Cells for drug delivery platforms.
Explore the source record for details and available documents.
Biomedical subjects
Publications and source records attributed to A G Mikos.
Explore the source record for details and available documents.
Recombinant human transforming growth factor beta1 (TGF-beta1) was incorporated into biodegradable microparticles of blends of poly(DL-lactic-co-glycolic acid) (PLGA) and poly(ethylene glycol) (PEG) at 6 ng/1 mg microparticles. Fluorescein isothiocynate labeled bovine serum albumin (FITC-BSA) was coencapsulated as a porogen at 4 microg/1 mg of microparticles. The effects of PEG content (0, 1, or 5 wt %) and buffer pH (3, 5, or 7.4) on the protein release kinetics and the degradation of PLGA were determined in vitro for up to 28 days. The entrapment yield of TGF-beta1 was 83.4 +/- 13.1 and 54.2 +/- 12.1% for PEG contents of 0 and 5%, respectively. The FITC-BSA and TGF-beta1 were both released in a multiphasic fashion including an initial burst effect. Increasing the PEG content resulted in the decreased cumulative mass of released proteins. By day 28, 3.8 +/- 0. 1 and 2.8 +/- 0.3 microg (based on 1 mg microparticles) of loaded FITC-BSA and 3.4 +/- 0.2 and 2.2 +/- 0.3 ng of loaded TGF-beta1 were released into pH 7.4 phosphate buffered saline (PBS) from microparticles with 0 and 5% PEG, respectively. Aggregation of FITC-BSA occurred at lower buffer pH, which led to decreased release rates of both proteins. For microparticles with 5% PEG, 2.3 +/- 0.1 microg of FITC-BSA and 2.0 +/- 0.2 ng of TGF-beta1 were released in pH 7.4 buffer after 28 days, while only 1.7 +/- 0.3 microg and 1.3 +/- 0.4 ng of the corresponding proteins were released in pH 3 buffer. The degradation of PLGA was also enhanced at 5% PEG content, which was significantly accelerated at acidic pH conditions. The calculated half-lives of PLGA were 20.3 +/- 0.9 and 15.9 +/- 1.2 days for PEG contents of 0 and 5%, respectively, in pH 7.4 PBS and 14.8 +/- 0.4 and 5.5 +/- 0.1 days for 5% PEG in pH 7.4 and 3 buffers, respectively. These results suggest that PLGA/PEG blend microparticles are useful as delivery vehicles for controlled release of growth factors.
Recombinant human transforming growth factor beta1 (TGF-beta1) was incorporated into microparticles of blends of poly(DL-lactic-co-glycolic acid) (PLGA) and poly(ethylene glycol) (PEG) to create a delivery vehicle for the growth factor. The entrapment efficiency of TGF-beta1 in the microparticles containing 5% PEG was 40.3 +/- 1.2% for a TGF-beta1 loading density of 6.0 ng/1 mg of microparticles. For the same loading, 17.9 +/- 0.6 and 32.1 +/- 2.5% of the loaded TGF-beta1 was released after 1 and 8 days, respectively, followed by a plateau for the remaining 3 weeks. Rat marrow stromal cells showed a dose response to TGF-beta1 released from the microparticles similar to that of added TGF-beta1, indicating the activity of TGF-beta1 was retained during microparticle fabrication and after TGF-beta1 release. An optimal TGF-beta1 dosage of 1.0 ng/mL was determined through a 3-day dose response study for maximal alkaline phosphatase (ALP) activity. The TGF-beta1 released from the microparticles loaded with 6.0 ng TGF-beta1/1 mg of microparticles for the optimal dosage of TGF-beta1 enhanced the proliferation and osteoblastic differentiation of marrow stromal cells cultured on poly(propylene fumarate) substrates. The cells showed significantly increased total cell number, ALP activity, and osteocalcin production with values reaching 138,700 +/- 3300 cells/cm(2), 22.8 +/- 1.5 x 10(-7) micromol/min/cell, and 15.9 +/- 1.5 x 10(-6) ng/cell, respectively, after 21 days as compared to cells cultured under control conditions without TGF-beta1. These results suggest that controlled release of TGF-beta1 from the PLGA/PEG blend microparticles may find applications in modulating cellular response during bone healing at a skeletal defect site.
This study investigated the in vitro degradation of porous poly(DL-lactic-co-glycolic acid) (PLGA) foams during a 20-week period in pH 7.4 phosphate-buffered saline (PBS) at 37 degrees C and their in vivo degradation following implantation in rat mesentery for up to 8 weeks. Three types of PLGA 85 : 15 and three types of 50 : 50 foams were fabricated using a solvent-casting, particulate-leaching technique. The two types had initial salt weight fraction of 80 and 90%, and a salt particle size of 106-150 microm, while the third type had 90% initial weight fraction of salt in the size range 0-53 microm. The porosities of the resulting foams were 0.82, 0.89, and 0.85 for PLGA 85 : 15, and 0.73, 0.87, and 0.84 for PLGA 50 : 50 foams, respectively. The corresponding median pore diameters were 30, 50, and 17 microm for PLGA 85: 15, and 19, 17, and 17 microm for PLGA 50 : 50. The in vitro and in vivo degradation kinetics of PLGA 85: 15 foams were independent of pore morphology with insignificant variation in foam weight, thickness, pore distribution, compressive creep behavior, and morphology during degradation. The in vitro foam half-lives based on the weight average molecular weight were 11.1 +/- 1.8 (80%, 106-150 microm), 12.0 +/- 2.0 (90%, 106-150 microm), and 11.6 +/- 1.3 (90%, 0-53 microm) weeks, similar to the corresponding values of 9.4 +/- 2.2, 14.3 +/- 1.5, and 13.7 +/- 3.3 weeks for in vivo degradation. In contrast, all PLGA 50 : 50 foams exhibited significant change in foam weight, water absorption, and pore distribution after 6-8 weeks of incubation with PBS. The in vitro foam half-lives were 3.3 +/- 0.3 (80%, 106-150 microm), 3.0 +/- 0.3 (90%, 106-150 microm), and 3.2 +/- 0.1 (90%, 0-53 microm) weeks, and the corresponding in vivo half-lives were 1.9 micro 0.1, 2.2 +/- 0.2, and 2.4 +/- 0.2 weeks. The significantly shorter half-lives of PLGA 50: 50 compared to 85: 15 foams indicated their faster degradation both in vitro and in vivo. In addition, PLGA 50: 50 foams exhibited significantly faster degradation in vivo as compared to in vitro conditions due to an autocatalytic effect of the accumulated acidic degradation products in the medium surrounding the implants. These results suggest that the polymer composition and environmental conditions have significant effects on the degradation rate of porous PLGA foams.
This study investigated the in vitro degradation of porous poly(L-lactic acid) (PLLA) foams during a 46-week period in pH 7.4 phosphate-buffered saline at 37 degrees C. Four types of PLLA foams were fabricated using a solvent-casting, particulate-leaching technique. The three types had initial salt weight fraction of 70, 80, and 90%, and a salt particle size of 106-150 microm, while the fourth type had 90% initial weight fraction of salt in the size range 0-53 microm. The porosities of the resulting foams were 0.67, 0.79, 0.91, and 0.84, respectively. The corresponding median pore diameters were 33, 52, 91, and 34 microm. The macroscopic degradation of PLLA foams was independent of pore morphology with insignificant variation in foam weight, thickness, pore distribution, compressive creep behavior, and morphology during degradation. However, decrease in melting temperature and slight increase in crystallinity were observed at the end of degradation. The foam half-lives based on the weight average molecular weight were 11.6+/-0.7 (70%, 106-150 microm), 15.8+/-1.2 (80%, 106-150 microm), 21.5+/-1.5 (90%, 106-150 microm), and 43.0+/-2.7 (90%, 0-53 microm) weeks. The thicker pore walls of foams prepared with 70 or 80% salt weight fraction as compared to those with 90% salt weight fraction contributed to an autocatalytic effect resulting in faster foam degradation. Also, the increased pore surface/volume ratio of foams prepared with salt in the range 0-53 microm enhanced the release of degradation products thus diminishing the autocatalytic effect and resulting in slower foam degradation compared to those with salt in the range 106-150 microm. Formation and release of crystalline PLLA particulates occurred for foams fabricated with 90% salt weight fraction at early stages of degradation. These results suggest that the degradation rate of porous foams can be engineered by varying the pore wall thickness and pore surface/volume ratio.
New injectable, in situ crosslinkable biodegradable polymer composites were investigated consisting of poly(propylene fumarate) (PPF), poly(ethylene glycol)-dimethacrylate (PEG-DMA), and beta-tricalcium phosphate (beta-TCP). We examined the effects of the PEG-DMA/PPF double-bond ratio and beta-TCP content on the crosslinking characteristics of the composites including the maximum crosslinking temperature and the gel point, as well as the properties of the crosslinked composites such as the compressive strength and modulus, and the water-holding capacity. The maximum crosslinking temperature was constant averaging 39.7 degrees C for the composite formulations tested. The gel points varied from 8.0 +/- 1.0 to 12.6 +/- 2.5 min and were not affected by the relative amounts of PEG-DMA. The compressive strength at yield of PEG-DMA/PPF composites without beta-TCP increased from 5.9 +/- 1.0 to 11.2 +/- 2.2 MPa as the double-bond ratio of PEG-DMA/PPF increased from 0.38 to 1.88. An increase in compressive modulus was also observed from 30.2 +/- 3.5 to 58.4 +/- 6.2 MPa for the same range of the PEG-DMA/PPF double-bond ratio. Also, the addition of beta-TCP (33 wt%) enhanced the mechanical properties of all composites. The equilibrium water content of networks without beta-TCP increased from 21.7 +/- 0.2 to 30.6 +/- 0.2% for a double-bond ratio of PEG-DMA/PPF ranging from 0.38 to 1.88. However, the mechanical properties of the swollen composites under compression were smaller than the dry ones. These data demonstrate the feasibility of fabricating injectable biodegradable polymer composites with engineered mechanical properties for orthopedic tissue engineering.
The large number of orthopedic procedures performed each year, including many performed arthroscopically, have led to great interest in injectable biodegradable materials for regeneration of bone and cartilage. A variety of materials have been developed for these applications, including ceramics, naturally derived substances and synthetic polymers. These materials demonstrate overall biocompatibility and appropriate mechanical properties, as well as promote tissue formation, thus providing an important step towards minimally invasive orthopedic procedures. This review provides a comparison of these materials based on mechanical properties, biocompatibility and regeneration efficacy. Advantages and disadvantages of each material are explained and design criteria for injectable biodegradable systems are provided.
Macroporous poly(2-hydroxyethyl methacrylate) (p(HEMA)) hydrogels were prepared in the presence of a 0.3-0.7 M NaCl solution. The pore morphology of the p(HEMA) hydrogels was dependent on the concentration of NaCl for a constant monomer solution to aqueous solution ratio. Swelling studies showed an increase in equilibrium water content and hydrogel porosity as the NaCl concentration in the polymerization medium increased from 0 to 0.7 M. The equilibrium water content, however, decreased as the NaCl concentration in the swelling medium increased. The frozen water content increased and non-frozen water decreased with an increase in the NaCl concentration in the polymerization medium. Mechanical testing indicated that the elastic modulus of the hydrogels was not affected by the increased porosity until the pores became interconnected. These data suggest that the addition of NaCl to the polymerization medium results in a multi-phase separation during fabrication that produces macroporous hydrogels of controlled morphology.
Joint pain due to cartilage degeneration is a serious problem, affecting people of all ages. Although many techniques, often surgical, are currently employed to treat this affliction, none have had complete success. Recent advances in biology and materials science have pushed tissue engineering to the forefront of new cartilage repair techniques. This review seeks to condense information for the biomaterialist interested in developing materials for this application. Articular cartilage anatomy, types of injury, and current repair methods are explained. The need for biomaterials, current commonly used materials for tissue-engineered cartilage, and considerations in scale-up of cell-biomaterial constructs are summarized.
The objective of this study was to assess the osteoconductivity of a poly(propylene fumarate)/beta-tricalcium phosphate (PPF/beta-TCP) composite in vitro. We examined whether primary rat marrow stromal cells would attach, proliferate, and express differentiated osteoblastic function when seeded on PPF/beta-TCP substrates. Attachment studies showed that a confluent monolayer of cells had adhered to the substrates within an 8 h time frame for marrow stromal cells seeded at confluent numbers. Proliferation and differentiated function of the cells were then investigated for a period of 4 weeks for an initial seeding density of 42,000 cells/cm2. Rapid proliferation during the first 24 h as determined by 3H-thymidine incorporation was mirrored by an initial rapid increase in total cell number by DNA assay. A lower proliferation rate and a gradual increase in cell number persisted for the remainder of the study, resulting in a final cell number of 128,000 cells/cm2. Differentiated cell function was assessed by measuring alkaline phosphatase (ALP) activity and osteocalcin (OC) production throughout the time course. Both markers of osteoblastic differentiation increased significantly over a 4-week period. By day 28, cells grown on PPF/beta-TCP reached a maximal ALP activity of 11 (+/- 1) x 10(-7) micromol/min/cell, while the OC production reached 40 (+/- 1) x 10(-6) ng/cell. These data show that a PPF/beta-TCP composite exhibits in vitro osteoconductivity similar to or better than that of control tissue culture polystyrene.
A tissue-engineered implant is a biologic-biomaterial combination in which some component of tissue has been combined with a biomaterial to create a device for the restoration or modification of tissue or organ function. Specific growth factors, released from a delivery device or from co-transplanted cells, would aid in the induction of host parenchymal cell infiltration and improve engraftment of co-delivered cells for more efficient tissue regeneration or ameliorate disease states. The characteristic properties of growth factors are described to provide a biological basis for their use in tissue engineered devices. The principles of polymeric device development for therapeutic growth factor delivery in the context of tissue engineering are outlined. A review of experimental evidence illustrates examples of growth factor delivery from devices such as microparticles, scaffolds, and encapsulated cells, for their use in the application areas of musculoskeletal tissue, neural tissue, and hepatic tissue.
Poly (Propylene Fumarate) (PPF), a novel, bulk erosion, biodegradable polymer, has been shown to have osteoconductive effects in vivo when used as a bone regeneration scaffold (Peter, S. J., Suggs, L. J., Yaszemski, M. J., Engel, P. S., and Mikos, A. J., 1999, J. Biomater. Sci. Polym. Ed., 10, pp. 363-373). The material properties of the polymer allow it to be injected into irregularly shaped voids in vivo and provide mechanical stability as well as function as a bone regeneration scaffold. We fabricated a series of biomaterial composites, comprised of varying quantities of PPF, NaCl and beta-tricalcium phosphate (beta-TCP), into the shape of right circular cylinders and tested the mechanical properties in four-point bending and compression. The mean modulus of elasticity in compression (Ec) was 1204.2 MPa (SD 32.2) and the mean modulus of elasticity in bending (Eb) was 1274.7 MPa (SD 125.7). All of the moduli were on the order of magnitude of trabecular bone. Changing the level of NaCl from 20 to 40 percent, by mass, did not decrease Ec and Eb significantly, but did decrease bending and compressive strength significantly. Increasing the beta-TCP from 0.25 g/g PPF to 0.5 g/g PPF increased all of the measured mechanical properties of PPF/NVP composites. These results indicate that this biodegradable polymer composite is an attractive candidate for use as a replacement scaffold for trabecular bone.
Human recombinant bone morphogenetic protein-2 (rhBMP-2) has been proven effective in stimulating the regeneration of bone in both skeletal and extraskeletal locations. Through encapsulation within, and release from, biodegradable poly(DL-lactic-co-glycolic acid) (PLGA) microspheres, a proven vehicle for sustained delivery of various proteins, the local concentrations of rhBMP-2 could be maintained at optimal levels to stimulate bone regeneration and remodeling at the site of healing in diverse clinical settings. Thus the purpose of this work was to investigate the encapsulation of rhBMP-2 in PLGA microspheres and its biologic activity upon release. Using in vitro tests in simulated body fluids, the effect of rhBMP-2 released from PLGA microspheres upon osteoblast cell cultures was found to be statistically similar to the effect produced by positive controls consisting of nonencapsulated aqueous rhBMP-2 in simulated body fluids. This clarifies an important step in skeletal tissue engineering strategies aimed at the use of encapsulated rhBMP-2 to stimulate bone regeneration and remodeling.
The adhesion of marrow stromal osteoblasts and the adsorption of fetal bovine serum (FBS) proteins to end-capped poly(D,L-lactic acid) 50:50 (PLA50) of molecular weight 17,000 (PLA5017), non-end-capped PLA50 of molecular weight 11,000 (PLA5011h), and a diblock copolymer made of poly(ethylene glycol)-monomethyl ether of molecular weight 5,000 and PLA50 of molecular weight 20,000 (Me. PEG5-PLA20) were investigated. Cell attachment and proliferation on both PLA50 polymers were equally good. The block copolymer did not allow the proliferation of cells. However, the attached cells were highly differentiated and metabolically active in contrast to the cells on PLA50. Moreover, surface analysis studies using electron spectroscopy revealed that FBS proteins adsorbed well from aqueous solutions to the PLA50 surfaces while they adsorbed substantially less to the block copolymer. These results suggest that Me.PEG-PLA block copolymers may be used to regulate protein adsorption and, therefore, cell adhesion by varying the block composition of the copolymer.
Since the first published examination of poly(ethylenimine) (PEI) as a gene delivery vehicle, there has been a flurry of research aimed at this polycation and its role in gene therapy. Here we will briefly review PEI chemistry and the characterization of PEI/DNA complexes used for gene delivery. Additionally, we will note various PEI transfection considerations and examine findings involving other polycationic gene delivery vehicles used with cellular targeting ligands. The current state of our knowledge regarding the mechanism of PEI/DNA transfection will also be discussed. Finally, we will survey toxicity issues related to PEI transfection.
Poly(ethylenimine) (PEI) samples of various molecular weights and pHs were used to transfect endothelial cells to achieve levels of gene expression for comparison. PEIs with nominal molecular weights of 600, 1200, 1800, 10,000, and 70,000 Da were examined at pHs of 5. 0, 6.0, 7.0, and 8.0, and the results were recorded in terms of transfection efficiencies at 24, 48, 68, 92, and 120 h post-transfection. Trials were performed on the human endothelial cell-derived cell line EA.hy 926. We found that, for the polymers tested, transfection efficiency increased as the molecular weight of PEI increased. Representative values of PEIs at pH 6 and molecular weight 70,000 produced average transfection efficiencies of 25.6 +/- 7.9% (n = 8) at the greatest average expression levels, while PEI of molecular weight 10,000 yielded efficiencies of only 11.4 +/- 1.7% (n = 6). Transfection efficiencies for molecular weight 1,800 PEI were essentially zero, and PEIs of lower molecular weights produced no transfection at all. In contrast, the pH of the PEI solutions had no discernible effect on transfection. Optimal expression of the green fluorescent protein reporter occurred between 2 and 3 days post-transfection. The amount of reporter expression also was noted, as determined by the brightness of fluorescing cells under UV. The data obtained demonstrate that the molecular weight of the PEI carrier has an effect on transfection efficiency while the pH of the PEI solutions prior to DNA complexation has no such effect.
Poly(ethylenimine) (PEI) is one of a number of polycations that has been used successfully to transfer genes into living cells. Although PEI shows promise in the field of gene therapy, to date no rigorous proof of mechanism has been published regarding the fate of PEI/DNA administered for transfection. Here we show, by using fluorescent labeling and confocal microscopy, the paths of PEI/DNA complexes from endocytosis to gene expression. We found that complexes attach to cell surfaces and migrate into clumps that are endocytosed. The endocytotic vesicles grow in number and size and are occasionally seen to lyse. Most interesting is the fact that endocytosed PEI, whether administered with or without DNA, undergoes nuclear localization in the form of ordered structures.
We investigated the crosslinking characteristics of an injectable composite paste of poly(propylene fumarate) (PPF), N-vinyl pyrrolidinone (N-VP), benzoyl peroxide (BP), sodium chloride (NaCl), and beta-tricalcium phosphate (beta-TCP). We examined the effects of PPF molecular weight, N-VP/PPF ratio, BP/PPF ratio, and NaCl weight percent on the crosslinking temperature, heat release upon crosslinking, gel point, and the composite compressive strength and modulus. The maximum crosslinking temperature did not vary widely among formulations, with the absolute values falling between 38 degrees and 48 degrees C, which was much lower than that of 94 degrees C for poly(methyl methacrylate) bone cement controls tested under the same conditions. The total heat released upon crosslinking was decreased by an increase in PPF molecular weight and a decrease in N-VP/PPF ratio. The gel point was affected strongly by the PPF molecular weight, with a decrease in PPF molecular weight more rapidly leading to a gel point. An increase in initiator concentration had the same effect to a lesser degree. The time frame for curing was varied from 1-121 min, allowing the composite to be tailored to specific applications. The compressive strength and compressive modulus values increased with decreasing N-VP/PPF, increasing NaCl content, and increasing BP/PPF ratio. For all formulations, the compressive strength values fell between 1 and 12 MPa, and the compressive modulus values fell between 23 and 265 MPa. These data suggest that injectable PPF/beta-TCP pastes can be prepared with handling characteristics appropriate for clinical orthopedic applications and that the mechanical properties of the cured composites are suitable for trabecular bone replacement.