline HCl.

The conditioning of root surfaces with saturated solutions of citric acid or tetracycline is unpredictable in facilitating new attachment, perhaps due to the low pH of these solutions which may be denaturing the organic matrix of the root as well as demineralizing the surface. The purpose of the present study was to compare the effects of a saturated solution of citric acid (pH = 1) with that of a 0.5% solution of tetracycline HCl (pH = 3.2) on radicular dentin with regard to the removal of the smear layer, exposure of dentinal tubule openings, and demineralization of the peritubular dentin. 10 bovine incisors were used in this study. The crowns and apical 1/3 of the root were resected and the resulting root segments were then frozen in icy freon. The cementum was fractured off of the root to produce a fracture-exposed, non-instrumented dentin surface. This fracture-exposed dentin surface was divided into 4 specimens, the 1st being a fracture-exposed, non-instrumented dentin control specimen (FE). After removal of the (FE) specimen from the root segment, the remainder of the fracture-exposed dentin surface was thoroughly root planed and then subdivided into the 3 remaining specimens. One of these specimens served as the root planed dentin surface (RP); another specimen (CA) was immersed in saturated citric acid (pH = 1) for 5 min and then washed in water for 5 min; the final specimen (T) was immersed in a 0.5 mg/ml solution of tetracycline HCl for 5 min and rinsed in water for 5 min.(ABSTRACT TRUNCATED AT 250 WORDS)

Animals↗

Evidence for a dentin-derived inhibitor of macrophage spreading.

The ability of macrophages to spread in vitro on mineralized and non-mineralized tissues extracted with guanidium hydrochloride (GuHCl) was studied in order to establish morphologic evidence for an extractable inhibitor of macrophage spreading present within dentin. Macrophages were seeded onto dentin, demineralized dentin, predentin and hyaline cartilage extracted with different concentrations of GuHCl. Macrophages were also seeded onto unextracted tissues. The results were evaluated with scanning electron microscopy after varying incubation periods. Macrophages readily attached and spread on extracted and unextracted dentin, extracted demineralized dentin, predentin, and hyaline cartilage. Cells seeded onto unextracted demineralized dentin, predentin, and hyaline cartilage attached, but showed no signs of spreading. It was concluded that an extractable inhibitor of macrophage spreading is present in the organic, non-collagenous component of dentin. This inhibitor may be responsible for the resistance of predentin and dentin to resorption.

Animals↗

Effect of fluoride on caries progression and dentin apposition in rats fed on a cariogenic or non-cariogenic diet.

The effect of fluoride in drinking water on the progression of dentinal caries and dentin apposition was studied in Wistar rats. The initiation of enamel caries lesions was first induced for 2 wk with S. sobrinus and a 43% sucrose diet after weaning. Thereafter the animals were fed on either a cariogenic or a non-cariogenic diet and distilled water supplemented with 0, 1, 7 or 19 ppm fluoride. The areas of dentinal caries and dentin apposition were quantified after tetracycline staining. Fluoride reduced dentinal caries progression after the initiation of lesions in the presence of a cariogenic diet at a concentration of 19 ppm F, and without sucrose at 1 ppm F. The effect of fluoride in reducing dentin apposition with a cariogenic diet was dose-dependent, whereas fluoride in non-cariogenic groups had practically no effect on dentin formation. These results suggest that fluoride together with a high concentration of sucrose in the diet might have an odontoblast-mediated effect on the regulation of the progression of dentinal caries.

Analysis of Variance↗

A comparative study of the transition between predentin and dentin, using various preparative procedures in the rat.

The appearance of the junction between predentin and dentin of rat incisors was investigated after chemical fixation (aldehyde), physical fixation (high pressure freezing and freeze substitution) and by histochemistry. Physical fixation revealed a 1-2 micron wide intermediary zone, in which only the collagen fibers were mineralized. In dentin, which looked denser and more homogeneous, both collagen fibers and intercollagenous spaces were mineralized. The intermediary layer could not been seen after aldehyde fixation. When cationic dyes were used during fixation in order to retain proteoglycans, a 0.5-5 micron border zone located at the junction between predentin and dentin was densely stained on the dentin side, whereas in dentin only the interglobular network displayed electron density. The periodic acid-thiocarbohydrazide-silver proteinate reaction, visualizing glycoproteins, and the phosphotungstic acid/chromic acid mixture, which reveals glycoproteins and phosphorylated proteins, produced extensive staining of the transitional zone located at the dentin edge, whereas staining was weaker in dentin. These morphological and histochemical investigations support the existence of an intermediary zone in which mineralization occurs. This transitional zone between predentin and dentin has specific properties; therefore we propose it be termed metadentin.

Aldehydes↗

Dentine hypersensitivity: a review.

Dentine hypersensitivity is a relatively common pain condition. Local pulpal inflammation, traumatic oral hygiene and dietary habits have been considered in the etiology of dentine hypersensitivity. Dentine hypersensitivity is probably caused by a change in fluid flow in the dentinal tubules, which in turn excites the nerve endings located at the pulp-dentine border. Consequently, treatment success would depend on the prevention of fluid flow across the dentinal tubules (sodium fluoride, stannous fluoride, sodium monofluorophosphate, strontium chloride, sodium citrate, potassium oxalate, and resins/adhesives), or on the desensitization of the nerve endings located at the pulp-dentine border (potassium nitrate). Although a wide variety of treatment methods have been available, clinical data is characterized with ambiguity, warranting further research of the factors which could possibly be implicated in the occurrence of dentine hypersensitivity.

Citrates↗

Adhesion to dentin.

The bond strengths of dentinal bonding systems to dentin and the microleakage at the dentinal bonding system to dentin interface are often determined in laboratory studies prior to the clinical evaluation of these systems. The shear bond strengths of some of the third generation dentinal bonding systems to dentin and the microleakage at the dentinal bonding system to dentin interface are discussed. In addition, the shear bond strengths of fluoride-containing liners/bases and the fluoride release from these systems are evaluated.

Dental Bonding↗

In vitro tensile bond strengths of amalgam to treated dentin.

Since amalgam traditionally relies on undercuts in the tooth preparation for retention, extensive tooth structure must be removed for amalgam core build-ups. In contrast, the ideal build-up material would achieve its retention by directly bonding to tooth structure. This study compared tensile bond strengths of amalgam to dentin using All-Bond Liner-FX with three different dentin pretreatment conditions and Amalgambond according to the manufacturer's directions. One hundred and twenty dentin samples were tested. Groups 1-3 used All-Bond Liner-FX as a bonding agent. Group 1 received a 15-second application of 10 percent phosphoric acid on the dentin; Group 2 received the recommended dentin conditioner; and Group 3 received no dentin pretreatment. Group 4 used Amalgambond as the bonding agent after a 10-second application of 10 percent citric acid/3 percent ferric chloride. Analysis of the data was conducted using both ANOVA and the Weibull statistic. Results of the analysis of variance indicate that there were no statistical differences among mean tensile bond strengths for the three dentin pretreatment conditions using All-Bond. All (30) of the Amalgambond specimens debonded prior to testing. The All-Bond fracture data was well described by the Weibull function as evidenced by the high coefficient of determination (R2 = 0.98-0.99). Fracture analysis indicated that all of the Amalgambond failures were adhesive at the Amalgambond-amalgam interface. All-Bond fractures were mixed cohesive/adhesive failures indicating similar bonding to amalgam and dentin.

Acid Etching, Dental↗

The measurement in vitro of enamel and dentine wear by toothpastes of different abrasivity.

OBJECTIVES: To investigate the in vitro enamel and dentine wear by toothpastes with a range of Relative Dentine Abrasivity (RDA) and Relative Enamel Abrasivity (REA) values. METHODS: Human enamel/dentine (approximately 50:50) blocks (approximately 4 x 4 mm) were polished and the enamel indented with four Knoop indents. The step across the enamel-dentine junction was measured by interference microscopy. Specimens were brushed in vitro with toothpastes with a range of RDA/REA values using a flat trim toothbrush mounted in a Wira brushing machine for 360 s and a load of 375 g. After brushing the Knoop indent length and the enamel-dentine step were remeasured and the amount of wear to the enamel and dentine was calculated. RESULTS: The mean enamel wear ranged from 0.05 to 0.40 microns, with the highest wear for the highest REA product. The mean dentine wear for all toothpaste products tested was positively correlated with RDA value (R2 = 0.897). The correlation was further improved if median wear values were used (R2 = 0.930). CONCLUSIONS: This study has demonstrated a rapid technique for the simultaneous investigation of the abrasive wear of toothpaste on enamel and dentine. There was a good correlation between median dentine wear and RDA values.

Dental Enamel↗

Effect of toothpicks with and without fluoride on De- and remineralization of enamel and dentine in situ.

The aim of this investigation was to study the effect of the interproximal use of fluoride (F)-impregnated and non-impregnated birch toothpicks on the degree of de- and remineralization of enamel and dentine in situ. Ten volunteers with complete dentures in the upper jaw participated. Each subject had four specimens: (1) sound enamel, (2) demineralized enamel, (3) sound dentine and (4) demineralized dentine; placed pairwise at two approximal sites (15/16 and 25/26) of the maxillary prosthesis. The study involved three test periods (A, B and C), each lasting 4 weeks. In A, the subjects used F toothpicks (impregnated in 4% NaF) and, in B, nonimpregnated toothpicks 3 times daily. During period C, no toothpicks were used. Dentifrice or other F-containing products were not allowed during the 4-week periods. Transversal microradiography was used to determine lesion depth (ld) and mineral loss (DeltaZ). The results revealed that all the sound samples lost mineral during the three experimental periods; DeltaZ for both enamel and dentine was less for A and B compared with C (p<0.01) and less for A compared with B and C for dentine (p<0.05, p<0.01). The demineralized samples also lost mineral, apart from dentine, during periods A and B, i.e. when F-impregnated and non-impregnated toothpicks were used; ld for enamel and DeltaZ for dentine were less for A compared with C (p<0.05). Four weeks' use of toothpicks, especially F-impregnated toothpicks, thus reduces the demineralization of enamel and dentine at approximal sites in situ.

Aged↗

Effect of fluoride-releasing filling materials on underlying dentinal lesions in vitro.

Fluoride-releasing materials placed over carious tissue are assumed to enhance remineralisation of the underlying lesion. This remineralisation, however, also depends on the availability of calcium and phosphate, which may be supplied by the pulpal fluid. The aim of this study was to measure the fluoride release of glass ionomer cements (GICs) into underlying dentin and to measure the effect of the released fluoride on the remineralisation of the underlying dentinal lesions using transversal microradiography. Discs of fluoride-releasing GIC were placed on top of dentinal lesions in an in vitro model. The discs and the dentin slabs were covered completely by a protective layer of nail varnish, leaving only the pulpal side of the dentin slab open, and hence the dentinal tubules as the pathway for the incubation fluid to the GIC disc. Specimens were incubated in a remineralisation buffer. The materials tested were a conventional GIC, an experimental GIC that was designed to have a high fluoride release, and an inert material. Fluoride was found to penetrate through the dentin slab into the surrounding fluid. Fluoride uptake from the experimental GIC was higher than from the conventional GIC. Mineral content-depth profiles after 10 weeks' remineralisation revealed that in the outer 30 microm of the lesion a higher mineral deposition occurred for the experimental GIC than in both other groups. No differences in the overall change of integrated mineral loss were found for the tested materials. We conclude that high fluoride release from filling materials only results in superficially increased remineralisation of underlying demineralised dentin.

Analysis of Variance↗

Accuracy and consistency of the visual diagnosis of exposed dentine on worn occlusal/incisal surfaces.

Most indices for the assessment of wear of various aetiologies include the distinction between 'enamel still present' and 'dentine exposed' for grading. Since the visual diagnosis of exposed dentine has not yet been validated, the present study is a first attempt to investigate its accuracy and consistency. Sixty-one examiners (23 scientists, 18 university dentists and 20 dental students) were asked to diagnose 49 tooth areas with different grades of wear and to decide whether dentine was exposed (positive test) or not (negative test). Afterwards, the teeth were histologically evaluated. In 44 areas, dentine (also in all cases with minor wear) was exposed, and in 5 areas enamel was present. Overall sensitivity was 0.65, specificity 0.88 and the proportion of correct diagnoses was 0.67. The diagnosis 'dentine is exposed' was about 5 times as likely and the diagnosis 'dentine is not exposed' half as likely to come from an area with exposed dentine than from an enamel-covered area. The closeness of the visual diagnosis to the histological findings was only fair (kappa=0.27), no significant impact of professional experience was found. For inter- and intra-examiner agreement, kappa was 0.28 and 0.55, respectively. It was concluded that the diagnosis of exposed dentine is difficult.

Dental Enamel↗

Dentine caries in vivo. Combined scanning electron microscopic and microradiographic investigation.

Dentine subjected to an in vivo demineralization challenge by plaque looses substantial amounts of mineral and is expected to change its ultrastructure. Results are presented of a combined microradiography and scanning electron microscopy (SEM) study on in vivo demineralized human dentine. The tissue was first demineralized in vivo under plaque for 3 weeks and subsequently analyzed by microradiography and SEM. In 6 participants dentine was positioned in a full prosthesis just under M2 in such a way that the outer surface of the tissue was 1.5 mm lower than the surface of the prosthesis; plaque accumulation takes place in the recessed area. A special technique allows SEM observations (at a given distance from the outer surface) on broken thin sections of demineralized dentine with a mineral content determined by microradiography. The results show that the ultrastructure of the dentine changes during severe demineralization. The main ultrastructural features are, however, still largely intact, even if half of the mineral originally present has been lost. In dentine with a mineral content of about 25 vol%, the dentinal tubules are enlarged by about 30%. In vivo demineralized dentine looses mineral in substantial amounts both from intertubular and from peritubular regions.

Adolescent↗

Remineralization of bovine dentine in vitro. The influence of the F content in solution on mineral distribution.

In this paper remineralization of bovine dentine is reported. After demineralization of the dentine in an acidic gel system creating lesions of about 180 microns depth, the tissue was remineralized in a 1.5 mM Ca and 0.9 mM phosphate containing solution at pH 7 and 37 degrees C for 8 or 21 days. The F content in the remineralization solution was 0.02, 2, or 10 ppm as NaF. Samples were analyzed by means of microradiography and scanning electron microscopy. The results show that remineralization (without F added in solution) causes a decrease in mineral loss and in lesion depth. With 2 or 10 ppm in solution, however, a substantial mineral accumulation in the lesion, but particularly on the original dentine surface, was observed. During 3 weeks of remineralization, mineral accumulations of 67 and 70 vol% of mineral for 2 and 10 ppm F in solution, respectively, were found near the original outer surface, with the sound dentine mineral value being 48 vol%. The combined microradiography and scanning electron microscopy data show that the mineral accumulated is for a major part deposited on the dentine tissue and partly inside. The latter deposition occurred both inside the tubules as well as in the intertubular areas. Inside the tubules dense precipitates were observed. Because several differences exist between bovine and human dentine, an extrapolation to the human in vivo situation is speculative. The results indicate that the presence of fluoride in the parts per million range is important for dentine remineralization efficacy and that the outer surface area in dentine can be 'overremineralized'.

Animals↗

Fluoride and mineral content in hyper-remineralized coronal bovine dentine in vitro after an acid challenge.

In this paper the acid resistance of hyper-remineralized dentine was quantified by means of fluoride and mineral measurements. Hyper-remineralization was achieved by demineralization of dentine in an acidic gel system (pH 5) for 3 weeks, followed by remineralization in a solution containing 1.5 mM Ca, 0.9 mM phosphate and 10 ppm F at pH 7 and 37 degrees C for 8 days. The samples were subsequently again demineralized in the gel system mentioned for 1, 2 and 3 weeks. Analysis for fluoride was done by means of the microdrill biopsy technique and to obtain information on the fluoride distribution by secondary ion mass spectrometry (SIMS); mineral was assessed by microradiography. The results showed that in hyper-remineralized dentine the original fluoride content was approximately 30,000 ppm F. This value was still in the same order after the acid challenge of 3 weeks at pH 5. These values were substantially higher than the baseline values in sound or in demineralized dentine being about 900 ppm F. The main microradiographic result was that there was no significant mineral change in the hyper-remineralized dentine due to the acid challenges. There was, however, a tendency for mineral redistribution deeper into the dentine lesion leading to lamination phenomena. The SIMS experiments on some of the samples showed a fluoride distribution in agreement with the microdrill fluoride data. Furthermore a fluoride redistribution took place in deeper parts of the lesion due to the acid challenges. The combined fluoride concentration and microradiographical data indicate that fluoride-enriched and highly mineralized hyper-remineralized dentine is more acid resistant than sound or demineralized dentine.

Animals↗

A microbiological study of recurrent dentinal caries.

A cross-sectional microbiological study of recurrent (secondary) dentinal caries was conducted. Freshly extracted human teeth containing amalgam restorations judged to be clinically intact were scrubbed with chlorhexidine soap and soaked in povidone-iodine solution. The teeth were then split to remove the fillings and examined for dentinal caries. Of 54 teeth examined, 22 (40%) were free of dentinal caries in the restored site. The remainder were assigned to arbitrary groups of questionable (15), initial (8) and active caries (9), based on the amount of dentinal decay observed. Comparison of pre-extraction bite-wing radiographs with the in situ findings revealed the sensitivity for secondary caries detection to be only about 50%. In contrast, the specificity for absence of caries was 73%. There was considerable variation in the numbers and types of micro-organisms found in dentine samples from lesions of comparable severity. Facultatively, anaerobic streptococci were the most numerous and most prevalent micro-organisms in the affected dentine, but no single species was significantly associated with recurrent caries. Mutans streptococci were found in 40% of sites with any degree of caries and in only 3 of the 9 sites with the most caries. Homofermentative lactobacilli were present in 18 of the 54 dentine samples, including 4 from caries-free sites. While the prevalence and numbers of lactobacilli increased with the degree of caries, they occurred in less than half of the affected dentine samples. Actinomyces occurred in 15 of 32 affected sites but only in 2 of the 9 most active sites. Their numbers never exceeded 3 x 10(3) CFU/mg.(ABSTRACT TRUNCATED AT 250 WORDS)

Actinomyces↗

Effect of lactic acid and proteolytic enzymes on the release of organic matrix components from human root dentin.

The mechanisms of organic matrix breakdown in the root caries process are not well understood. Therefore, the combined and separate effects of lactic acid and proteolytic enzymes on the degradation of human dentin collagen, glycoproteins, proteoglycans and phosphoproteins were investigated in the present study. Dentin powder was pretreated with lactic acid (pH 4.0), distilled and deionized (dd) water (pH 7.0) and EDTA/guanidine HCl (pH 7.4) for 24 h. Pellets of acid- or dd water-pretreated dentin powder were washed, dried, and then treated with trypsin, bacterial or mammalian tissue collagenase, or control buffer for 3 h. The released dentin proteins were analyzed by reducing sodium dodecyl sulfate-polyacrylamide gel electrophoresis and immunoblotting to identify degraded type I collagen, proteoglycans, glycoproteins and phosphoproteins. All water and acid pretreatment and enzyme treatment groups demonstrated two collagen fragment bands with molecular weights at approximately 79 kD. Further studies showed that the 79 kD proteins from acid-pretreated dentin collagen were degraded by tissue collagenase, suggesting that endogenous collagenase may be involved in the degradation of root dentin collagen. Dentin proteoglycans were detectable in all the treatment groups by protein slot blotting. Relatively few distinct glycoproteins and proteoglycans, and no phosphoproteins were detected by immunoblotting. Results from this study suggest that both acids and proteolytic enzymes from either host or microbial origin are important in the degradation of human dentin matrix and the mechanisms involved in the release of various noncollagenous proteins may be different.

Adolescent↗

Changes in bovine dentin mineral with sodium hypochlorite treatment.

Dentin powders from bovine incisors were treated with 10% NaClO solution. Differential thermal analysis (DTA) indicated the removal of organic material from the dentin sample following the treatment, since the exothermic reaction at 320 degrees C had disappeared. X-ray diffraction studies revealed a change in the crystallinity of the dentin crystals and the formation of calcite after the treatment. Infrared absorption analysis showed that the band due to carbonate ions was weakened after the treatment, while atomic absorption spectroscopic analysis showed that magnesium ions had been dissolved from the dentin sample. The a-axis lengths of treated and heated dentin samples differed from those of untreated and heated samples. Whitlockite was always found in the untreated/heated samples, whereas it was absent in the treated/heated samples. The unit cell dimensions of the whitlockite indicated the partial substitution of magnesium for calcium. Magnesium ions seemed to be more effective than carbonate ions in forming whitlockite. These results showed that some magnesium and carbonate ions were removed from the dentin crystal structure upon NaClO treatment, while at the same time organic materials were removed from the dentin sample. It was suggested that crystals in the NaClO-treated dentin were similar to enamel crystals from a crystallographic viewpoint.

Animals↗