Metallic materials stimulating bone formation.

Abstract

Metallic materials implanted into bone defects are generally encapsulated by a fibrous tissue. Some metallic materials such as titanium and tantalum, however, have been revealed to bond to the living bone without forming the fibrous tissue, when they were subjected to NaOH solution and heat treatments. Thus treated metals form bone tissue around them even in muscle, when they take a porous form. This kind of osteoconductive and osteoinductive properties are attributed to sodium titanate or tantalate layer on their surfaces formed by the NaOH and heat treatments. These layers induce the deposition of bonelike apatite on the surface of the metals in the living body. This kind of bioactive metals are useful as bone substitutes even highly loaded portions, such as hip joint, spine and tooth root.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

T Kokubo. 2004. Metallic materials stimulating bone formation.. https://pubmed.ncbi.nlm.nih.gov/15468833/

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related citations

Electrolytic deposition of calcium phosphate/chitosan coating on titanium alloy: growth kinetics and influence of current density, acetic acid, and chitosan.

Electrolytically deposited calcium phosphate/chitosan coating demonstrated good bone marrow stromal cell attachment. The aim of this study was to understand the coating's growth kinetics as well as the effects of current density, acetic acid, and chitosan on the coating's formation. The scanning electron micrographs found that calcium phosphate crystals homogeneously distributed into chitosan aggregates as early as 30 min. X-ray diffraction patterns and Fourier transform infrared spectra demonstrated that the coating experienced a compositional conversion from octacalcium phosphate to carbonate apatite during the deposition process. Electric current influenced the deposition. Higher current density accelerated the process and induced faster and more chitosan deposition. Both acetic acid and chitosan were found to inhibit calcium phosphate deposition. Chitosan was thought to induce stronger effects than acetic acid did. Furthermore, the inhibitive effect related to their concentration in the electrolyte. When chitosan concentration increased to a certain degree, this inhibitive effect not only affected calcium phosphate deposition, but also affected its own deposition. The chitosan content within the hybrid coating was small, which could be verified through Raman spectrum. At the same time, no clear evidence of chemical reactions could be found between these two components. We considered that both components were just naturally wrapped to form as a whole.

Alloys↗

Corrosion resistance of a laser spot-welded joint of NiTi wire in simulated human body fluids.

The purpose of this study was to investigate corrosion resistance of a laser spot-welded joint of NiTi alloy wires using potentiodynamic tests in Hank's solution at different PH values and the PH 7.4 NaCl solution for different Cl- concentrations. Scanning electron microscope observations were carried out before and after potentiodynamic tests. The composition of a laser spot-welded joint and base metal were characterized by using an electron probe microanalyzer. The results of potentiodynamic tests showed that corrosion resistance of a laser spot-welded joint of NiTi alloy wire was better than that of base metal, which exhibited a little higher breakdown potential and passive range, and a little lower passive current density. Corrosion resistances of a laser spot-welded joint and base metal decreased with increasing of the Cl- concentration and PH value. The improvement of corrosion resistance of the laser spot-welded joint was due to the decrease of the surface defects and the increase of the Ti/Ni ratio.

Alloys↗

Plasma-immersion ion-implanted nitinol surface with depressed nickel concentration for implants in blood.

Ion implantation into nitinol had been shown previously to decrease the surface nickel concentration of this alloy and produce a titanium oxide layer. Nothing is known yet about the blood compatibility of this surface and the suitability for implants in the blood vessels, like vascular stents. Nickel depletion of superelastic nitinol was obtained by oxygen or helium plasma-immersion ion implantation. The latter leads to the formation of a nickel-poor titanium-oxide surface with a nanoporous structure, which was used for comparison. Fibrinogen adsorption and conformation changes, blood platelet adhesion, and contact activation of the blood clotting cascade have been checked as in vitro parameters of blood compatibility; metabolic activity and release of cytokines IL-6 and IL-8 from cultured endothelial cells on these surfaces give information about the reaction of the blood vessel wall. The oxygen-ion-implanted nitinol surface adsorbed less fibrinogen on its surface and activated the contact system less than the untreated nitinol surface, but conformation changes of fibrinogen were higher on the oxygen-implanted nitinol. No difference between initial and oxygen-implanted nitinol was found for the platelet adherence, endothelial cell activity, or cytokine release. The nanoporous, helium-implanted nitinol behaved worse than the initial one in most aspects. Oxygen-ion implantation is seen as a useful method to decrease the nickel concentration in the surface of nitinol for cardiovascular applications.

Alloys↗