Fourteen titanium dental implants (Tioblast) were implanted singly in the proximal tibia of New Zealand rabbits for 120 days. A bone defect was surgically produced and filled with Bio-Oss around six of these implants. After the animals were sacrificed and their organs harvested, bone segments were fixed and methacrylate embedded after the push-in test had been performed. Microradiography was performed on longitudinal sections of the implants, whereas scanning electron microscope analysis was performed on the remaining embedded half-implants using secondary electrons only. The results showed that the implants were apically and coronally surrounded by bone, whether Bio-Oss was used or not. Fractures were evident through the newly formed bone and between the pre-existing and newly formed bone. Some fracture lines propagated through the bone and stopped at the implant surface without continuing along the bone-titanium interface. Detachment between the implant and the bone occurred at the coronal extremity of the implants and along its cervical region. These results highlight the fact that the bone-titanium interface has a high resistance to loading. It exhibited greater resistance than the newly formed bone and seems to behave in a manner similar to the cement lines of osteons.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
Davide Zaffe, Ruggero Rodriguez Y Baena, Silvana Rizzo, Cesare Brusotti, Monica Soncini, Riccardo Pietrabissa, Francesco Cavani, Virginio Quaglini. 2003-02-01. Behavior of the bone-titanium interface after push-in testing: a morphological study.. https://doi.org/10.1002/jbm.a.10366
Cite the original work for its findings. Save a collection to share your selection of sources.