PubMed Health⌕ Search

PubMed · 10530107

Ceramic materials more durable, suitable for fixed prosthetics.

Abstract

The practice of dentistry progressed with the recent developments and innovations in dental materials. The clinicians need to be familiar with these materials to successfully incorporate them in their practices. Fixed prosthodontics has assumed a growing role in the practice of restorative dentistry since the application of the lost wax casting technique. With the increased life expectancy, a greater demand of fixed prosthodontics is expected in the future. Recent material and technical and clinical advances have made treatment planing and decision-making more complex; most have attempted to improve current techniques to achieve the ideal pleasant smile. Intelligently planned, well documented, evidence-based research has provided a reliable foundation to many of these advances affecting the practice of fixed prosthodontics. This article will attempt to focus on some of these clinically relevant and applicable developments and briefly review the current literature and encourage pratictioners to review subsequent literature.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

S C Isikbay. Ceramic materials more durable, suitable for fixed prosthetics.. https://pubmed.ncbi.nlm.nih.gov/10530107/

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related citations

Threshold intensity factors as lower boundaries for crack propagation in ceramics.

BACKGROUND: Slow crack growth can be described in a v (crack velocity) versus KI (stress intensity factor) diagram. Slow crack growth in ceramics is attributed to corrosion assisted stress at the crack tip or at any pre-existing defect in the ceramic. The combined effect of high stresses at the crack tip and the presence of water or body fluid molecules (reducing surface energy at the crack tip) induces crack propagation, which eventually may result in fatigue. The presence of a threshold in the stress intensity factor, below which no crack propagation occurs, has been the subject of important research in the last years. The higher this threshold, the higher the reliability of the ceramic, and consequently the longer its lifetime. METHODS: We utilize the Irwin K-field displacement relation to deduce crack tip stress intensity factors from the near crack tip profile. Cracks are initiated by indentation impressions. The threshold stress intensity factor is determined as the time limit of the tip stress intensity when the residual stresses have (nearly) disappeared. RESULTS: We determined the threshold stress intensity factors for most of the all ceramic materials presently important for dental restorations in Europe. Of special significance is the finding that alumina ceramic has a threshold limit nearly identical with that of zirconia. CONCLUSION: The intention of the present paper is to stress the point that the threshold stress intensity factor represents a more intrinsic property for a given ceramic material than the widely used toughness (bend strength or fracture toughness), which refers only to fast crack growth. Considering two ceramics with identical threshold limits, although with different critical stress intensity limits, means that both ceramics have identical starting points for slow crack growth. Fast catastrophic crack growth leading to spontaneous fatigue, however, is different. This growth starts later in those ceramic materials that have larger critical stress intensity factors.

Ceramics↗

Partial ceramic crowns. Influence of preparation design and luting material on margin integrity--a scanning electron microscopic study.

This in vitro study examines the effects of three preparation designs and different luting agents on the marginal integrity of partial ceramic crowns. One hundred forty-four extracted human molars were prepared according to the following preparation designs: A. Coverage of functional cusps, B. Horizontal reduction of functional cusps and C. Complete reduction of functional cusps. Partial ceramic crowns (Vita Mark II, Cerec 3 System) were bonded to the cavities with: Variolink II/Excite (Vivadent), Panavia F/ED primer (Kuraray), Dyract/Prime and Bond NT (Detrey/Dentsply), and Fuji Plus/GC cavity conditioner (GC). The specimens were exposed to thermocycling and mechanical loading. Marginal adaptation was assessed on replicas using quantitative margin analysis in the scanning electron microscope (SEM). Significant differences were observed between the preparation designs in general. Coverage of functional cusps with preparation of butt joints and use of Variolink as luting material showed a tendency toward the lowest values for compromised adhesion, especially within the dentin. Significant differences could be determined between luting systems: resin-modified glass ionomer cement (RMGIC) caused fracture of the restorations and revealed higher values than all other luting materials for compromised adhesion at ceramic-luting agent and tooth-luting agent interfaces. The dentin-luting material interface, in general, showed higher percentages of compromised adhesion (38-100%) than enamel- and ceramic-luting material interfaces (0-30%). In conclusion, the SEM data indicate that, with adhesively bonded partial ceramic crowns, retentive preparation is not contraindicated and the choice of luting material is more relevant than the preparation design. Margins below the cemento-enamel junction reveal significant loss of adhesion in spite of adhesive luting techniques. The RMGIC cannot be recommended as a luting material for feldspathic partial ceramic crowns.

Ceramics↗

Marginal and internal adaptation of Class II ormocer and hybrid resin composite restorations before and after load cycling.

To overcome the shortcomings of the conventional composite restorative materials, ormocer materials have been introduced over the past few years. The purpose of this study was to evaluate the marginal and internal adaptation of two ormocer restorative systems (Admira, Voco and Definite, Degussa) compared to a hybrid composite one (TPH Spectrum, Dentsply/ DeTrey), before and after load cycling in Class II restorations. Standardized Class II restorations with cervical margins on enamel were divided into three groups ( n=16). Teeth of each group were filled with one of the restoratives tested and its respective bonding agent. Each group was divided into two equal subgroups. The marginal and internal adaptation of the first subgroup was evaluated after 7-day water storage at room temperature and of the second after cyclic loading in a mastication simulator (1.2x10(6) cycles, 49 N, 1.6 Hz). The occlusal and cervical marginal evaluation was conducted by videomicroscope and ranked as "excellent" and "not excellent". One thin section (150 microm), in mesial-distal direction, of each restoration, was examined under metallographic microscope to determine the quality of internal adaptation. The occlusal and cervical adaptation of both ormocer restorative systems was similar and clearly worse compared with the hybrid composite restorative one before as well as after load cycling. Concerning internal adaptation, no gap-free ormocer restorations were detected, whereas all Spectrum restorations presented perfect adaptation. The bonding agents of the ormocers formed layers with unacceptable features (pores, fractures) whereas that of the hybrid composite achieved perfect bonding layer even after loading. The rheological characteristics of the bonding agents of the ormocer restorative systems are proposed to be responsible for their inferior marginal and internal quality in Class II restorations compared with the hybrid composite one.

Ceramics↗