PubMed Health⌕ Search

SEARCH · PubMed Health

Results for “Compressive Strength”

Explore indexed PubMed citations for clinical trials, systematic reviews and public health research. Read source abstracts and follow each citation to its original PubMed record.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,405 records · Page 78Linked to original sources

Possible stimuli for strength and power adaptation : acute metabolic responses.

The metabolic response to resistance exercise, in particular lactic acid or lactate, has a marked influence upon the muscular environment, which may enhance the training stimulus (e.g. motor unit activation, hormones or muscle damage) and thereby contribute to strength and power adaptation. Hypertrophy schemes have resulted in greater lactate responses (%) than neuronal and dynamic power schemes, suggesting possible metabolic-mediated changes in muscle growth. Factors such as age, sex, training experience and nutrition may also influence the lactate responses to resistance exercise and thereafter, muscular adaptation. Although the importance of the mechanical and hormonal stimulus to strength and power adaptation is well recognised, the contribution of the metabolic stimulus is largely unknown. Relatively few studies for example, have examined metabolic change across neuronal and dynamic power schemes, and not withstanding the fact that those mechanisms underpinning muscular adaptation, in relation to the metabolic stimulus, remain highly speculative. Inconsistent findings and methodological limitations within research (e.g. programme design, sampling period, number of samples) make interpretation further difficult. We contend that strength and power research needs to investigate those metabolic mechanisms likely to contribute to weight-training adaptation. Further research is also needed to examine the metabolic responses to different loading schemes, as well as interactions across age, sex and training status, so our understanding of how to optimise strength and power development is improved.

Biotransformation↗

Evaluation of the effects of khaya gum on the mechanical and release properties of paracetamol tablets.

A study of the comparative effects of khaya gum and two standard binding agents-polyvinylpyrrolidone (PVP) and gelatin--on crushing strength and friability, and the disintegration and dissolution characteristics of paracetamol tablets was made. The crushing strength-friability ratio (CSFR), the disintegration times, D, and the dissolution times t50, t90, and t1 (derived from the equation of Noyes and Whitney), all increased with an increase in binder concentration; however, the dissolution rate constants, k1 and k2, decreased. The ranking for the values of CSFR for tablets containing the different binders was PVP > gelatin > khaya gum. The ranking for D and the dissolution times was gelatin > khaya gum > PVP, whereas the ranking for the dissolution rate constants was PVP > khaya gum > gelatin. There were significant linear correlations between CSFR, D, t50, t90, and t1 for the tablets. There were also significant correlations between k1 and D, t50, t90, and t1, and between k2 and t90. The results suggest that khaya gum could be useful as an alternative binding agent to produce tablets with particular mechanical strength and drug release profiles.

Acetaminophen↗

Segmentation of bone CT images and assessment of bone structure using measures of complexity.

A nondestructive and noninvasive method for numeric characterization (quantification) of the structural composition of human bone tissue has been developed and tested. In order to quantify and to compare the structural composition of bones from 2D computed tomography (CT) images acquired at different skeletal locations, a series of robust, versatile, and adjustable image segmentation and structure assessment algorithms were developed. The segmentation technique facilitates separation from cortical bone and standardizes the region of interest. The segmented images were symbol-encoded and different aspects of the bone structural composition were quantified using six different measures of complexity. These structural examinations were performed on CT images of bone specimens obtained at the distal radius, humeral mid-diaphysis, vertebral body, femoral head, femoral neck, proximal tibia, and calcaneus. In addition, the ability of the noninvasive and nondestructive measures of complexity to quantify trabecular bone structure was verified by comparing them to conventional static histomorphometry performed on human fourth lumbar vertebral bodies. Strong correlations were established between the measures of complexity and the histomorphometric parameters except for measures expressing trabecular thickness. Furthermore, the ability of the measures of complexity to predict vertebral bone strength was investigated by comparing the outcome of the complexity analysis of the CT images with the results of a biomechanical compression test of the third lumbar vertebral bodies from the same population as used for histomorphometry. A multiple regression analysis using the proposed measures including structure complexity index, structure disorder index, trabecular network index, index of a global ensemble, maximal L-block, and entropy of x-ray attenuation distribution revealed an excellent relationship (r=0.959, r2=0.92) between the measures of complexity and compressive bone strength. In conclusion, the image segmentation techniques and the assessment of bone architecture by measures of complexity have been successfully applied to analyze high-resolution peripheral quantitative computed tomography (pQCT) and CT images obtained from the distal radius, humeral mid-diaphysis, third and fourth lumbar vertebral bodies, proximal femur, proximal tibia, and calcaneus. The proposed approach is of broad interest as it can be applied for the quantification of structures and textures originating from different imaging modalities in other fields of science.

Aged↗

In vivo degradation characteristics of poly(glycerol sebacate).

We have developed a series of biodegradable elastomers, poly(glycerol sebacate) (PGS), based on glycerol and sebacic acid. The polymers are potentially useful in soft tissue regeneration and engineering. To evaluate the performance of PGS in a physiological environment, we compared their degradation profiles with poly(DL-lactide-co-glycolide) (50:50, carboxyl ended, M(w) 15,000) in vivo. Among the parameters examined are changes in weight and mechanical strength with time, implant geometry, surface characteristics, and degree of swelling. Unlike poly(DL-lactide-co-glycolide), PGS primarily degrades by surface erosion, which gives a linear degradation profile of mass, preservation of geometry and intact surface, and retention of mechanical strength.

Absorbable Implants↗

Effects of magnesia and potassium sulfate on gypsum-bonded alumina dental investment for high-fusing casting.

The purpose of this study was to improve the characteristics of gypsum-bonded alumina investments using magnesia and potassium sulfate as chemical additives. Magnesia content improved fluidity, delayed setting reaction, increased green strength, and decreased setting expansion, when mixed with distilled water. When the investment was mixed with potassium sulfate, the setting time and setting expansion were reduced, and the thermal expansion increased, however, the green strength decreased. Therefore, the investment with a small amount of magnesia mixed with potassium sulfate was considered a suitable composition, having adequate setting behavior, enough green strength and sufficient compensate expansion for casting.

Aluminum Oxide↗

Effect of loading rate on endplate and vertebral body strength in human lumbar vertebrae.

Previous studies have implied that increases in loading rate resulted in changes in vertebral mechanical properties and these changes were causative factors in the different fracture types seen with high-speed events. Thus many researchers have explored the vertebral body response under various loading rate conditions. No other study has investigated the role of the endplate in high-speed vertebral injuries. The current study determined changes in the endplate and vertebral body strength with increases in displacement rate. The endplate and vertebral body failure loads in individual lumbar vertebrae were documented for two displacement rates: 10 and 2500 mm/s. Using cross-sectional areas from the endplate and vertebral body, failure stresses for both components were calculated and compared. Both the endplate and vertebral body failure loads increased significantly with increased loading rate (p<0.005). Although the vertebral body failure stress increased significantly with loading rate as well (p<0.01), the endplate stresses did not (p>0.35). In addition, the endplate and vertebral strengths were not significantly different under high-speed loading (p>0.60), which inhibits possible predictions as to which bony component would fail initially during a high-speed injury event. It is possible that load distribution may contribute more to the fracture patterns seen at high speeds over vertebral component strength.

Aged↗

Surface properties of calcium phosphate particles for self setting bone cements.

Calcium phosphate cements (CPC), consist of multicomponent powder mixtures of calcium orthophosphates with grain sizes in the region of 1-20 microm. Due to the small particle sizes surface properties as the zeta potential and adsorption processes play a significant role during manufacturing and application. In the context of this work zeta potentials of different calcium phosphates, like dicalcium phosphate anhydride (DPCA) tetracalcium phosphate (TTCP) and hydroxyapatite were measured in various organic/aqueous media with different pH values. The results show a strong dependency of the zeta potential on the kind of suspension medium used associated with different milling properties. The addition of sodium phosphate leads to a pH value dependent stabilization of the particles in the liquid phase; the zeta potential of the surface increases from about -15 to -18 mV in water and from -35 to -45 mV in 0.05 mol/l sodium phosphate solution. Besides the interaction of particles with various antibiotics was determined on the basis of the zeta potential of the surface. The substances partly cause a tremendous change of the surface load. This is accompanied by a change of the rheological properties of the cement paste, the morphology of the hardened cement matrix and a significant deterioration of the application-relevant properties as setting time or mechanical strength.

Anti-Bacterial Agents↗

Effect of shape and size of silanated fillers on mechanical properties of experimental photo cure composite resins.

The binary system of hybrid fillers selected from four irregular fillers (1.7-21.5 microns), five spherical fillers (0.46-31.2 microns), and a microfiller of 0.04 micron, were applied to photo cure composite resin and mechanical properties were measured. The strength for the hybrid of irregular and spherical fillers tended to increase as the size of component fillers decreased. The strength for the hybrid of the same fillers in shape also increased as the size of fillers decreased. The strength for the hybrid containing 30% microfiller showed the same trend, especially, the largest strength was obtained from hybrids containing small spherical fillers.

Analysis of Variance↗

The effect of veneering materials on stress distribution in implant-supported fixed prosthetic restorations.

In this study, the effect of various materials used in fabricating superstructures for implant-retained fixed partial dentures on stress distribution around implant tissues was investigated. Five different mathematical models consisting of 11,361 nodes and 54,598 elements were constructed to study porcelain, gold alloy, composite resin, reinforced composite resin, and acrylic resin veneering materials using the 3-dimensional finite element analysis method. MARC K7.2/Mentat 3.2 software was used for the analysis. Reference points were determined on the cortical bone, where perpendicular, oblique, and horizontal forces were applied. Stress values created by oblique and horizontal forces appeared to be higher than those created by vertical forces. Stress seemed to be concentrated at the cortical bone around the cervical region of the implant. Gold alloy and porcelain produced the highest stress values in this region. Stresses created by acrylic resin and reinforced composite resin were 25% and 15% less, respectively, than porcelain or gold alloy. Porcelain and gold alloy produced stress values at the lingual implant sites that reached the ultimate strength values of the cortical bone.

Acrylic Resins↗

A new technology for direct restorative alloys.

OBJECTIVES: The purpose of this study was to develop a new technology for preparing mercury-free metallic dental restorative materials. METHODS: The novel approach relies on the cold welding of surface treated silver particles. At ambient temperature, intermetallic compound formation takes place spontaneously at the silver-tin interface. The ability of a loose powder to consolidate at ambient temperature under moderate pressure and within a short time duration was investigated for various mixtures of elemental silver, tin, and pre-alloyed silver-coated powders. Surface treatment aimed at removing silver surface oxide layers is done with a dilute acid. The compressive and the transverse rupture strengths of several of the consolidated powder mixtures were determined. RESULTS: Cold-welding of surface-treated powder particles takes place across the silver-silver interface and is promoted by exposure to a mild acid. Powder mixtures containing approximately 50% silver powder, 40% silver-coated silver-tin intermetallic compound particles, and a small silver-tin fraction deposited from an aqueous solution display very good condensability, depending on the amount of silver-silver interface area available. The attained rupture strength values (200 Mpa) were higher than those of amalgams; the compressive strengths (120 MPa) and hardness values (100 KHN), however, were lower than those found for amalgams. SIGNIFICANCE: Mercury-free silver-tin powder mixtures can be processed for use as metallic composite dental restorative materials.

Analysis of Variance↗

Effect of excitation energy on dentine bond strength and composite properties.

A number of available dentine adhesives and dental composites require light activation for polymerization. There are many variables which affect the light absorbing properties (e.g. bond strength) of these materials. The purpose of this study was to determine the influence of excitation energy (EE) on the dentine shear bond strength (SBS) of two lengths (2.1 mm and 3.25 mm) of light-cured (or dual-cured) dentine adhesives/dental composites. Diametral tensile (DTS) and compressive (CS) strengths of the same composites were also studied as a function of EE. Three resin composites with their respective adhesives (Marathon One/Tenure, Z100/Scotchbond Multi-Purpose and Herculite XRV/Optibond) were used. Five commercial curing lights were used to produce spectra of 100-650 mW cm-2. The data were analysed using ANOVA and the Tukey LSD test. No significant correlation was observed at the P > 0.05 level between EE and SBS in the shorter specimens. The SBS of Optibond is independent of EE and composite length. The SBS data were also analysed with Weibull statistics. The characteristic strengths calculated varied between 14 and 27 MPa. For the composites tested, mean values of DTS varied between 33 and 54 MPa and CS varied between 167 and 414 MPa. The DTS and CS of Z100 were significantly greater than those of the other materials. Intensities > or = 250 mW cm-2 produced equivalent mechanical properties within all composite materials and equivalent bond strengths in systems which included dentine, adhesive and composite resin.

Absorption↗

Particle size distribution and evolution in tablet structure during and after compaction.

The objective of this study was to investigate the effect of the distribution in size of free-flowing particles for the evolution in tablet structure and tablet strength. For sucrose and sodium chloride, three powders of different size distributions were prepared by mixing predetermined quantities of particle size fractions. For paracetamol, three batches with varying particle size distributions were prepared by crystallisation. The powders were formed into tablets. Tablet porosity and tensile strength were determined directly after compaction and after short-term storage at two different relative humidities. Tablets were also formed after admixture of a lubricant (magnesium stearate) and the tablet tensile strength was determined. For the test materials used in this study, the spread in particle size had no influence on the evolution in tablet porosity and tensile strength during compression. However, the spread in particle size had a significant and complex influence on the short-term post-compaction increase in tablet tensile strength. The effect of the spread was related to the instability mechanism and the presence of lubricant. It is concluded that the distribution in size of free-flowing particles is not critical for the tablet porosity but may give significant effects on tablet tensile strength due to a post-compaction reaction.

Acetaminophen↗

[Strength testing of pins made of human femur cortical bone].

For biomechanical evaluation of cortical bone as a potential source for internal fixation devices, pins of 2 and 3 mm in diameter were made from fresh human femora and subjected to bending loads. Some of the pins were tested without further treatment; others were defatted and dried in acetone solution. Of the acetone-treated pins, some were autoclaved either at 121 degrees C for 20 min or at 134 degrees C for 8 min. Acetone treatment of the pins caused a 5.5% increase in bending strength (p < or = 0.05) and a 6.6% increase in the elastic modulus (p < or = 0.05). The mean bending strength of the acetone-treated pins was 257 +/- 52 N/mm2 and the mean elastic modulus was 18,346 +/- 1292 N/mm2. Autoclaving of the pins at the lower temperature for a longer time led to a decrease in the bending strength of up to 16% and at the higher temperature for a shorter time to a decrease of up to 41%. To compare the strengths of the cortical and synthetic pins, 2-mm Biofix pins were also tested. The Biofix pins showed a 25% higher bending strength than the acetone-treated pins but a 12.5% lower elastic modulus. It should be noted that in animal studies the synthetic Biofix pins showed a 20% loss of strength within 2 days after implantation in situ.

Bioprosthesis↗

Improvement of strength parameters of a leucite-reinforced glass ceramic by dual-ion exchange.

An innovative dual ion-exchange process can improve the limited strength and the scatter-in-strength of technical glasses. The objective of this study was to prove whether such a two-stage ion-exchange process can also improve the limited strength and the problematic scatter-in-strength of dental ceramic materials. The first exchange was done in KNO3 on a leucite-reinforced glass-ceramic material, the second exchange in 70 mol% KNO3, 30 mol% Na NO3 at different treatment times and temperatures. The dual-exchange process approximately doubled the Weibull strength. Moreover, the Weibull modulus showed a four-fold increase, i.e., the coefficients of variation were reduced from 18.3 to 4.7%. We conclude that the dual-exchange process may help significantly to increase the clinical reliability of glass-ceramic dental restorations, because the strength and the scatter-in-strength will be substantially improved by this treatment.

Aluminum Silicates↗

The effect on anterior column loading due to different vertebral augmentation techniques.

BACKGROUND: Vertebral compression fractures are a significant cause of morbidity amongst the elderly, resulting in pain, kyphosis, decreased mobility, and often depression. The two most popular operative treatments of compression wedge fractures are vertebroplasty and kyphoplasty, however, which method leads to restoration of normal spinal loading is unknown. METHODS: A cadaveric thoracolumbar spine model was fractured and then treated using one of two techniques: vertebroplasty or kyphoplasty. Three non-destructive loading regimes were applied to the intact, fractured and treated cases. Sub-adjacent nuclear pressure, used as a measure of anterior column loading, was determined for each experimental variant and loading case. FINDINGS: The data indicate that nuclear pressure was substantially reduced after the spine was fractured. These pressures were minimally increased after treatment, however, not to the level of the pre-fractured condition. In all loading cases, there were no significant differences between the two treatment types. INTERPRETATION: While our data show that both vertebroplasty and kyphoplasty allow the disc to generate higher nuclear pressures, neither treatment increased nucleus pulposus pressure above the level of the intact state. This directly relates to the clinical condition in that adjacent segment fractures sustained subsequent to either treatment is likely the result of overall disease progression, and not a direct result of the intervention.

Adult↗

Failure strength of the bovine caudal disc under internal hydrostatic pressure.

The structure of the disc is both complex and inhomogeneous, and it functions as a successful load-bearing organ by virtue of the integration of its various structural regions. These same features also render it impossible to assess the failure strength of the disc from isolated tissue samples, which at best can only yield material properties. This study investigated the intrinsic failure strength of the intact bovine caudal disc under a simple mode of internal hydrostatic pressure. Using a hydraulic actuator, coloured hydrogel was injected under monitored pressure into the nucleus through a hollow screw insert which passed longitudinally through one of the attached vertebrae. Failure did not involve vertebra/endplate structures. Rather, failure of the disc annulus was indicated by the simultaneous manifestation of a sudden loss of gel pressure, a flood of gel colouration appearing in the outer annulus and audible fibrous tearing. A mean hydrostatic failure pressure of 18+/-3 MPa was observed which was approximated as a thick-wall hoop stress of 45+/-7 MPa. The experiment provides a measurement of the intrinsic strength of the disc using a method of internal hydrostatic loading which avoids any disruption of the complex architecture of the annular wall. Although the disc in vivo is subjected to a much more complex pattern of loading than is achieved using simple hydrostatic pressurization, this latter mode provides a useful tool for investigating alterations in intrinsic disc strength associated with prior loading history or degeneration.

Animals↗