Decrease in power output of new light-emitting diode (LED) curing devices with increasing distance to filling surface.

Abstract

PURPOSE: This study compares the percentage decrease in power output of light-emitting diode (LED) and quartz-tungsten-halogen (QTH) curing devices at different distances between the light guide tip and a radiometer. MATERIALS AND METHODS: Three LED curing devices (Elipar FreeLight/3M ESPE, Luxomax/Akeda, e-Light/GC) were compared to two QTH curing devices (Elipar TriLight/3M ESPE, Optilux 501 conventional and Turbo light guides/Kerr-Demetron). Power density was measured with a Fieldmaster GS/Coherent unit (Sensor LM-3 HTD) at increasing distances from the light guide tip (0 to 20 mm at 1-mm increments, n=6). RESULTS: The mean decrease in power density available for curing at a distance of 10 mm between the light guide tip and the radiometer was 68% for the FreeLight, 83% for the e-Light, 42% for the Luxomax, 38% for the TriLight, 33% for the Optilux with the standard light guide, and 44% for the Optilux with the turbo light guide. The power density of the Luxomax was only 40% of that of the other LED curing devices at 0 mm distance. CONCLUSION: The blue LED curing devices Elipar FreeLight and GC e-Light showed a significantly higher percentage decrease in power output at a distance of 10 mm from the light guide tip to the radiometer compared to the QTH curing devices. Therefore, although blue LED curing devices might have the same curing potential compared to a QTH device when placed in direct contact to a resin composite, blue LED curing devices may not provide a sufficient cure when placed at a clinically relevant distance of 10 mm to the resin composite surface.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Gerrit R Meyer, Claus-Peter Ernst, Brita Willershausen. 2002. Decrease in power output of new light-emitting diode (LED) curing devices with increasing distance to filling surface.. https://pubmed.ncbi.nlm.nih.gov/12666755/

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related citations

Modified dissolved organic matter fractionation technique for natural water.

A technique to fractionate dissolved organic materials (DOMs) from low DOM water (<5mg/l) was developed by using triple columns of DAX-8 adsorption resin, one column of AG-MP-50 cationic resin, and another column of WA 10 weak anionic resin in sequence. The procedure was then applied to fractionate water samples obtained at various sampling locations throughout two surface water treatment plants (WTPs) in central New Jersey to study its effectiveness, DOM occurrence, and variation along treatment units. The treatment plants utilize different treatment methods, hence producing variability in DOM fractions suitable for examining the procedure's effectiveness. This procedure was compared with current fractionation protocols and proved to be accurate in fractionation of low DOM water.

Composite Resins↗

Measurement of the optical density of packable composites: comparison between direct and indirect digital systems.

The aim of this study was to measure the optical density of four packable composite resins with widths of 1, 2, 3 and 4 mm, by means of Digora (direct) and DentScan DentView (indirect) digital imaging systems, in order to compare both methods. Twenty acrylic plates, with the proposed thicknesses, were used, each one containing a sample of each resin. Each acrylic plate was radiographed three times, under a standardized technique. For the Digora system, an optical plate was used under each resin sample, and, for the DentScan DentView system, occlusal films were employed, totalizing 60 exposures for each system. Optical plates and films were scanned and three consecutive optical readouts were carried out, totalizing 1,440 readouts. The results were submitted to statistical analysis and revealed that the average optical density of the four resins always increased as thickness increased. Regarding the comparisons between the composite resins, in both analysis the resin with the greater optical density was Surefil followed by Prodigy Condensable, Alert and Solitaire . The correlations between the results of Digora and DentScan DentView were significant for the different thicknesses and materials. The observed tendency is that as the values obtained with the Digora system increase, so do the values obtained with DentScan DentView . While thickness increased, the values of optical density in both Digora and DentScan DentView tended to approach each other. The Digora system presented smaller amplitude between the results obtained in adjacent thicknesses.

Composite Resins↗