BIO-OSS is an allergen-free bone substitute material of bovine origin, used to fill bone defects or to reconstruct ridge configurations. Seventy one patients (39 female, 32 male) received 126 BIO-OSS implantations. Some health parameters or habits were documented to eliminate possible risk factors of influence. The diameter of jaw defects filled with BIO-OSS was measured. There was a significant influence of the defect size on the healing result. In X-ray controls, BIO-OSS served to identify the surrounding native bone. The density of the BIO-OSS areas was higher than in control sites. These radiological results were supported by bone biopsies. Histologically, the permanency of the BIO-OSS was still recognizable after 6 years and longer. The ingrowth of newly formed bone in the BIO-OSS scaffold explained the increased density of the implanted regions. There were no clinical signs of BIO-OSS resorption. Therefore, we can assume that form corrections achieved by BIO-OSS insertions will last.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

A K Schlegel, K Donath. 1998. BIO-OSS--a resorbable bone substitute?. https://pubmed.ncbi.nlm.nih.gov/10186966/

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related citations

Filler-coupling agent-matrix interactions in silica/polymethylmethacrylate composites.

The interactions of the silane coupling agent methacryloxypropyltrimethoxysilane (MPS) with both fumed silica and a polymethylmethacrylate (PMMA) resin matrix were investigated using thermogravimetric analysis and Fourier transform infrared spectroscopy. OX 50 fumed silica was silanated with MPS at concentrations of 1% and 5% in aqueous ethanol (95%), acetone, and anhydrous toluene. Methyl methacrylate was polymerized with the silanated fumed silica (5% wt/wt) to form composites. The amount of MPS adsorption on the fumed silica and the amount of PMMA attached to the silanated fumed silica were determined by thermogravimetric analysis. MPS could be removed from the fumed silica after washing with methanol, but not after it underwent a drying process at 25 degrees C under vacuum. After vacuum drying at 25 degrees C, two types of adsorbed silane were found, i.e., firmly adsorbed and loosely adsorbed silane. The loosely adsorbed silane could desorb from silica and be incorporated into the polymer matrix through copolymerization with monomeric methyl methacrylate, resulting in crosslinking of the matrix. When the silanated silica was dried at 110 degrees C for 2 h, the loosely adsorbed silane was removed and the amount of firmly adsorbed silane increased. There was a positive correlation between the amount of firmly adsorbed MPS and the amount of PMMA attachment. The highest efficiency for PMMA attachment was found when MPS was adsorbed as a monolayer, because the loosely adsorbed silane did not contribute to the bonding of PMMA, and this suggested that not all of the double bonds of the MPS were accessible for reaction with the methacrylate monomer. Drying at 110 degrees C may also decrease the number of unsaturated double bonds of MPS.

Absorption↗

Colonic metabolism of ranitidine: implications for its delivery and absorption.

The aim of this study was to assess the in vitro stability of ranitidine to colonic bacteria by utilising a batch culture fermentation system to simulate the conditions of the colon. Three quantities of ranitidine, 100, 200 and 500 mg, in the form of the hydrochloride salt, were introduced into individual 100 ml fermenters consisting of buffer medium inoculated with freshly voided human faeces (10% w/v). Control experiments were also run in parallel using equivalent drug quantities in buffer medium without the presence of faeces. Samples were removed at pre-determined time intervals over a 24 h period and were subsequently analysed by high-performance liquid chromatography (HPLC) for drug concentration. A selection of the samples removed from the fermenters was also analysed by conventional UV spectroscopy and mass spectrometry. Subsequent to an initial dissolution phase in the fermentation system, a marked decline in ranitidine concentration was noted over time, thereby suggesting degradation and metabolism of the drug by colonic bacteria. No such decline in concentration was noted in the control buffer systems. The rate and extent of metabolism was rapid and complete within 12 and 24 h for the 100 mg and 200 mg samples, respectively, although the largest sample size, 500 mg, was only partly metabolised over the course of the experiment. UV and mass spectrometry analysis indicated that metabolism occurred via cleavage of an N-oxide bond within the molecule with the resultant loss of an oxygen atom, although further metabolic reactions are possible. Such metabolism may in part be responsible for the poor bioavailability of ranitidine from the colon.

Absorption↗

Effect of poly-L-arginine on the nasal absorption of FITC-dextran of different molecular weights and recombinant human granulocyte colony-stimulating factor (rhG-CSF) in rats.

The effect of poly-L-arginine (poly-L-Arg) on the in vivo nasal absorption of FITC-dextrans with a mean molecular weight ranging from 4.3 to 167 kDa and recombinant human granulocyte colony-stimulating factor (rhG-CSF) in rats were studied. When FITC-dextrans were co-administered intranasally with 1.0 w/v% poly-L-Args of different molecular weight (MW, ca. 45.5 and 92 kDa, poly-L-Arg (50) and poly-L-Arg (100)), the bioavailability (F(infinity)) increased markedly compared with that after administration of FITC-dextran alone. However, the F(infinity) decreased exponentially with the increasing molecular weight of FITC-dextrans. There was no significant difference between the enhanced nasal absorption of FITC-dextrans achieved by the co-administration of poly-L-Arg (50) and poly-L-Arg (100). Moreover, the relationship between the F(infinity) and the molecular weight of FITC-dextrans indicated that the molecular weight of protein drugs, which exhibited efficient absorption with poly-L-Arg, was about 20 kDa, when the lower limit of bioavailability for developing a potent transnasal delivery system was assumed to be about 10%. Indeed, the nasal absorption of rhG-CSF, which has a molecular weight of 18.8 kDa, was also increased after co-administration of 1.0 w/v% poly-L-Arg (50) and the F(infinity) was about 11%. It seems likely that poly-L-Arg can be used to provide adequate nasal absorption of various protein drugs which have a molecular weight of about 20 kDa, thereby allowing the successful development of a variety of transnasal drug delivery systems.

Absorption↗