Adhesion between the resin shell and composite resin.
Abstract
Adhesiveness between the resin shell and composite resin was examined. As the resin shell, SR-PE-ISOCETTE, made from thermosetting crown and bridge resin, was used. The shear bond strengths between the resin shell and photocurable composite resin bonded by various methods were measured after 1-day of immersion in water at 37 degrees C. Super-bond C & B treatment to the resin shell effectively improved the adhesiveness, giving a bond strength of about 14 MPa. Clearfil new bond, Clearfil porcelain bond, Unifast and MMA/TBBO treatment gave almost the same bond strengths of about 7-9 MPa. Silane coupling agents were not effective for improving the bond strength. It was revealed that 4-META was necessary for obtaining good adhesion between SR-PE-ISOCETTE and composite resin.
Explore related subjects
Keep this discovery
Explore connections, maps & timelines
M Aida, H Kanaya, Y Murata, T Hayakawa, K Horie. 1992. Adhesion between the resin shell and composite resin.. https://doi.org/10.2334/josnusd1959.34.167
Cite the original work for its findings. Save a collection to share your selection of sources.