In vivo degradation of resin-dentin bonds produced by a self-etch and an etch-and-rinse adhesive.

Resin-dentin bonds are known to degrade in the relatively aggressive oral environment. In order to obtain greater insight into the interfacial degradation process, we examined, by using transmission electron microscopy (TEM), the interfacial ultrastructure of two adhesives bonded to dentin after 1 yr in vivo. Class V cavities were prepared on the buccal surfaces of 14 intact teeth of two monkeys and then restored by using either the two-step self-etch adhesive, Unifil Bond, or the two-step etch-and-rinse adhesive, Single Bond, in combination with the restorative microhybrid composite, Z250. After 1 yr, 10 other teeth were restored by using the same materials (controls). One day later, the monkeys were killed, following which the microtensile bond strength to dentin was determined and the interfacial ultrastructure was examined by TEM. Whereas no noticeable changes in the morphology of the resin-dentin interface were observed between the 1-d and 1-yr specimens for Unifil Bond, Single Bond exhibited signs of interfacial degradation, in particular at the bottom of the 3 microm-deep hybrid layer. In conclusion, the adhesive interface produced by the etch-and-rinse adhesive was less resistant to degradation than that produced by the self-etch system.

Acid Etching, Dental↗

Translucency and characteristics of newly developed polymer-based dental tooth coating material.

The purpose of this study was to evaluate the translucency and color change of simulated heavily discolored teeth using polymer-based dental tooth coating materials and flowable resin composites. Five shades of coating material and two shades of flowable resin composite were used. Colorimetric values of the materials in different shades were determined using the L*a*b* system of the Commission Internationale de l'Eclairage (CIE). Colorimetric examination was performed on white, black, and shade guide (C4) backgrounds using specimens of various thickness (0.2, 0.3, 0.5, 1.0, and 2.0 mm). New coating material showed less translucent than flowable resin composites. Moreover the new material showed the potential to improve the appearance of heavily discolored teeth when being applied as a thin first layer.

Analysis of Variance↗

Color and translucency of resin composites for layering techniques.

The purpose of this study was to evaluate the colors of resin composites used for the layering technique, as well as the translucency at various thickness. For the purpose of calculating the translucency parameter (TP), black and white backings were used to evaluate the CIELAB parameters of Filtek Supreme (3M) and Gradia Direct (GC) disks of various thicknesses (0.5, 1.0, 2.0, 3.0 and 4.0 mm) and of three different shades (enamel-shade, body-shade, and opaque-shade). As for the color of each shade, it was evaluated using 4mm thick specimens on the white backing. Regarding TP, the opaque-shades were less translucent than the other shades. It was also found that translucency increased exponentially as thickness was reduced--regardless of shade. Regarding color, enamel-shades were more bluish (especially in GD) compared to the other shades, and the opaque-shades displayed a brighter and yellowish characteristic. In the layering technique, it is fundamental to have an accurate knowledge about the translucency and colors of the materials/shades used.

Color↗

Micro-shear bond strength of five single-step adhesives to dentin.

The micro-shear bond strengths (MSBSs) of five single-step self-etch adhesives (Adper Prompt L-Pop [APL], AQ Bond plus [AQP], OBF-2 [OB2], Reactmer Bond [RB], and Xeno III [XIII]) were compared with that of a two-step self-etch adhesive, Clearfil SE Bond [SE]. The adhesives were applied on dentin surfaces, according to manufacturers' instructions, for bonding of resin composite to dentin. After 24 hours, a micro-shear bond test was carried out and the data were analyzed by one-way ANOVA and Bonferroni test (p<0.05). The mean MSBSs in MPa were APL: 22.8, AQP: 37.4, OB2: 34.7, RB: 28.3, XIII: 30.3, and SE: 47.2. Among the single-step adhesives, the MSBS of AQP and OB2 were significantly higher than APL (p<0.05). In conclusion, the single-step adhesives used in this study, apart from AQP, produced significantly lower MSBS than the two-step adhesive (p<0.05).

Acid Etching, Dental↗

Bisphenol A from dental polycarbonate crown upregulates the expression of hTERT.

Bisphenol A (BPA) is one of the endocrine-disrupting chemicals (EDCs) that possess estrogen-like biologic activity. Many dental materials have been reported to release BPA. However, there are few reports available on the release of BPA from dental polycarbonates. The purpose of this study was to investigate the release of BPA from dental polycarbonate crowns and to evaluate the estrogenic activity of BPA. Polycarbonate crowns were immersed in five solvents (water, ethanol, n-hepthane, acetic acid, and acetonitrile) at 37 or 65 degrees C for 24 h. The elution from the material was analyzed by high-performance liquid-chromatography (HPLC) and mass-spectrometry (MS) analysis. BPA release was detected corresponding to the degradation of dental polycarbonates under the some storage conditions (ethanol, acetic acid, and acetonitrile). A previous report proved that estrogen increased human telomerase catalytic subunit (hTERT) mRNA, whereas the effect of EDCs on the hTERT promoter has never been reported. The estrogenic activity of BPA was analyzed by luciferase assay with the use of the hTERT promoter. This assay revealed that BPA was a positive regulator of hTERT transcription. In addition, quantitative real-time PCR analysis showed that BPA increased the expression level of hTERT mRNA in MCF7 cells. Herein, it is demonstrated that hTERT is a new target of BPA.

Benzhydryl Compounds↗

Deproteinizing effects on resin-tooth bond structures.

This study investigated the effects of NaOCl on resin-tooth bonds to simulate the situations of long-term durability and caries invasion. Resin-tooth bonded specimens were produced with the use of two resin adhesives (Excite and One-Bond). Resin-tooth bonded beams (adhesive area; 0.9 mm2) were serially sectioned and the specimens were immersed in 10% NaOCl medium for 0 (control), 2, 4, and 6 h after being stored in water for 24 h. After immersion, microtensile bond tests were performed. SEM fractography was conducted to calculate each failure mode by image analysis. In addition, the adhesive interface was examined with the use of TEM. In the control specimens, enamel bond strengths had no difference between Excite (45.6 +/- 15.0) and One-Bond (56.9 +/- 12.9). On the other hand, dentin bond strengths had significant difference between Excite (80.6 +/- 21.2) and One-Bond (50.7 +/- 11.2). The bond strengths decreased with increased storage time for both systems with enamel and dentin bonds. The deteriorated mineralized dentin of beams resulted in bond-strength reduction for resin-enamel bonds. For dentin bonding, the adhesive interface was gradually dissolved from the outer to the center portion of the beam. The depletion of collagen fibrils within the demineralized dentin or hybrid layer deformation was found under SEM and TEM examinations. These morphological changes are responsible for bond strength reduction of resin-dentin bonds.

Dental Materials↗

Comparison of bonding efficacy of an all-in-one adhesive with a self-etching primer system.

The aim of this study was to compare the bonding efficacy of an all-in-one adhesive with that of a self-etching primer system by measuring microleakage after thermocycling and the microtensile bond strength (microTBS) to enamel and dentin. Circular class V cavities along cement-enamel junctions were prepared in 20 extracted human premolars. Each 10 teeth were bonded with either AD Bond (AD) or Clearfil SE Bond (SE), and filled with a resin composite (Charisma). After thermocycling and staining with 0.5% basic fuchsin, the microleakage at the coronal and apical walls was evaluated using longitudinal sections. In addition 20 premolars were used to measure microTBS at 24 h after bonding for these adhesives to enamel and dentin that corresponded to the coronal and apical walls of the class V cavities. AD showed more microleakage than SE in the coronal walls, but there was less microleakage in the apical walls and no difference in apical leakage between the two adhesives. microTBS (SD) in MPa to enamel and dentin were 25.2 (7.3) and 68.3 (9.4) for AD, and 35.8 (7.4) and 76.4 (7.8) for SE, respectively. AD gave a lower microTBS to enamel than did SE. The results suggested that the poor adaptation at the coronal wall in AD might be caused by the lower bond strength to enamel.

Acid Etching, Dental↗

Effects of incremental curing on contraction stresses associated with various resin composite buildups.

OBJECTIVE: The purpose of this study was to photoelastically evaluate contraction stresses associated with various resin composite build-up procedures, including incremental curing and the use of flowable composite for pulpless molars. METHOD AND MATERIALS: Life-sized photoelastic models of an endodontically treated molar were fabricated. The cavity represented a conservative access preparation and included four lateral walls. The following materials were used for buildup: dual-cured hybrid composite (Cleafil DC Core [DC], BIS-CORE [BC]); light-cured flowable composite (AELITEFLO LV [ALV]); and chemical-cured flowable composite (CORE-FLO [CF]). The photoelastic models were built up with the following techniques: bulk-cured (BDd [dual-cured DC], BDc [chemically-cured DC], BBd [dual-cured BC], and BC [CF]); and incremental-cured (1 mm gingivally + 3.5 mm occlusally; IAB [ALV + BC], ICB [CF + BC], and IBB [BC + BC]). Isochromatic fringes developed in the models were recorded photographically in the field of a circular polariscope, and maximum fringe order was determined. Five specimens were tested for each condition. RESULTS: Stress intensity of the build-up methods fell into two categories: high (BDd, BBd, BC, and IAB) and low (BDc, ICB, and IBB). The difference between high and low groups was statistically significant, except between BC and ICB. The maximum fringe order was developed around the point angles at the cavity floor for all the conditions tested. CONCLUSIONS: Type and setting mechanism of resin composite build-up technique had considerable influence on contraction stress. Incremental buildup using composites with low elastic modulus did not reduce contraction stress intensity compared with bulk-cured techniques.

Barium Compounds↗

Translucency of opaque-shade resin composites.

PURPOSE: To measure the translucency parameter of opaque-shade resin composites. The secondary purpose was to evaluate the ability of the materials to mask dark background color. METHODS: CIELAB coordinates (L*, a*, b*) of three resin composites: UniFil S (UF), Palfique Estelite (PE), and Filtek A110 (FA) were determined in two shades (Opaque A3 and A3) at 1 mm and 2 mm thickness on a white backing, a backing of material itself and a black backing using a colorimeter. From the L* a* b* of 2 mm thick specimens on the white and black backing, translucency parameter (TP) were calculated for each material and shade to evaluate opacity of the materials. In addition, CIELAB color differences (deltaE*) were also calculated from the L*, a*, b* of 1 mm and 2 mm thick specimens on the material itself and on black backing, in order to estimate effectiveness of the resin composite materials to mask dark background color. If the calculated deltaE* were above 2, color differences were estimated as "perceptible." RESULTS: The TP values of Opaque A3 shade resins were lower than those of A3 resins for all the materials evaluated. When comparing the materials used, the Opaque A3 shade of FA indicates a higher TP value than those indicated for the Opaque A3 shade of the other two materials, while the A3 shade of FA revealed a higher TP value than the A3 shade of UF. As for the deltaE* values, the deltaE* recorded for 1 mm-thick specimens were in the range of "perceptible" and larger than those of 2 mm specimens, regardless of the shades and materials. For the 2 mm specimens, all of the deltaE* values for the Opaque A3 shade were classified as "imperceptible," whereas all deltaE* values for A3 shade were evaluated as "perceptible." CLINICAL SIGNIFICANCE: The opaque-shade resin composites were less translucent than the usual composites. Hence, if a restoration was relatively thick, the opaque-shade resin composites might effectively mask the dark background color from the oral cavity. However, if a restoration was relatively thin, the opaque-shade resin composites could not mask the dark background color as well as the usual composites. Therefore, clinicians should take into consideration the effect of dark background color in the shade matching procedure for a relatively thin restoration, even if opaque-shade resin composite is used.

Color↗

Effect of bur-cut dentin on bond strength using two all-in-one and one two-step adhesive systems.

PURPOSE: To compare the microtensile bond strength (MTBS) of two all-in-one adhesive systems and one experimental two-step self-etching adhesive system to two types of bur-cut dentin. MATERIALS AND METHODS: Using one of the three adhesives, Xeno CF Bond (Xeno), Prompt L-Pop (PL), or the experimental two-step system ABF (ABF), resin composite was bonded to flat buccal and root dentin surfaces of eight extracted human premolars. These surfaces were produced using either regular-grit or superfine-grit diamond burs. After storage overnight in 37 degrees C water, the bonded specimens were sectioned into six or seven slices approximately 0.7 mm thick perpendicular to the bonded surface. They were then subjected to microtensile testing. The surfaces of the fractured specimens were observed microscopically to determine the failure mode. In addition, to observe the effect of conditioning, the two types of bur-cut dentin surfaces were conditioned with the adhesives, rinsed with acetone, and observed with SEM. RESULTS: When Xeno and PL were bonded to dentin cut with a regular-grit diamond bur, MTBS values were lower than to superfine bur-cut dentin, and failures occurred adhesively at the interface, whereas the experimental two-step adhesive showed no significant difference in microtensile bond strength between two differently cut surfaces. CONCLUSION: The all-in-one adhesives tested here improved bond strengths when bonded to superfine bur-cut dentin as a substrate, whereas the experimental two-step adhesive system showed unchanged bonding to both regular and superfine bur-cut dentin surfaces.

Acetone↗

In vitro testing of all-in-one adhesives as fissure sealants.

PURPOSE: To evaluate the clinical efficacy of all-in-one adhesives as fissure sealants. METHODS: Resin-enamel bonded specimens were fabricated between polished and ground enamel surfaces using two all-in-one adhesives (One-Up Bond F and Xeno CF Bond) and two resin sealants (Teethmate F-1 and Helioseal F). Specimen beams were prepared and microtensile bond tests were performed at a crosshead speed of 1 mm/minute. The bond strengths obtained were subjected to one-way ANOVA and Scheffe's F test (P < 0.05: n=12 for each group). To evaluate the etching effect of phosphoric acid and the all-in-one adhesives, the treated enamel surfaces (37% phosphoric acid, 40% phosphoric acid, or all-in-one adhesives) were examined by FE-SEM. RESULTS: The bond strengths of the two all-in-one adhesives tested to the polished enamel surface were significantly lower (P < 0.05) than to ground enamel. However, no significant differences (P > 0.05) were found between the polished and ground enamel surfaces for resin sealants using phosphoric acid. Under SEM examination, 37% or 40% phosphoric acid etched the enamel surface more than all-in-one adhesives.

Acid Etching, Dental↗

In vitro sealing performance of two one-step adhesive systems in cervical cavities.

PURPOSE: To evaluate the effects of 1) wall grinding status, 2) thermal stress, and 3) time of polishing on sealing performance of two one-step bonding systems in cervical cavities. MATERIALS AND METHODS: Semicircular cavities with dimensions of 3 x 3 x 1.5 mm were prepared along the CEJ of extracted human premolars. In experiment 1, the cavity walls were additionally ground with round steel diamond burs (regularly ground) or finished with superfine diamond burs. The cavities were treated with AQ Bond (AQ) or One-up Bond F (OB) and filled with a resin composite. Then thermocycling (5 degrees C to 55 degrees C, 1000 x) was performed. In experiment 2, the regularly ground cavities were used. After restoration, the teeth were subjected to thermocycling (1,000 to 5,000 x). In experiment 3, the restorations in the regularly ground cavities were polished immediately or 24 h after filling. No thermocycling was carried out in this group. All specimens were immersed in a dye solution for 2 h. Microleakage at coronal and apical walls was evaluated on the longitudinal sections of the restorations. RESULTS: For OB, the cavities finished with superfine burs exhibited more microleakage at the coronal wall than the regularly ground cavity (p < 0.05). The leakage at the coronal walls increased with the number of thermal cycles for both systems (p < 0.05). The delayed polishing generated better adaptation at the apical wall of AQ and at the coronal wall of OB (p < 0.05). CONCLUSION: Grinding status, thermocycling, and time of polishing had influences on the sealing performance of the two one-step adhesive systems.

Bicuspid↗

EWS/ETS fusions activate telomerase in Ewing's tumors.

EWS/ETS is a chimeric protein identified in most Ewing's sarcomas. Although EWS/ETS has been shown to activate transcription as a transcription factor, the detailed targets of EWS/ETS in transformed cells have not been clarified. Herein, we demonstrate that telomerase is a new target of EWS/ETS fusions. Both telomerase activity and the expression level of telomerase reverse transcriptase (TERT) mRNA were up-regulated in NIH3T3 cells transformed by EWS/E1AF and EWS/FLI1 as well as in two Ewing's sarcoma cell lines. Luciferase assay using the TERT promoter revealed that EWS/E1AF and EWS/FLI1 function as positive regulators of TERT transcription in an ETS binding site-independent manner. EWS/ETS appeared to be included in the initiation complex of TERT transcription and to cooperate with CREB-binding protein (CBP)/p300. When EWS/FLI1 was knocked down in Ewing's sarcomas cells by RNA interference, the expression level of TERT mRNA and the telomerase activity were significantly decreased. These findings indicate that EWS/ETS fusion proteins activate human telomerase activity in Ewing's tumors through up-regulation of TERT gene expression, probably as a transcriptional coactivator.

Adenovirus E1A Proteins↗

Nuclear export of adenovirus E4orf6 protein is necessary for its ability to antagonize apoptotic activity of BH3-only proteins.

The adenovirus E4orf6 is a viral oncoprotein known to cooperate with the E1A gene product in transforming primary murine cells. It has been shown to inhibit the apoptotic activities of p53 and p73 through direct binding to these proteins. Here, we demonstrate that the adenovirus E4orf6 protein inhibits apoptosis mediated by BNIP3 and Bik, which are BH3-only proteins of the Bcl-2 family. This activity was not mediated by p53 and p73 because E4orf6 had the same effect on the apoptosis in Saos-2 cells that do not express p53-related genes. It was also ascertained that E4orf6 could change the mitochondrial localization of BNIP3 and Bik. A mutant lacking the nuclear export signal of E4orf6 failed to inhibit apoptosis and to translocate BNIP3 protein from the mitochondria. Moreover, it was also established that E4orf6 was able to interact with BNIP3 and Bik. In BNIP3 protein, the region required for the interaction included the transmembrane domain, which is required for the localization of BNIP3 to the mitochondria. These results suggest that E4orf6 is exported from the nucleus to the cytoplasm, enabling it to interact with BH3-only proteins, eventually leading to the inhibition of apoptotic activity.

Active Transport, Cell Nucleus↗

Effect of sphered particles on the firing contraction of porcelain inlay processed by cold isostatic pressing.

The effect of the sphered particles on the contraction ratio of porcelain inlay processed by the cold isostatic pressure (CIP) method was investigated. The conventional lathe-cut porcelain powder was crushed to finer particles and the secondary particles with spherical shape by adding binders of acrylic resin, wax, and polyvinyl alcohol, respectively. Porcelain powder was molded as a disc-shaped green body in a refractory model and compressed at 200 MPa by CIP. From this green compact, the sintered porcelain was obtained by only one step of firing. The porcelain discs were then used for the measurements of contraction ratio, scanning microscopic observation, biaxial flexure strength, Vickers hardness, and density. Firing contraction was decreased to about 1% in the sphered particle groups, compared with 7% of the lathe-cut porcelain powder. Although biaxial flexure strength was about 85 MPa, which is lower than the 120 MPa of the control group, and the density was significantly decreased by about 10% from the 2.4 g/cm3 of the control substance, Vickers hardness, which ranged from 531 to 537, showed no significant differences among all of the groups. The CIP method could save labor in the process of making porcelain inlays, and sphered powders could contribute significantly to a decrease in the contraction ratio in the sintering process.

Biocompatible Materials↗

Degradation patterns of different adhesives and bonding procedures.

Various types of resin adhesives and procedures are available in the clinical field, so comprehensive understanding of degradation is required for each material and bonding procedure. The objective of this study was to investigate the bond durability for different adhesives and bonding procedures. Resin-dentin bonded beams were prepared with the use of two adhesives (One-Up Bond F/self-etching primer system and One Bond/total-etch adhesive) and two experimental groups for the bonding procedure (wet and dry bonding of the total-etch adhesive). Those samples were soaked in water for 24 h(control), 6 and 12 months. After the water immersion, the bond strengths were measured by the microtensile bond test, and subsequently fractography was performed with the use of SEM. Statistically significant reduction of the bond strength (p < 0.05) was apparent after 12 months of water exposure in the range 22-48% of the control. The bonding resin was eluted from the hybrid layer of the self-etching and the total-etch adhesives for the wet bonding. Micromorphological alterations were found due to the hydrolysis of collagen fibrils with the total-etch adhesive for the dry bonding mode. These pathologic alterations were in accord with the bond strength.

Adhesives↗

SEM and TEM analysis of water degradation of human dentinal collagen.

Recently several long-term studies have reported evidence of the hydrolytic degradation of collagen fibrils based on fractured surface observations after bond testing. Those studies suggested that one cause of the decline in the bond strength was the degradation of the collagen fibrils within the bonds. However, one concern has been raised that the dentinal collagen fibrils may be stable in water that does not contain oral bacteria or enzymes. Therefore, the present study aimed to clarify the micromorphological change in naked collagen fibrils after 500 days of water storage. To prepare exposed collagen fibrils, sectioned and polished human dentin surfaces were acid conditioned for 15 s with the use of two commercially available acid conditioners: All-Etch (10% phosphoric acid) and Uni-Etch (32% phosphoric acid) (Bisco, Inc.). Those specimens were stored in distilled water at 37 degrees C for 1 day (control) for 500 days. After the storage periods, the samples were examined with the use of SEM and TEM. Under SEM and TEM examination, micromorphological alterations (disarrangement of collagen web, widening the interfibrillar space, and the thinning diameter of collagen fibrils) were found in the specimens after 500 days in water.

Acid Etching, Dental↗

Submicron hiati in acid-etched dentin are artifacts of desiccation.

OBJECTIVES: The submicron hiatus represents a potential space between the base of the collagen network and the mineralized dentin when dentin is acid-etched for bonding. These spaces were observed in SEM studies after acid-etched dentin specimens were critical point dried or dehydrated in hexamethyldisilasane. However, they have never been identified in TEM studies of dentin hybrid layers. This study critically examined the cause of submicron hiati formation using a silver staining technique to measure nanoleakage. METHODS: Two multi-step, total-etch adhesives (One-Step, Bisco; Single Bond, 3M) and two single-step, self-etching adhesives (Prompt L-Pop, ESPE; One-Up Bond F, Tokuyama) were examined. Flat dentin surfaces were bonded with these adhesives and a lining composite. In each adhesive group, 0.8mm thick slabs from the same bonded tooth were coated with nail varnish applied 1mm from the bonded interfaces. The varnish was either left to dry completely for 10min before immersing in 50wt% silver nitrate (AgNO(3)) for 24h (group D), or painted on blotted tooth slabs that were immediately dropped into the AgNO(3) solution (group M). After developing, undemineralized, unstained, epoxy resin-embedded sections were prepared for transmission electron microscopy (TEM) to identify the amount and distribution of silver uptake. RESULTS: Nanoleakage patterns were observed in all adhesive-bonded teeth, regardless of brand. Fine reticular silver deposits were also found in the underlying undemineralized dentin. In group D, submicron hiati were seen as tunnels of heavy silver deposits beneath hybrid layers. Specifically, a hiatus occurred between the undemineralized intertubular dentin and a cohesively fractured layer of the same matrix that was attached to the base of the hybrid layer. Hiati were completely absent in group M, regardless of the brand of adhesive. SIGNIFICANCE: Submicron hiati are artifacts created by desiccation during specimen processing, and should be referred to as such in future studies of bonded dentin interfaces.

Acid Etching, Dental↗