Implant surfaces and interface processes.

The past decades and current R&D of biomaterials and medical implants show some general trends. One major trend is an increased degree of functionalization of the material surface, better to meet the demands of the biological host system. While the biomaterials of the past and those in current use are essentially bulk materials (metals, ceramics, polymers) or special compounds (bioglasses), possibly with some additional coating (e.g., hydroxyapatite), the current R&D on surface modifications points toward much more complex and multifunctional surfaces for the future. Such surface modifications can be divided into three classes, one aiming toward an optimized three-dimensional physical microarchitecture of the surface (pore size distributions, "roughness", etc.), the second one focusing on the (bio) chemical properties of surface coatings and impregnations (ion release, multi-layer coatings, coatings with biomolecules, controlled drug release, etc.), and the third one dealing with the viscoelastic properties (or more generally the micromechanical properties) of material surfaces. These properties are expected to affect the interfacial processes cooperatively, i.e., there are likely synergistic effects between and among them: The surface is "recognized" by the biological system through the combined chemical and topographic pattern of the surface, and the viscoelastic properties. In this presentation, the development indicated above is discussed briefly, and current R&D in this area is illustrated with a number of examples from our own research. The latter include micro- and nanofabrication of surface patterns and topographies by the use of laser machining, photolithographic techniques, and electron beam and colloidal lithographies to produce controlled structures on implant surfaces in the size range 10 nm to 100 microns. Examples of biochemical modifications include mono- or lipid membranes and protein coatings on different surfaces. A new method to evaluate, e.g., biomaterial-protein and biomaterial-cell interactions--the Quartz Crystal Microbalance--is described briefly.

Biocompatible Materials↗

Measurements Using the Quartz Crystal Microbalance Technique of Ferritin Monolayers on Methyl-Thiolated Gold: Dependence of Energy Dissipation and Saturation Coverage on Salt Concentration.

The adsorption kinetics of ferritin as a function of ionic strength has been studied with a new quartz crystal microbalance technique, allowing simultaneous measurement of the frequency shift (proportional to the mass uptake under certain conditions) and of changes in the energy dissipation caused by the adlayer. The measurements were performed with methyl-terminated (hydrophobic) thiol-covered gold surfaces, at pH 7.0 and ionic strengths in the range 1-200 mM KCl. The saturation uptake increases rapidly with increasing ionic strength in the range 20-50 mM and is then independent of ionic strength at >100 mM. The dissipation factor reveals, in the low coverage regime, distinct differences in the adlayer properties at low and high ionic strength, respectively. These results are briefly discussed in terms of the screening properties of the solvent and its influence on the protein-protein interaction in solution and on the surface. Copyright 1998 Academic Press.

Journal Article↗

Structural changes in hemoglobin during adsorption to solid surfaces: effects of pH, ionic strength, and ligand binding.

We have studied the adsorption of two structurally similar forms of hemoglobin (met-Hb and HbCO) to a hydrophobic self-assembled methyl-terminated thiol monolayer on a gold surface, by using a Quartz Crystal Microbalance (QCM) technique. This technique allows time-resolved simultaneous measurements of changes in frequency (f) (c.f. mass) and energy dissipation (D) (c.f. rigidity/viscoelastic properties) of the QCM during the adsorption process, which makes it possible to investigate the viscoelastic properties of the different protein layers during the adsorption process. Below the isoelectric points of both met-Hb and HbCO, the DeltaD vs. Deltaf graphs displayed two phases with significantly different slopes, which indicates two states of the adsorbed proteins with different visco-elastic properties. The slope of the first phase was smaller than that of the second phase, which indicates that the first phase was associated with binding of a more rigidly attached, presumably denatured protein layer, whereas the second phase was associated with formation of a second layer of more loosely bound proteins. This second layer desorbed, e.g., upon reduction of Fe3+ of adsorbed met-Hb and subsequent binding of carbon monoxide (CO) forming HbCO. Thus, the results suggest that the adsorbed proteins in the second layer were in a native-like state. This information could only be obtained from simultaneous, time-resolved measurements of changes in both D and f, demonstrating that the QCM technique provides unique information about the mechanisms of protein adsorption to solid surfaces.

Adsorption↗

Monte Carlo simulation of denaturation of adsorbed proteins.

Denaturation of model proteinlike molecules at the liquid-solid interface is simulated over a wide temperature range by employing the lattice Monte Carlo technique. Initially, the molecule containing 27 monomers of two types (A and B) is assumed to be adsorbed in the native folded state (a 3 x 3 x 3 cube) so that one of its sides is in contact with the surface. The details of the denaturation kinetics are found to be slightly dependent on the choice of the side, but the main qualitative conclusions hold for all the sides. In particular, the kinetics obey approximately the conventional first-order law at T > Tc (Tc is the collapse temperature for solution). With decreasing temperature, below Tc but above Tf (Tf is the folding temperature for solution), deviations appear from the first-order kinetics. For the most interesting temperatures, that is, below Tf, the denaturation kinetics are shown to be qualitatively different from the conventional ones. In particular, the denaturation process occurs via several intermediate steps due to trapping in metastable states. Mathematically, this means that (i) the transition to the denatured state of a given molecule is nonexponential, and (ii) the denaturation process cannot be described by a single rate constant kappar. One should rather introduce a distribution of values of this rate constant (different values of kappar correspond to the transitions to the altered state via different metastable states).

Adsorption↗

Monte Carlo simulation of the kinetics of protein adsorption.

Adsorption of proteins occurs via diffusion toward the interface, actual adsorption, and subsequent irreversible conformational changes resulting in denaturation of the native protein structure. The conventional kinetic models describing these steps are based on the assumption that the denaturation transitions obey the first-order law with a single value of the denaturation rate constant kappar. Meanwhile, recent Monte Carlo simulations indicate that, in general, the denaturation process cannot be described by a single rate constant kappar. One should rather introduce a distribution of this rate constant (physically, different values of kappar correspond to the transitions to the altered state via different metastable states). We have calculated the kinetics of irreversible adsorption of proteins with and without distribution of the denaturation rate constant kappar in the limits when protein diffusion in the solution is, respectively, rapid or slow. In both cases, the adsorption kinetics with distribution of kappar are found to be close to those with a single-valued rate constant kappar provided that the average value of kappar in the former case is equal to kappar for the latter case. This conclusion holds even for wide distributions of kappar. The consequences of this finding for the fitting of global experimental kinetics on the basis of phenomenological equations are briefly discussed.

Adsorption↗

Surface specific kinetics of lipid vesicle adsorption measured with a quartz crystal microbalance.

We have measured the kinetics of adsorption of small (12.5-nm radius) unilamellar vesicles onto SiO2, oxidized gold, and a self-assembled monolayer of methyl-terminated thiols, using a quartz crystal microbalance (QCM). Simultaneous measurements of the shift in resonant frequency and the change in energy dissipation as a function of time provide a simple way of characterizing the adsorption process. The measured parameters correspond, respectively, to adsorbed mass and to the mechanical properties of the adsorbed layer as it is formed. The adsorption kinetics are surface specific; different surfaces cause monolayer, bilayer, and intact vesicle adsorption. The formation of a lipid bilayer on SiO2 is a two-phase process in which adsorption of a layer of intact vesicles precedes the formation of the bilayer. This is, to our knowledge, the first direct evidence of intact vesicles as a precursor to bilayer formation on a planar substrate. On an oxidized gold surface, the vesicles adsorb intact. The intact adsorption of such small vesicles has not previously been demonstrated. Based on these results, we discuss the capacity of QCM measurements to provide information about the kinetics of formation and the properties of adsorbed layers.

Adsorption↗

In vitro real-time characterization of cell attachment and spreading.

A method based on the piezoelectric quartz crystal microbalance (QCM) technique for in vitro real-time characterization of cell attachment and spreading on surfaces has been developed. The method simultaneously measures the resonant frequency, f, and the dissipation energy, D, of the oscillating system. The QCM responses are sensitive to very small amounts (a few hundreds) of cells and highly specific to surface chemical properties. The first results from deposition of cells on two polystyrene surfaces of different wettability in serum-containing medium are reported. It has previously been shown that a decrease in f is related to the degree of cell spreading. In our data it appears that the extent or quality of cell attachment is reflected in an increase in D caused by adhering cells. The combined information from f and D measured by this technique might therefore be useful to probe cell-surface interactions for biomaterials.

Journal Article↗

Monte Carlo simulation of protein folding with orientation-dependent monomer-monomer interactions.

We present the results of lattice Monte Carlo simulations of protein folding in the framework of a model taking into account (i) the dependence of the energy of interaction of amino-acid residues on their orientation and (ii) the rigidity of the polypeptide chain with respect to the formation of kinks. If the chain is flexible, the final protein structures are predicted to be compact. Increasing the energy cost of creation of kinks is found to favor the formation of flat structures mimicking an ideal antiparallel beta sheet. For compact structures, the kinetics of folding exhibit the standard two-phase regime (a rapid collapse to one of the metastable stable, followed by slow reconfiguration of the chain to the native structure). For flat structures, the transition to the native state is often gradual.

Algorithms↗

Glow discharge plasma treatment for surface cleaning and modification of metallic biomaterials.

Glow discharge plasma treatment is a frequently used method for cleaning, preparation, and modification of biomaterial and implant surfaces. The merits of such treatments are, however, strongly dependent on the process parameters. In the present work the possibilities, limitations, and risks of plasma treatment for surface preparation of metallic materials are investigated experimentally using titanium as a model system, and also discussed in more general terms. Samples were treated by different low-pressure direct current plasmas and analyzed using Auger electron spectroscopy (AES), x-ray photoelectron spectroscopy (XPS), atomic force microscopy, scanning electron microscopy, and light microscopy. The plasma system is a home-built, ultra-high vacuum-compatible system that allows sample introduction via a load-lock, and precise control of pressure, gas composition and flow rate, etc. This system allows uniform treatment of cylindrical and screw-shaped samples. With appropriate plasma parameters, argon plasma remove all chemical traces from former treatments (adsorbed contaminants and other impurities, and native oxide layers), in effect producing cleaner and more well-controlled surfaces than with conventional preparation methods. Removal (sputtering) rates up to 30 nm/min are possible. However, when inappropriate plasma parameters are used, the result may be increased contamination and formation of unintentional or undesired surface layers (e.g., carbides and nitrides). Plasma-cleaned surfaces provide a clean and reproducible starting condition for further plasma treatments to form well-controlled surface layers. Oxidation in pure O2 (thermally or in oxygen plasmas) results in uniform and stoichiometric TiO2 surface oxide layers of reproducible composition and thicknesses in the range 0.5-150 nm, as revealed by AES and XPS analyses. Titanium nitride layers were prepared by using N2 plasmas. While mild plasma treatments leave the surface microstructure unaffected, heavy plasma treatment can give rise to dramatic morphologic changes. Comparison of these results with corresponding analyses of commercial implants and electropolished and/or anodically oxidized samples shows that the plasma treatment offers superior control of the surface status. However, it is also shown that improper control of the plasma process can produce unwanted and irreproducible results.

Argon↗

Bone response to surface modified titanium implants - studies on the tissue response after 1 year to machined and electropolished implants with different oxide thicknesses.

The bone formation around titanium implants with varied surface properties was investigated after 1 year in rabbits. Machined and electropolished samples with and without thick, anodically formed surface oxides were prepared, surface characterized and inserted in the cortical bone of rabbits. Scanning electron microscopy, scanning Auger electron spectroscopy and atomic force microscopy revealed marked differences in oxide thickness, surface topography and roughness, but no significant differences in surface chemical composition between the different groups of implants. Light microscopic morphology and morphometry showed that all implants were in contact with bone and had a large proportion of bone within the threads. There were no significant differences between the differently prepared implant groups. Our study shows that a high degree of bone contact and bone formation is achieved after 1 year with titanium implants which are modified with respect to oxide thickness and surface topography. There is no indication that a reduction of surface roughness, which in the initial phase decreases the rate of bone formation, had any influence on the amount of bone after 1 year in rabbit cortical bone.

Journal Article↗

Structure of the interface between rabbit cortical bone and implants of gold, zirconium and titanium.

The role of surface properties (chemical and structural) for the interaction between biomaterials and tissue is not yet understood. In the present study, implants made of titanium, zirconium (transition metals with surface oxides) and gold (metallic surface) were inserted into the rabbit tibia. Light microscopic (LM) morphometry showed that after 1 and 6 mo the gold implants had less amount of bone within the threads and a lower degree of bone-implant contact than the titanium and zirconium implants, which did not differ from each other. These quantitative differences were supported by LM and ultrastructural observations of the interface. The ultrastructural observations in addition demonstrated that the layer of non-collagenous amorphous material located between the implant and the calcified bone was appreciably thicker around zirconium than around titanium implants. The factors potentially responsible for the observed morphological differences in the bone around the different material surfaces are discussed.

Journal Article↗

Morphological and chemical characterization of microfabricated fibres for biological applications.

Monodisperse fibres and particulates of different materials with controllable three-dimensional shape, size and chemical composition are of interest in research on toxic respirable fibres as well as wear debris around orthopaedic implants. We have previously demonstrated the production of well-controlled, metal and oxide microfabricated fibres having dimensions 0.1 to 10 microm. While our previous results focused on how controlled fibres can be prepared by microfabrication methods, this paper evaluates property-production relationships for microfabricated fibres. Here we have briefly reviewed the production of 0.1 microm x 0.5 microm x 10 microm microfabricated fibres made by electron beam lithography from evaporated titanium or silicon oxide films using a double lift-off method. We have also analysed the properties of these fibres with respect to morphology and chemical composition, and how they are affected by variations in the production process. Two different solution types have been used to place fibres into liquid suspension and to clean and sterilize them for biological testing. One method involves the use of organic solvents; the other a hydroxide solution and water. While fibre dimensions appear to be material-specific, differences can be corrected for by compensation of the size of the lithographic pattern. Similarly the crystallinity of fibres is material-specific, as is to be expected of evaporated thin films, but should be possible to modify by varying deposition parameters or heat treating, for example. Of the cleaning methods used, the one using an aqueous hydroxide solution is preferred over solvent cleaning, as it is easier to perform and appears to be more effective at removing resist from the fibre suspension.

Journal Article↗

Simultaneous frequency and dissipation factor QCM measurements of biomolecular adsorption and cell adhesion.

We have measured the energy dissipation of the quartz crystal microbalance (QCM), operating in the liquid phase, when mono- or multi-layers of biomolecules and biofilms form on the QCM electrode (with a time resolution of ca. 1 s). Examples are taken from protein adsorption, lipid vesicle adsorption and cell adhesion studies. Our results show that even very thin (a few nm) biofilms dissipate a significant amount of energy owing to the QCM oscillation. Various mechanisms for this energy dissipation are discussed. Three main contributions to the measured increase in energy dissipation are considered. (i) A viscoelastic porous structure (the biofilm) that is strained during oscillation, (ii) trapped liquid that moves between or in and out of the pores due to the deformation of the film and (iii) the load from the bulk liquid which increases the strain of the film. These mechanisms are, in reality, not entirely separable, rather, they constitute an effective viscoelastic load. The biofilms can therefore not be considered rigidly coupled to the QCM oscillation. It is further shown theoretically that viscoelastic layers with thicknesses comparable to the biofilms studied in this work can induce energy dissipation of the same magnitude as the measured ones.

Adsorption↗

Chemical characterization and reactivity of iron chelator-treated amphibole asbestos.

Iron in amphibole asbestos is implicated in the pathogenicity of inhaled fibers. Evidence includes the observation that iron chelators can suppress fiber-induced tissue damage. This is believed to occur via the diminished production of fiber-associated reactive oxygen species. The purpose of this study was to explore possible mechanisms for the reduction of fiber toxicity by iron chelator treatments. We studied changes in the amount and the oxidation states of bulk and surface iron in crocidolite and amosite asbestos that were treated with iron-chelating desferrioxamine, ferrozine, sodium ascorbate, and phosphate buffer solutions. The results have been compared with the ability of the fibers to produce free radicals and decompose hydrogen peroxide in a cell-free system in vitro. We found that chelators can affect the amount of iron at the surface of the asbestos fibers and its valence, and that they can modify the chemical reactivity of these surfaces. However, we found no obvious or direct correlations between fiber reactivity and the amount of iron removed, the amount of iron at the fiber surface, or the oxidation state of surface iron. Our results suggest that surface Fe3+ ions may play a role in fiber-related carboxylate radical formation, and that desferrioxamine and phosphate groups detected at treated fiber surfaces may play a role in diminishing and enhancing, respectively, fiber redox activity. It is proposed that iron mobility in the silicate structure may play a larger role in the chemical reactivity of asbestos than previously assumed.

Asbestos, Amphibole↗

Bone response to surface-modified titanium implants: studies on the early tissue response to machined and electropolished implants with different oxide thicknesses.

The bone formation around titanium implants with varied surface properties is investigated. Machined and electropolished samples with and without thick, anodically formed surface oxides were prepared, surface characterized and inserted in the cortical bone of rabbits (1, 3 and 6 weeks). Scanning electron microscopy, scanning Auger electron spectroscopy and atomic force microscopy revealed marked differences in oxide thickness, surface topography and roughness, but no significant differences in surface chemical composition, between the different groups of implants. Light microscopic morphology and morphometry showed that all implants were in contact with bone and had a large proportion of bone within the threads at 6 weeks. The smooth, electropolished implants, irrespective of anodic oxidation, were surrounded by less bone than the machined implants after 1 week. After 6 weeks the bone volume as well as the bone-implant contact were lower for the merely electropolished implants than for the other three groups. Our study shows that a high degree of bone contact and bone formation are achieved with titanium implants which are modified with respect to oxide thickness and surface topography. However, the result with the smooth (electropolished) implants indicates that a reduction of surface roughness, in the initial phase, decreases the rate of bone formation in rabbit cortical bone.

Animals↗

Bone response to surface modified titanium implants: studies on electropolished implants with different oxide thicknesses and morphology.

In a series of experimental studies, bone formation was analysed around systematically modified titanium implants. In the present study, machined, electropolished and anodically oxidized implants were prepared, surface characterized and inserted in the cortical bone of rabbits (7 wks and 12 wks). SEM, scanning Auger electron spectroscopy and atomic force microscopy revealed no differences in surface composition but marked differences in oxide thickness, surface topography and roughness. Light microscopic morphology and morphometry showed that all implants were in contact with bone, and had a large proportion of bone within the threads. The smooth, electropolished implants were surrounded by less bone than the machined implants with similar oxide thickness, (4-5 nm) and the anodically oxidized implants with thicker oxides (21 nm and 180 nm, respectively) after 7 wks. These studies show that a high degree of bone contact and bone formation can be achieved with titanium implants which are modified with respect to oxide thickness and surface topography. However, it appears that a reduction of surface roughness may influence the rate of bone formation in rabbit cortical bone.

Animals↗