We developed a new titanium spray technique using an inert gas shielded arc spray (titanium arc spray). Hydroxyapatite (HA)-coating can be applied to the implant without any surface pore obstruction after the rough surface is made by this technique. Scanning electron microscopy (SEM) of various porous implant surfaces after HA-coating revealed that the bead and fiber metal-coated implants had either a pore obstruction or an uneven HA-coating. On the other hand, the titanium arc sprayed implant demonstrated an even HA-coating all the way to the bottom of the surface pore. In the first set of animal experiments (Exp. 1), the interfacial shear strength to bone of four kinds of cylindrical Ti-6A1-4V (Ti) implants were compared using a canine transcortical push-out model 4 and 12 weeks after implantation. The implant surfaces were roughened by titanium arc spray (group A-C) and sand blasting (group D) to four different degrees (roughness average, Ra = group A: 56.1, B: 44.9, C: 28.3, D: 3.7 microns). The interfacial shear strength increased in a surface roughness-dependent manner at both time periods. However, the roughest implants (group A) showed some failed regions in the sprayed layers after pushout test. In the second set of animal experiments (Exp. 2), four kinds of Ti implants; HA-coated smooth Ti (sHA) with Ra of 3.4 microns, bead-coated Ti (Beads), titanium arc sprayed Ti (Ti-spray) with Ra of 38.1 microns and HA-coated Ti-spray (HA + Ti-spray) with Ra of 28.3 microns were compared using the same model as that in Exp. 1. The interfacial shear strength of HA + Ti-spray was significantly greater than that of sHA and Beads at both time periods, and that of Ti-spray at 4 weeks. Although a histological examination revealed that HA-coating enhanced bone ingrowth, sHA showed the lowest shear strength at both time periods. SEM after pushout test showed that sHA consistently demonstrated some regional failure at the HA-implant substrate interface. HA + Ti-spray had many failed regions either at the HA-bone interface or within the bone tissue rather than at the HA-implant substrate interface. These results suggested that the HA-coated smooth surfaced implants had a mechanical weakness at the HA-substrate interface. Therefore, HA should be coated on the rough surfaced implants to avoid a detachment of the HA-coating layer from the substrate and thus obtain a mechanical anchoring strength to bone. HA-coating on this new type of surface morphology may thus lead to a solution to the problems of conventional HA-coated and porous-coated implants.

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Y Nakashima, K Hayashi, T Inadome, K Uenoyama, T Hara, T Kanemaru, Y Sugioka, I Noda. 1997-06-05. Hydroxyapatite-coating on titanium arc sprayed titanium implants.. https://doi.org/10.1002/(sici)1097-4636(19970605)35%3A3%3C287%3A%3Aaid-jbm3%3E3.0.co%3B2-d. https://pubmed.health/record/pubmed%3A9138063/hydroxyapatite-coating-on-titanium-arc-sprayed-titanium-implants

Citations retain the original authors and DOI and include this site’s record URL. If this discovery service contributed to your research, you can also cite PubMed Health by Indiciae: BibTeX · RIS.

KEEP EXPLORING

Related citations

Electrochemical characterization of albumin protein on Ti-6AL-4V alloy immersed in a simulated plasma solution.

The effect of oxygen and albumin on the electrochemical behavior of a Ti-6Al-4V alloy immersed in a simulated inorganic plasma (SIP) solution was studied with a rotating-cylindrical electrode configuration to focus on the surface/electrolyte reactions. Potentiokinetic scans and electrochemical impedance spectroscopy have been used to characterize the interface by determining the passive current density and capacitance. For the polarization scans, an albumin addition of 37.7 mg/cm(3) to the SIP solution (oxygenated and unoxygenated) decreased the passive current density, indicating a lowering of the corrosive rate. The surface capacitance for the Ti-6Al-4V alloy immersed in a SIP solution averaged 13 microF/cm(2), which transformed after albumin addition (37.7 mg/cm(3)) from a potential independent behavior to the capacitance ranging from 23 to 6 microF/cm(2) with increasing potentials from -800 to 1500 mV(SCE), respectively, indicative of albumin adsorption. Within the same potential range and albumin addition to oxygenated solutions, the capacitances expanded slightly with a similar decreasing trend from 31 to 6 microF/cm(2), although the capacitance depicts an interaction between the hydrated passive film and the adsorbed albumin from -550 to 500 mV(SCE) in which the capacitance plateaued at 15 microF/cm(2). The hydrated porous oxide film results from the porous rutile layer reacting with H(2)O(2) formed as an intermediary component of oxygen reduction at the Ti-6Al-4V surface. The passive film-albumin interaction would affect the processing of titanium alloys in their surface preparation for biocompatibility, as well as determining the reactivity of titanium alloys to proteins.

Alloys↗

Fatigue-crack growth properties of thin-walled superelastic austenitic Nitinol tube for endovascular stents.

Over the past 10 years, the supereleastic nickel-titanium alloy Nitinol has found widespread application in the manufacture of small-scale biomedical devices, such as self-expanding endovascular stents. Although conventional stress/strain-life (S/N) analyses are invariably used as the primary method for design against fatigue loading and for predicting safe lifetimes, fracture mechanics-based methodologies provide a vital means of assessing the quantitative effect of defects on such lifetimes. Unfortunately, fracture mechanics studies on fatigue in Nitinol are scarce, and most results do not pertain to the (thin-walled tube) product forms that are typically used in the manufacture of endovascular stents. In the current work, we document the basic fatigue-crack growth properties of flattened thin-walled ( approximately 400 microm thick) Nitinol tubing in a 37 degrees C air environment. Crack-growth behavior is characterized over a wide range of growth rates ( approximately 6 orders of magnitude) and load ratios, that is, as a function of the alternating and maximum stress intensities, at 50 Hz. Limited experiments at both 5 and 50 Hz were also performed in 37 degrees C air and simulated body fluid to determine whether the cyclic frequency affects the fatigue behavior. Fatigue-crack growth-rate properties in such thin-walled Nitinol tube are found to be quite distinct from limited published data on other (mainly bulk) product forms of Nitinol, for example, bar and strip, both in terms of the relative fatigue thresholds and the variation in steady-state growth rates.

Alloys↗