Structure and morphology changes during in vitro degradation of electrospun poly(glycolide-co-lactide) nanofiber membrane.

Electrospun poly(glycolide-co-lactide) (PLA10GA90, LA/GA ratio 10/90) biodegradable nanofiber membranes possessed very high surface area to volume ratios and were completely noncrystalline with a relatively lowered glass transition temperature. These characteristics led to very different structure, morphology, and property changes during in vitro degradation, which were examined systematically. A shrinkage study showed that the electrospun crystallizable but amorphous PLA10GA90 membranes exhibited a very small shrinkage percentage when compared with the electrospun membranes of noncrystallizable poly(lactide-co-glycolide) (PLA75GA25, LA/GA 75/25) and poly(d,l-lactide). Although the weight loss of electrospun PLA10GA90 membranes exhibited a similar degradation behavior as cast thin films, detailed studies showed that the structure and morphology changes in electrospun membranes followed different pathways during the hydrolytic degradation. After 1 day of degradation in buffer solution at 37 degrees C, electrospun PLA10GA90 membranes exhibited a sudden increase in crystallinity and glass transition temperature, due to the fast thermally induced crystallization process. The continuous increase in crystallinity and apparent crystal size, as well as the decrease in long period and lamellae thickness, indicated that the thermally induced crystallization was followed by a chain cleavage induced crystallization process. The mass loss rate was accelerated after 6 days of degradation. The increase in glass transition temperature during this period further confirmed that the degradation of PLA10GA90 nanofibers was initiated from the amorphous region within the lamellar superstructures. A mechanism of structure and morphology changes during in vitro degradation of electrospun PLA10GA90 nanofibers is proposed.

Calorimetry, Differential Scanning↗

Optimization and characterization of dextran membranes prepared by electrospinning.

Dextran is soluble in both water and organic solvents, so it could be a versatile biomacromolecule for preparing nanofibrous electrospun membranes by blending with either water-soluble bioactive agents or hydrophobic biodegradable polymers for biomedical applications. We have formulated electrospun dextran membranes, and the effects of various processing parameters on the membrane properties were investigated. It was found that uniform nanofibrous dextran membranes could be formed by using water, DMSO/water, and DMSO/DMF mixtures as solvents through adjusting the processing conditions (solution concentration, voltage, and the distance between the electrode and the collecting plate). When water was used as a solvent, up to 10% (w/w) of bovine serum albumin (BSA) or lysozyme could be directly incorporated into the dextran electrospun membrane without compromising its morphology. No significant effect of the electrospinning process on lysozyme activity was observed. The composite electrospun membranes consisting of poly(D,L-lactide-co-glycolide) (PLGA) and dextran were obtained using DMSO/DMF (50/50, volume ratio) mixture as solvents. For cross-linking the electrospun membrane, dextran was modified by substitution of methacrylate groups at the hydroxyl sites. It was found that the electrospun membranes prepared from methacrylated dextran can be cured by UV irradiation in the presence of 1% of 2,2-dimethoxy-2-phenylacetophenone (DMPA) as a photoinitiator.

Animals↗

Nanostructures of complexes formed by calf thymus DNA interacting with cationic surfactants.

Synchrotron small-angle X-ray scattering was used to study the nanostructures of the complexes formed by calf thymus DNA interacting with cationic lipids (or surfactants) of didodecyldimethylammonium bromide (DDAB), cetyltrimethylammonium bromide (CTAB), and their mixture with a zwitterionic lipid of 1-palmitoyl-2-hydroxy-sn-glycero-3-phosphocholine (PHGPC). The effects of lipid/DNA ratios, DNA chain flexibility, lipid topology, and neutral lipid mixing on the nanostructures of DNA-lipid complexes were investigated. The complexes between double-stranded DNA (dsDNA) and double-tailed DDAB formed a bilayered lamellar structure, whereas the complexes between dsDNA and single-tailed CTAB preferred a structure of 2D hexagonal close packing of cylinders. With single stranded DNA (ssDNA) interacting with CTAB, the complexes showed a Pm3n cubic structure due to the different chain flexibility between dsDNA and ssDNA. The lipid molecules bound by rigid dsDNA like to form cylindrical micelles, whereas lipids bound to flexible ssDNA could form spherical or short cylindrical micelles. The addition of the neutral single-chained PHGPC lipids to the CTAB lipids could induce a structural transition of dsDNA-lipid complexes from a 2D hexagonal to a multi-bilayered lamellar structure. The parallel DNA strands were intercalated in the water layers of lamellar stacks of the mixed lipid bilayers. The DNA-DNA spacing depended on the ratios of charged lipid to neutral lipid, and charged lipid to DNA, respectively.

Animals↗

Electro-spinning and electro-blowing of hyaluronic acid.

In this study, hyaluronic acid (HA) was electro-spun and electro-blown to prepare nonwoven nanofibrous membranes. Critical parameters for processing and corresponding effects on the membrane morphology were investigated using the methods of rheology and scanning electron microscopy (SEM). During electro-spinning, the optimal HA concentration window for nanofibrous formation was determined within a narrow range of 1.3-1.5 w/v %, corresponding to a solution viscosity range of 3-30 Pa s at a shear rate of 1 s(-1). SEM results indicated that, with increases in (1) the total concentration by blending of low molecular weight HA, (2) the evaporation rate by the addition of ethanol, and/or (3) the feeding rate of solution, the electro-spinning performance for creating nanofibers was improved. However, the improvement was not sufficient to achieve a consistent production of high quality nonwoven nanofiber membranes. This problem was overcome by a new electro-blowing process using the combination of air flow and electro-spinning. Although air blowing at room temperature around the spinneret orifice did not exhibit a remarkable enhancement of nanofiber formation of HA, the performance was significantly improved with an increase in the air blowing rate. SEM results showed that the temperature of air-blowing was the most effective parameter in ensuring HA nanofiber formation. As the temperature of the blown air increased from 25 to 57 degrees C, the nanofiber formation became consistent and uniform. A high quality HA nonwoven membrane of nanofibers was successfully produced by blowing air at 57 degrees C with a 70 ft(3)/hr flow rate.

Electricity↗